A comparison of the high-temperature oxidation of 17Cr-2Ni and 18Cr-8Ni austenitic stainless steels at 973 K

被引:27
|
作者
Botella, J [1 ]
Merino, C
Otero, E
机构
[1] Acerinox, Ctr Invest & Ensayos, Cadiz 11379, Spain
[2] Univ Complutense, Fac Quim, Dept Ciencia Mat, E-28040 Madrid, Spain
来源
OXIDATION OF METALS | 1998年 / 49卷 / 3-4期
关键词
AISI; 304; low-nickel austenitic stainless steel; high temperature; high manganese; isothermal air oxidation;
D O I
10.1023/A:1018830424480
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The oxidation behavior in air at 973 K of the austenitic stainless steels 18Cr-8Ni and 17Cr-2.5Ni-10.5Mn-2Cu-0.17N (low-nickel content), was studied in a thermobalance. The steels were heated from room temperature up to 973 K at 10 K min(-1), oxidized for 80 hr and then cooled to room temperature at 80 K min(-1). The two steels had the same weight gains, 0.18 mg cm(-2), which is equivalent to oxidation layers about 1.15 mu m theoretical thickness. In both cases, the general shapes of the Delta W S-1 (mg cm(-2)) curves vs. t (hours) were parabolic, but X-ray diffraction of the oxidized surfaces, surface and cross-section optical microscopy and SEM observations and EDS microanalysis show important differences between them.
引用
收藏
页码:297 / 324
页数:28
相关论文
共 50 条
  • [21] Modification of inclusions by Al and Ca in ferrosilicon during alloying process of 18Cr-8Ni stainless steels
    Li, Weifu
    Ren, Ying
    Zhang, Lifeng
    IRONMAKING & STEELMAKING, 2020, 47 (01) : 40 - 46
  • [22] High-cycle fatigue behavior of 18Cr-8Ni austenitic stainless steels with grains ranging from nano/ultrafine-size to coarse
    Liu, J.
    Deng, X. T.
    Huang, L.
    Wang, Z. D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 733 : 128 - 136
  • [23] Heat-to-Heat Variation in Creep Life and Fundamental Creep Rupture Strength of 18Cr-8Ni, 18Cr-12Ni-Mo, 18Cr-10Ni-Ti, and 18Cr-12Ni-Nb Stainless Steels
    Abe, Fujio
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2016, 47A (09): : 4437 - 4454
  • [24] Stochastic Model for High Temperature Oxidation of Cr–Ni Austenitic Steels Assisted by Spallation
    Simon N. Lekakh
    Oleg Neroslavsky
    Mei Li
    Larry Godlevski
    Oxidation of Metals, 2022, 98 : 239 - 254
  • [25] PITTING RESISTANCE OF HIGH CR HIGH NI AUSTENITIC STAINLESS-STEELS
    YOSHII, T
    NISHIKAWA, M
    KAWAMURA, S
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1976, 16 (09) : 481 - 485
  • [26] High-temperature oxidation behavior of austenitic stainless steel Cr20Ni12Si2RE
    ZHANG Zhixia
    HONG Liu
    BI Hongyun
    BaosteelTechnicalResearch, 2019, 13 (01) : 32 - 37
  • [27] Auger Electron Microscopic Analysis on Microstructure of Inner Scale Developed with Steam Oxidation of Commercial 18Cr-8Ni Stainless Steels
    Nanko, Makoto
    Gocho, Akira
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2017, 81 (09) : 435 - 440
  • [28] Processing an 18Cr-8Ni Austenitic Stainless Steel Without the Dilemma of the Strength and Ductility Trade-Off
    He, Chengjie
    Zhu, Xiaoxiong
    Hu, Chengyang
    Dong, Hangyu
    Wan, Xiangliang
    Liu, Enyong
    Li, Guangqiang
    Wu, Kaiming
    JOM, 2024, 76 (02) : 829 - 842
  • [29] Processing an 18Cr-8Ni Austenitic Stainless Steel Without the Dilemma of the Strength and Ductility Trade-Off
    Chengjie He
    Xiaoxiong Zhu
    Chengyang Hu
    Hangyu Dong
    Xiangliang Wan
    Enyong Liu
    Guangqiang Li
    Kaiming Wu
    JOM, 2024, 76 : 829 - 842
  • [30] MICROSTRUCTURAL CORROSION BEHAVIOR OF CAST 18CR-8NI STAINLESS-STEEL
    AGARWALA, VS
    GREENE, ND
    METALLOGRAPHY, 1987, 20 (03): : 277 - 290