Spectra-Dependent Stability of the Passivation Quality of Al2O3/c-Si Interfaces

被引:7
|
作者
Veith-Wolf, Boris [1 ]
Witteck, Robert [1 ]
Morlier, Arnaud [1 ]
Schulte-Huxel, Henning [1 ]
Vogt, Malte Ruben [1 ]
Schmidt, Jan [1 ,2 ]
机构
[1] Inst Solar Energy Res Hamelin, D-31860 Emmerthal, Germany
[2] Leibniz Univ Hannover, Dept Solar Energy, Inst Solid State Phys, D-30167 Hannover, Germany
来源
IEEE JOURNAL OF PHOTOVOLTAICS | 2018年 / 8卷 / 01期
关键词
Accelerated testing; aluminum oxide (Al2O3); carrier lifetime; crystalline silicon; degradation; long-term stability; silicon nitride (SiNx); surface passivation; ultraviolet (UV) stability; ATOMIC-LAYER DEPOSITION; SURFACE PASSIVATION; OPTICAL-CONSTANTS; SOLAR; LIFETIME; SILICON; POWER;
D O I
10.1109/JPHOTOV.2017.2775147
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
We examine the stability of the c-Si surface passivation quality by spatial atomic-layer-deposited aluminum oxide (Al2O3), plasma-enhanced chemical vapor deposited silicon nitride (SiNx), and Al2O3/SiNx stacks under illumination with two different spectra. The Al2O3-passivated c-Si surfaces annealed at 350 degrees C show a weak degradation due to UV illumination, with surface recombination velocities (SRVs) of 122 cm/s after receiving a ultraviolet (UV) dose of 275 kWh/m(2). Silicon samples passivated with Al2O3 layers that received a fast-firing step show an improvement due to UV illumination with a reduction of the SRVs initially from 14 to 5 cm/s for single Al2O3 layers. For the fired Al2O3 layers the negative fixed charge density increases from -6x10(12) cm(-2) up to -1.2x10(13) cm-2 during UV illumination. We demonstrate that for the SiNx and the fired Al2O3 single layers, photons with energy greater than 3.4 eV are necessary to reduce the passivation quality. In contrast, low-temperature-annealed Al2O3 single layers and nonfired Al2O3/SiNx stacks showed a degradation already under illumination with a halogen lamp. Importantly, we observe a perfectly stable passivation on boron-diffused p(+) emitter for fired Al2O3/SiNx stacks featuring a stable saturation current density of 18 fA/cm(2) for a p(+) sheet resistance of 90 Omega/sq.
引用
收藏
页码:96 / 102
页数:7
相关论文
共 50 条
  • [31] Effect of the native oxide on the surface passivation of Si by Al2O3
    Getz, Michael N.
    Povoli, Marco
    Monakhov, Eduard
    JOURNAL OF APPLIED PHYSICS, 2021, 129 (20)
  • [32] Temperature-Dependent Thermal Boundary Conductance at Al/Al2O3 and Pt/Al2O3 interfaces
    Patrick E. Hopkins
    R. N. Salaway
    R. J. Stevens
    P. M. Norris
    International Journal of Thermophysics, 2007, 28 : 947 - 957
  • [33] Temperature-dependent thermal boundary conductance at Al/Al2O3 and Pt/Al2O3 interfaces
    Hopkins, Patrick E.
    Salaway, R. N.
    Stevens, R. J.
    Norris, P. M.
    INTERNATIONAL JOURNAL OF THERMOPHYSICS, 2007, 28 (03) : 947 - 957
  • [34] Stability of Al2O3 and Al2O3/a-SiNx:H stacks for surface passivation of crystalline silicon
    Dingemans, G.
    Engelhart, P.
    Seguin, R.
    Einsele, F.
    Hoex, B.
    van de Sanden, M. C. M.
    Kessels, W. M. M.
    JOURNAL OF APPLIED PHYSICS, 2009, 106 (11)
  • [35] Thermal stability of silicon surface passivation by APCVD Al2O3
    Black, Lachlan E.
    Allen, Thomas
    Cuevas, Andres
    McIntosh, Keith R.
    Veith, Boris
    Schmidt, Jan
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2014, 120 : 339 - 345
  • [36] Al+-doping of Si by laser ablation of Al2O3/SiN passivation
    Harder, Nils-Peter
    Larionova, Yevgeniya
    Brendel, Rolf
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2013, 210 (09): : 1871 - 1873
  • [37] Electrical and Chemical Characterization of Al2O3 Passivation Layer Deposited by Plasma-Assisted Atomic Layer Deposition in c-Si Solar Cells
    Shin, Kyong Cheol
    Lee, Jeong In
    Kang, Min Gu
    Song, Hee-eun
    2016 IEEE 43RD PHOTOVOLTAIC SPECIALISTS CONFERENCE (PVSC), 2016, : 2935 - 2937
  • [38] Fabrication of low cost nano-grass n-type C-Si solar cell with sol–gel Al2O3 passivation
    Soma Ray
    Anup Mondal
    Utpal Gangopadhyay
    SN Applied Sciences, 2020, 2
  • [39] Variation of the layer thickness to study the electrical property of PECVD Al2O3/c-Si interface
    Saint-Cast, Pierre
    Heo, Youn-Ho
    Billot, Etienne
    Olwal, Peter
    Hofmann, Marc
    Rentsch, Jochen
    Glunz, Stefan W.
    Preu, Ralf
    PROCEEDINGS OF THE SILICONPV 2011 CONFERENCE (1ST INTERNATIONAL CONFERENCE ON CRYSTALLINE SILICON PHOTOVOLTAICS), 2011, 8 : 642 - 647
  • [40] 2 μm thin film c-Si cells on near-Lambertian Al2O3 substrates
    Shimokawa, R
    Takahashi, T
    Takato, H
    Ozaki, A
    Takano, Y
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2001, 65 (1-4) : 593 - 598