Influence of ICCGHAZ on the Low-Temperature Toughness in HAZ of Heavy-Wall X80 Pipeline Steel

被引:10
|
作者
Fu, Chao [1 ,2 ]
Li, Xueda [3 ]
Li, Haichuan [4 ]
Han, Tao [3 ]
Han, Bin [3 ]
Wang, Yong [3 ]
机构
[1] China Univ Petr East China, Coll New Energy, Qingdao 266580, Peoples R China
[2] Shandong Inst Petr & Chem Technol, Dongying 257061, Peoples R China
[3] China Univ Petr East China, Sch Mat Sci & Engn, Qingdao 266580, Peoples R China
[4] PipeChina West East Gas Pipeline Co, Shanghai 200122, Peoples R China
基金
中国国家自然科学基金;
关键词
pipeline steel; low-temperature toughness; ICCGHAZ; LBZ; Arctic regions; MARTENSITE-AUSTENITE CONSTITUENTS; AFFECTED ZONE; CLEAVAGE FRACTURE; IMPACT TOUGHNESS; CHARPY IMPACT; MICROSTRUCTURE; IMPROVEMENT; MECHANISMS; PHASE; STRIP;
D O I
10.3390/met12060907
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Low-temperature embrittlement in the heat-affected zone (HAZ) of heavy-wall X80 weld joints is a primary challenge for arctic oil & gas exploitation. In this paper, the influence of inter-critically reheated coarse-grained HAZ (ICCGHAZ) on the low-temperature toughness of the weld joint in a 22 mm thick X80 spiral submerged arc welded pipe was studied through instrumented Charpy V-notch impact test at -80 similar to 20 degrees C and corresponding fracture surface characterization. The results indicated that the influence of ICCGHAZ on the overall toughness of the weld joint is related to temperature. At temperatures below -45 degrees C, individual and tiny martensite-austenite (MA) constituent debonding can trigger cleavage fracture-which was proved to be nucleation-controlled-and the probability of embrittlement of the ICCGHAZ increases. At temperatures higher than -45 degrees C, only relatively large or closely distributed MA constituent in ICCGHAZ satisfies the conditions to trigger propagation-controlled cleavage fractures, and the influence of ICCGHAZ on the overall toughness is not remarkable.
引用
收藏
页数:14
相关论文
共 50 条
  • [11] Control of Microstructures and the Practical Properties of API X80 Grade Heavy-Wall High-Frequency Electric Resistance-Welded Pipe with Excellent Low-Temperature Toughness
    Sota Goto
    Hiroshi Nakata
    Shunsuke Toyoda
    Takatoshi Okabe
    Tomohiro Inoue
    Metallurgical and Materials Transactions A, 2017, 48 : 5075 - 5084
  • [12] Microstructure and property of coarse grain HAZ X80 pipeline steel
    Zhou, Y
    Xue, XH
    Qian, BN
    Li, JL
    Shan, YY
    Lou, SN
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2005, 12 (06) : 54 - 58
  • [13] Enhancing the Toughness of Heavy thick X80 Pipeline Steel Plates By Microstructure Control
    Nie, Wenjin
    Xin, Weifeng
    Xu, Tianming
    Shi, Peijian
    Zhang, Xiaobing
    ADVANCED ENGINEERING MATERIALS, PTS 1-3, 2011, 194-196 : 1183 - 1191
  • [14] Insight into the Role of Mo Content on the Microstructure and Impact Toughness of X80 Thick-Walled Low-Temperature Pipeline Steel
    Jiang, Jinxing
    Zhang, Zhongde
    Zhao, Liyang
    Guan, Yingping
    Yuan, Liangzeng
    Wang, Qingfeng
    METALS, 2023, 13 (09)
  • [15] Effect of Ce on low temperature impact toughness of X80 steel
    Cao, X.-E., 1600, Editorial Office of Chinese Rare Earths, No. 36 Huanghe Street, RE Development Zone, Baotou, 014030, China (34):
  • [16] Material development for grade X80 heavy-wall hot induction bends
    Wang, Xu
    Xiao, Fu-ren
    Fu, Yan-hong
    Chen, Xiao-wei
    Liao, Bo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 530 : 539 - 547
  • [17] Fracture toughness of the materials in welded joint of X80 pipeline steel
    Yang, Yonghe
    Shi, Lei
    Xu, Zhen
    Lu, Hongsheng
    Chen, Xu
    Wang, Xin
    ENGINEERING FRACTURE MECHANICS, 2015, 148 : 337 - 349
  • [18] Effects of Alloy Content on Impact Toughness in X80 Pipeline Steel
    Wu, Guoxi
    Liu, Chengjun
    Chen, Ren
    Li, Xiaoliang
    Jiang, Maofa
    PROCEEDINGS OF THE 2015 2ND INTERNATIONAL FORUM ON ELECTRICAL ENGINEERING AND AUTOMATION (IFEEA 2015), 2016, 54 : 261 - 264
  • [19] CORROSION RESISTANT CERAMIC COATING FOR X80 PIPELINE STEEL BY LOW-TEMPERATURE PACK ALUMINIZING AND OXIDATION TREATMENT
    Huang Min
    Fu Qian-Gang
    Wang Yu
    Zhong Wen-Wu
    SURFACE REVIEW AND LETTERS, 2013, 20 (06)
  • [20] Statistical Assessment of Fracture Toughness Results from the HAZ of X80 Pipeline FCAW Girth Weld
    Chen, Hongyuan
    Feng, Qingshan
    Bi, Ying
    Gao, Xiongxiong
    Dai, Lianshuang
    Chi, Qiang
    MATERIALS, 2022, 15 (17)