A modified trilayer membrane for suppressing Li dendrite growth in all-solid-state lithium-metal batteries

被引:17
|
作者
Beshahwured, Shimelis Lemma [1 ,2 ]
Wu, Yi-Shiuan [1 ]
Truong, Thi BeTa [1 ]
Jose, Rajan [3 ]
Yang, Chun-Chen [1 ,2 ,4 ,5 ]
机构
[1] Ming Chi Univ Technol, Battery Res Ctr Green Energy, New Taipei 24301, Taiwan
[2] Ming Chi Univ Technol, Dept Chem Engn, New Taipei 24301, Taiwan
[3] Univ Malaysia Pahang, Fac Ind Sci & Technol, Nanostruct Renewable Energy Mat Lab, Kuantan 26300, Malaysia
[4] Chang Gung Univ, Dept Chem & Mat Engn, Taoyuan 333, Taiwan
[5] Chang Gung Univ, Green Technol Res Ctr, Taoyuan 333, Taiwan
关键词
All-solid-state lithium-metal batteries; Modified trilayer HSE membrane; f-VGCF; NCM622 cathode material; Needle-like filler; COMPOSITE POLYMER ELECTROLYTES; IONIC-CONDUCTIVITY; PVDF-HFP; TRANSPORT; ANODE; ALUMINA;
D O I
10.1016/j.cej.2021.131850
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Mechanically robust trilayer HSE membrane modified with an optimized amount of functionalized vapor-grown carbon fiber (f-VGCF) is prepared using a solution-casting method. This trilayer membrane had the structure SPE0 (PVDF-HFP/LiTFSI/SN)|SPE2 (PVDF-HFP/Al-doped-LLZO/LiTFSI/SN)|SPE1 (PVDF-HFP/LiTFSI/SN/f-VGCF). The SPE0 (unmodified) and SPE1 (modified) layers faced the cathode and anode sides, respectively; SPE2 is the same as SPE0 but loaded with needle-like Li6.25Al0.25La3Zr2O12 filler. The modified trilayer HSE membrane possessed an ionic conductivity (4.72 x 10(-4) S cm(-1)) and a Li transference number (0.52) higher than unmodified trilayer HSE membrane (3.68 x 10(-4) S cm(-1) and 0.41, respectively). A Li/SPE1-SPE2-SPE1/Li symmetric cell displayed extremely stable Li plating/stripping performance when tested sequentially at 0.1, 0.2, 0.5, and 1 mA cm(-2) for 800 h (200 h for each current density). A 2032 coin cell incorporating NCM622/SPE0-SPE2-SPE1/Li delivered a desirable capacity output with excellent cycling stability (85.04% capacity retention after 627 cycles with an average coulombic efficiency of 99.17% at a rate of 0.5C at room temperature). A pouch cell based on NCM622/SPE0-SPE2-SPE1/Li also achieved excellent capacity retention of 95.37% after 100 cycles with an average coulombic efficiency of 99.81% at 0.2C at room temperature. Thus, ASSLMBs incorporating such modified trilayer HSE membranes have potential for practical applications.
引用
收藏
页数:16
相关论文
共 50 条
  • [1] Suppressing dendrite growth through the design of glassy sulfide for all-solid-state lithium metal batteries
    Kuang, Juner
    Su, Han
    Zhong, Yu
    Zhou, Chengao
    Wang, Xiuli
    Tu, Jiangping
    [J]. Chemical Engineering Journal, 2024, 501
  • [2] Dendrite-free lithium-metal all-solid-state batteries by solid-phase passivation
    Gao, Qifa
    Wu, Dengxu
    Zhu, Xiang
    Lu, Pushun
    Ma, Tenghuan
    Yang, Ming
    Chen, Liquan
    Li, Hong
    Wu, Fan
    [J]. NANO ENERGY, 2023, 117
  • [3] Controlling the Lithium-Metal Growth To Enable Low-Lithium-Metal-Excess All-Solid-State Lithium-Metal Batteries
    Liu, Ming
    Wang, Chao
    Cheng, Zhu
    Ganapathy, Swapna
    Haverkate, Lucas A.
    Unnikrishnan, Sandeep
    Wagemaker, Marnix
    [J]. ACS MATERIALS LETTERS, 2020, 2 (07): : 665 - 670
  • [4] Lithium-Metal Batteries via Suppressing Li Dendrite Growth and Improving Coulombic Efficiency
    Su, Laisuo
    Manthiram, Arumugam
    [J]. SMALL STRUCTURES, 2022, 3 (10):
  • [5] Lithium anode interlayer design for all-solid-state lithium-metal batteries
    Zeyi Wang
    Jiale Xia
    Xiao Ji
    Yijie Liu
    Jiaxun Zhang
    Xinzi He
    Weiran Zhang
    Hongli Wan
    Chunsheng Wang
    [J]. Nature Energy, 2024, 9 : 251 - 262
  • [6] Lithium anode interlayer design for all-solid-state lithium-metal batteries
    Wang, Zeyi
    Xia, Jiale
    Ji, Xiao
    Liu, Yijie
    Zhang, Jiaxun
    He, Xinzi
    Zhang, Weiran
    Wan, Hongli
    Wang, Chunsheng
    [J]. NATURE ENERGY, 2024, 9 (03) : 251 - 262
  • [7] Interfacial engineering of suppressing Li dendrite growth in all solid-state Li-metal batteries
    Yang, Xinyi
    Wang, Youwei
    Guo, Yuanhang
    Liao, Ziyan
    Fu, Wensheng
    Liu, Jianjun
    [J]. JOURNAL OF MATERIALS CHEMISTRY A, 2024, 12 (25) : 14848 - 14865
  • [8] Dendrite growth and inhibition in all-solid-state lithium metal batteries: in situ optical observation
    Liu, Haowen
    Jiang, Weining
    Chen, Wenjie
    Lin, Qiyuan
    Ren, Shuaiyang
    Su, Yipeng
    Tong, Ruoyu
    Zhang, Yuegang
    [J]. JOURNAL OF MATERIALS CHEMISTRY A, 2024, 12 (06) : 3575 - 3579
  • [9] Linking the Defects to the Formation and Growth of Li Dendrite in All-Solid-State Batteries
    Wang, Hongchun
    Gao, Haowen
    Chen, Xiaoxuan
    Zhu, Jianping
    Li, Wangqin
    Gong, Zhengliang
    Li, Yangxing
    Wang, Ming-Sheng
    Yang, Yong
    [J]. ADVANCED ENERGY MATERIALS, 2021, 11 (42)
  • [10] Anode interface in all-solid-state lithium-metal batteries: Challenges and strategies
    Yu Qi-Peng
    Liu Qi
    Wang Zi-Qiang
    Li Bao-Hua
    [J]. ACTA PHYSICA SINICA, 2020, 69 (22)