Hot deformation behavior in Mg-Al alloy, AZ91D grain refined by isothermal-rolling

被引:0
|
作者
Torisaka, Y
Fudetani, S
Hirohashi, M
机构
[1] Natl Inst Adv Ind Sci & Technol, Tsukuba, Ibaraki 3058564, Japan
[2] Chiba Univ, Grad Sch Sci & Technol, Chiba, Japan
关键词
magnesium alloys; AZ91D; isothermal rolling; high temperature deformation; activation energy; volume diffusion; grain boundary diffusion;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The isothermal-rolling mill has been developed for non-working materials, for example, like Mg-Al alloy. The recrystallization behavior of Mg-Al alloy, AZ91D has been investigated. The starting and finishing temperatures of recrystallization are 523K and 648K, respectively. AZ91D sheets tempered to fine grain size by recrystallization have been prepared and tensed at high temperatures. Both the total elongation and strain-rate sensitivity m have been obtained and discussed. The values of total elongation have exceeded over 100% at testing temperature over 623K with strain-rate below 1.0 x 10(-2) s(-1) and 170% of maximum total elongation has been obtained. The ill values have indicated over 0.5 in range of 1.0 x 10(-4) s(-1) to 2.5. x 10(-4) s(-1) except testing temperature of 573K. The activation energy required for high temperature deformation has been calculated to be about 124kJ.mol(-1), which is almost same of the activation energy for self-diffusion coefficient in Mg. Therefore, the deformation of AZ91D has been accommodated by volume diffusion.
引用
收藏
页码:67 / 71
页数:5
相关论文
共 50 条
  • [31] High-temperature compression deformation behavior of fly ash cenosphere/AZ91D Mg alloy composites
    College of Mechanical and Electronic Engineering, China University of Petroleum, Qingdao
    266580, China
    不详
    154007, China
    Fuhe Cailiao Xuebao, 5 (1461-1468):
  • [32] Effect of Mg-TiB2 master alloy on the grain refinement of AZ91D magnesium alloy
    Liu, Shengfa
    Zhang, Yuan
    Han, Hui
    Li, Bo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 487 (1-2) : 202 - 205
  • [33] Semisolid Microstructure Evolution of AZ91D Magnesium Alloy Refined by Al-Ti-B
    Chen, Ti Jun
    Wang, Rui Quan
    Ma, Ying
    Hao, Yuan
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2011, 14 (04): : 532 - 540
  • [34] Plastic deformation of AZ91D magnesium alloy and recrystallization structure simulation in heated roll rolling
    Mei R.-B.
    Shi X.-L.
    Bao L.
    Li C.-S.
    Liu X.-H.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2022, 32 (05): : 1289 - 1301
  • [35] Fretting wear behavior of AZ91D magnesium alloy
    陈安华
    黄伟九
    李兆峰
    Transactions of Nonferrous Metals Society of China, 2006, (S3) : 1879 - 1883
  • [36] Electrodeposition of chemically and mechanically protective Al-coatings on AZ91D Mg alloy
    Yang, Haiyan
    Guo, Xingwu
    Wu, Guohua
    Ding, Wenjiang
    Birbilis, Nick
    CORROSION SCIENCE, 2011, 53 (01) : 381 - 387
  • [37] Fretting wear behavior of AZ91D magnesium alloy
    Chen An-hua
    Huang Wei-jiu
    Li Zhao-feng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1879 - S1883
  • [38] Tensile and fatigue behavior of AZ91D magnesium alloy
    Bag, A
    Zhou, W
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2001, 20 (05) : 457 - 459
  • [39] Investigation on aging behavior of AZ91D magnesium alloy
    Liu, Guanjun
    Li, Wenfang
    Peng, Jihua
    ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 1386 - +
  • [40] Grain refinement of AZ91D magnesium alloy by a new Mg-50%Al4C3 master alloy
    Liu, Shengfa
    Chen, Yang
    Han, Hui
    Journal of Alloys and Compounds, 2015, 624 : 266 - 269