Effect of Sensitization on Hydrogen Embrittlement in a 5083 Aluminum Alloy

被引:0
|
作者
Ghorani, Alireza [1 ]
Itoh, Goroh [2 ]
Ohbuchi, Tomoyuki [2 ]
Kiuchi, Tomoya [2 ]
机构
[1] Ibaraki Univ, Grad Sch Sci & Engn, Complex Syst Sci, Hitachi 3168511, Japan
[2] Ibaraki Univ, Grad Sch Sci & Engn, Mech Syst Engn, Hitachi 3168511, Japan
关键词
hydrogen embrittlement; humid air; 5083 aluminum alloy; welded joint; sensitization; STRESS-CORROSION CRACKING; AL-MG;
D O I
10.2320/matertrans.MT-M2022088
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The 5000 series non-heat-treatable Al -Mg alloys are widely used as structural members, because of excellent combination of weldability, corrosion resistance and mechanical properties. It is well known that these alloys can become susceptible to inter-granular stress corrosion cracking. In the previous paper, the authors revealed that hydrogen embrittlement (HE) takes place in weld corner (fusion zone adjacent to HAZ) in an MIG-welded joint of 5083 alloy. In this study, the base material and MIG-welded joint of the 5083 alloy were sensitized, and their resistance to HE was investigated by two methods: humid gas stress corrosion cracking (HG-SCC) and slow strain rate tensile (SSRT) tests. The results obtained were discussed, in comparison with the previous results obtained in the non-sensitized joint. Discussion was also made in terms of the difference of the two testing methods. Extension of HG-SCC cracks were observed for all sensitized 5083 alloy samples, base and welded samples tested in humid air, and hence HE was confirmed. Fractography and surface observation on the crack tip of HG-SCC revealed that the crack propagates in a transgranular manner. The extent of HG-SCC was greater in the present sensitized specimens in all the locations except the weld corner, but the position dependency has been the same: crack propagation amount was largest in the weld corner. On the other hand, SSRT test results did not indicate any reduction in ductility or strength when testing environment was changed from dry nitrogen gas to humid air. Therefore, it is concluded that HG-SCC test is more sensitive for detecting HE of 5083 alloy
引用
收藏
页码:1425 / 1430
页数:6
相关论文
共 50 条
  • [31] WELDING AND CHARACTERIZATION OF 5083 ALUMINUM ALLOY
    Hakem, Maamar
    Lebaili, S.
    Miroud, J.
    Bentaleb, A.
    Toukali, S.
    21ST INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2012), 2012, : 1478 - 1484
  • [32] Effect of carbon alloying on hydrogen embrittlement of a Cantor alloy
    Panchenko, M. Yu.
    Melnikov, E., V
    Gurtova, D. Yu.
    Astafurova, E. G.
    LETTERS ON MATERIALS, 2022, 12 (04): : 282 - 286
  • [33] THE EFFECT OF AGING ON HYDROGEN EMBRITTLEMENT OF A NICKEL-ALLOY
    COYLE, RJ
    KARGOL, JA
    FIORE, NF
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (04): : 653 - 658
  • [34] Microforming of superplastic 5083 aluminum alloy
    Hossain, Md. Abu Mowazzem
    Hong, Sung-Tae
    Park, Kyu-Yeol
    Na, Young-Sang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 : S656 - S660
  • [35] Microforming of superplastic 5083 aluminum alloy
    Md.Abu Mowazzem HOSSAIN
    Sung-Tae HONG
    Kyu-Yeol PARK
    Young-Sang NA
    TransactionsofNonferrousMetalsSocietyofChina, 2012, 22(S3) (S3) : 656 - 660
  • [36] INVESTIGATION OF SUPERPLASTICITY IN ALUMINUM ALLOY 5083
    Zhao, Shasha
    Qayyume, Rehan
    Diao, Haoyan
    Ma, Chaoli
    Wu, Xiaowei
    Wang, Yong
    PROCEEDINGS OF THE 13TH INTERNATIONAL CONFERENCE ON ALUMINUM ALLOYS (ICAA13), 2012, : 825 - 830
  • [37] HYDROGEN EMBRITTLEMENT OF 1100 ALUMINUM
    LOUTHAN, MR
    DEXTER, AH
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1975, 6 (08): : 1655 - 1657
  • [38] Effect of a trace of sodium on the high temperature ductility of 5083 aluminum alloy
    Fujiwara Y.
    Tanigaki K.
    Horikawa K.
    Kobayashi H.
    Keikinzoku/Journal of Japan Institute of Light Metals, 2016, 66 (08): : 426 - 431
  • [39] Effect of Microstructure on Corrosion Behavior of Cold Sprayed Aluminum Alloy 5083
    Kim, Munsu
    Perez-Andrade, Lorena
    Brewer, Luke N.
    Kubacki, Gregory W.
    CORROSION AND MATERIALS DEGRADATION, 2024, 5 (01) : 27 - 51
  • [40] Effect on formation of 5083 aluminum alloy of activating flux in FBTIG welding
    Zhao, Yong
    Yang, Gang
    Yan, Keng
    Liu, Wei
    ADVANCED MATERIALS AND PROCESSES, PTS 1-3, 2011, 311-313 : 2385 - +