摘要
Polyphenylene sulfide (PPS) is a high-performance plastic with outstanding mechanical, physical and thermal characteristics for lightweight automobiles and rail-mounted vehicles. The adhesive behavior of PPS with aluminum plates by using epoxy (EP) and polyurethane (PU) adhesives is the subject of these investigations, whereby the activation of the PPS surfaces took place by means of low-pressure plasma treatment. The determination of the changes caused in terms of topography, surface tension and chemical composition of the PPS surfaces after low-pressure plasma treatment was carried out by means of scanning electron microscopy (SEM), contact angle measurements and energy dispersive X-ray analysis (EDX). The adhesion bond strength increased after oxygen plasma treatment by 103% (EP 1), 134% (EP 2) and 56% (PU). After argon plasma treatment, the increase in adhesive bond strength was only 79% (EP 1), 122% (EP 2) and 27% (PU). The failure took place with increasing adhesive strength with EP I predominantly cohesively in the PPS at the aluminum lap end, with EP 2 adhesively at the aluminum surface and with PU cohesively in the adhesive layer. The surface energy and the polar contributions increased significantly with treatment time with both plasma gases. This was more pronounced with oxygen than with argon plasma. The dispersive contributions to the surface free energy hardly changed with increasing treatment time. The SEM shows that the surface roughness also increases with treatment time in the case of the oxygen plasma more compared with the argon plasma. Furthermore, a deposit of reaction products on the surfaces was detected. (c) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:16 / 22
页数:7
相关论文
共 50 条
  • [31] Low-pressure water vapour plasma treatment of surfaces for biomolecules decontamination
    Fumagalli, F.
    Kylian, O.
    Amato, L.
    Hanus, J.
    Rossi, F.
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2012, 45 (13)
  • [32] Low-pressure plasma cleaning of Au and PtIr noble metal surfaces
    Fuchs, P.
    APPLIED SURFACE SCIENCE, 2009, 256 (05) : 1382 - 1390
  • [33] Low pressure plasma pretreatment of ASA/PC-blend surfaces
    Anagreh, N.
    Dorn, L.
    KGK-Kautschuk und Gummi Kunststoffe, 2002, 55 (11): : 574 - 579
  • [34] Low pressure plasma pretreatment of ASA/PC-blend surfaces
    Anagreh, N
    Dorn, L
    KAUTSCHUK GUMMI KUNSTSTOFFE, 2002, 55 (11): : 574 - +
  • [35] Ultraviolet light pretreatment of polymers and polymer composite surfaces for adhesive bonding
    Dontula, N
    Weitzsacker, CL
    Drzal, LT
    RADTECH'98 NORTH AMERICA UV/EB CONFERENCE PROCEEDINGS, 1998, : 125 - 132
  • [36] STABILITY OF A LOW-PRESSURE PLASMA
    AGARWAL, DC
    INDIAN JOURNAL OF THEORETICAL PHYSICS, 1973, 21 (03): : 79 - 88
  • [37] Low-Temperature Low-Pressure Bonding by Nanocomposites
    Wu, Ting-Jui
    Liu, Jen-Hsiang
    Song, Jenn-Ming
    2017 5TH INTERNATIONAL WORKSHOP ON LOW TEMPERATURE BONDING FOR 3D INTEGRATION (LTB-3D), 2017, : 33 - 33
  • [38] A COMPARISON OF LOW-PRESSURE ARC AND LOW-PRESSURE PLASMA SPRAYED TITANIUM COATINGS
    STEFFENS, HD
    ERTURK, E
    BUSSE, KH
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1985, 3 (06): : 2459 - 2463
  • [39] TREATMENT OF LOW-ENERGY SURFACES FOR ADHESIVE BONDING
    BREWIS, DM
    MATHIESON, I
    WOLFENSBERGER, M
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1995, 15 (02) : 87 - 90
  • [40] Atmospheric-pressure plasma pretreatment for direct bonding of silicon wafers at low temperatures
    Eichler, M.
    Michel, B.
    Thomas, M.
    Gabriel, M.
    Klages, C. -P.
    SURFACE & COATINGS TECHNOLOGY, 2008, 203 (5-7): : 826 - 829