Preparation of semi-solid A380 aluminum alloy slurry by serpentine channel

被引:24
|
作者
Liu, Zhi-yong [1 ]
Mao, Wei-min [1 ]
Wang, Wei-pan [1 ]
Zheng, Zhi-kai [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
A380 aluminum alloy; semi-solid slurry; serpentine channel; primary alpha(Al); A356; ALLOY; MICROSTRUCTURAL EVOLUTION; GRAIN-REFINEMENT;
D O I
10.1016/S1003-6326(15)63741-4
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The semi-solid slurry of A380 aluminum alloy was prepared by the serpentine channel. The effects of pouring temperature, curve number and curve diameter of the serpentine channel on the microstructure of the semi-solid A380 aluminum alloy slurry were investigated. The results show that the satisfactory semi-solid A380 aluminum alloy slurry could be obtained when the pouring temperature ranged from 630 to 650 degrees C. Under the same conditions, increasing the curve number or reducing the curve diameter of the serpentine channel would decrease the average diameter and increase the shape factor of the primary alpha(Al) grains. The "self-stirring" of the alloy melt in the serpentine channel was beneficial to the ripening of the dendrites and the spheroidizing of the primary alpha(Al) grains.