Influence of peritectic phase transformation on hot ductility of high aluminium TRIP steels containing Nb

被引:8
|
作者
Tuling, A. [1 ]
Banerjee, J. R. [1 ]
Mintz, B. [1 ]
机构
[1] Univ Pretoria, ZA-0028 Pretoria, South Africa
关键词
TRIP steels; Hot ductility; High Al and Nb; Peritectic; TRANSVERSE CRACKING; C-MN; AL;
D O I
10.1179/1743284711Y.0000000013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Increasing Al from 0.05 to 1% in Nb containing transformation induced plasticity steel resulted in deepening and considerable widening of the hot ductility trough. Further increase in the Al level to 1.5% produced a trough similar to the low Al steel but having better ductility in the temperature range of 650-800 degrees C. This improved ductility could be ascribed to its finer austenite grain size. Nb( CN) was able to precipitate readily in these steels and was important in influencing the hot ductility of the 0.05 and 1.5% Al steel in the temperature range of 750-1000 degrees C, with ductility improving as the particle size increased with test temperature. No AlN was found in 0.05% Al containing steel, and there was no significant dendritic precipitation of AlN in 1.5% Al containing steel, although precipitation of AlN in plate form was readily observed. In 1% Al steel, copious dendritic precipitation of AlN was present at the c grain boundaries, leading to rock candy fracture. The poor ductility shown in 1% Al containing steel is due to a combination of this dendritic precipitation, which took place only in a steel of peritectic carbon composition, and its coarse grain size. Both low and 1.5% Al containing steels had compositions outside the peritectic range. It is strongly advised that for this type of steel, the composition should be designed to fall outside the peritectic carbon range.
引用
收藏
页码:1724 / 1731
页数:8
相关论文
共 50 条
  • [21] INFLUENCE OF CARBON ON HOT DUCTILITY OF STEELS
    CROWTHER, DN
    MINTZ, B
    MATERIALS SCIENCE AND TECHNOLOGY, 1986, 2 (07) : 671 - 676
  • [23] Hot ductility behavior of vanadium containing steels
    Mohamed, Z
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 326 (02): : 255 - 260
  • [24] Influence of titanium and nitrogen on hot ductility of C-Mn-Nb-Al steels
    Comineli, O
    Abushosha, R
    Mintz, B
    MATERIALS SCIENCE AND TECHNOLOGY, 1999, 15 (09) : 1058 - 1068
  • [25] Influence of manganese, silicon and aluminium on the transformation behavior of low alloyed TRIP-steels
    Traint, S
    Pichler, A
    Tikal, R
    Stiaszny, P
    Werner, EA
    42ND MECHANICAL WORKING AND STEEL PROCESSING CONFERENCE PROCEEDINGS, 2000, 38 : 549 - 561
  • [26] Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels
    Guo Junli
    Wen Guanghua
    Fu Jiaojiao
    Tang Ping
    Hou Zibing
    Gu Shaopeng
    ACTA METALLURGICA SINICA, 2019, 55 (10) : 1311 - 1318
  • [27] Influence of S and AlN on hot ductility of high Al, TWIP steels
    Kang, S. E.
    Banerjee, J. R.
    Mintz, B.
    MATERIALS SCIENCE AND TECHNOLOGY, 2012, 28 (05) : 589 - 596
  • [28] Influence of Ti on the Hot Ductility of High-manganese Austenitic Steels
    Liu, Hongbo
    Liu, Jianhua
    Wu, Bowei
    Su, Xiaofeng
    Li, Shiqi
    Ding, Hao
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2017, 36 (07) : 725 - 732
  • [29] THE INFLUENCE OF INCLUSION SHAPE ON THE HOT DUCTILITY OF STEELS
    CROWTHER, DN
    MINTZ, B
    CIM BULLETIN, 1986, 79 (890): : 78 - 78
  • [30] Effect of niobium on the phase transformation behavior of aluminum containing steels for TRIP products
    Fonstein, N
    Yakubovsky, O
    Bhattacharya, D
    Siciliano, F
    MICROALLOYING FOR NEW STEEL PROCESSES AND APPLICATIONS, 2005, 500-501 : 453 - 460