Effect of Shield Gas Composition on Cold Cracking Susceptibility of YS 600 MPa Flux Cored Arc Weld Metal
被引:3
|作者:
Xian, Guo
[1
]
Lee, Myungjin
[1
]
Lee, Junghoon
[1
]
Kang, Namhyun
[1
]
机构:
[1] Pusan Natl Univ, Dept Mat Sci & Engn, Busan 609735, South Korea
来源:
基金:
新加坡国家研究基金会;
关键词:
metals;
welding;
microstructure;
transmission electron microscopy (TEM);
cold crack;
ACICULAR FERRITE;
TOUGHNESS;
SIZE;
D O I:
10.3365/KJMM.2015.53.7.480
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
Cold cracking is one of the most common catastrophic defects in welds. In this study, we investigated the effect of the shield gas composition (specifically Ar+5 similar to 20% CO2) on the cold-crack ratio on the preheating temperature of 20 degrees C similar to 100 degrees C in flux-cored arc welds. Critical assessment of the cold-crack ratio was achieved by observing the weld cross-section, appearance of surface cracks, and fractography. The cold-crack ratio decreased as the preheating temperature increased from 20 to 100 degrees C. For the preheating temperature of 50 degrees C, the shield gas (containing 20% CO2) provided higher oxygen content in the weld metal and increased the number of nucleant inclusions for acicular ferrite; thereby eliminating cold cracks. The shield gas with 15% CO2 produced welds that had nearly the same amount of acicular ferrite as compared with the 5% and 10% CO2 cases. However, the 15% CO2 shield gas produced the greatest hardness and largest amount of non-nucleant inclusions in the weld metal, therefore exhibiting the largest cold-crack ratio. If the volume fraction of acicular ferrite remains unchanged, hardness and non-nucleant inclusions should be considered roughly for assessment of the cold-crack ratio.