Effect of B addition on thermal stability of lamellar structure in Ti-47Al-2Cr-2Nb alloys

被引:0
|
作者
Yamamoto, Y [1 ]
Evans, ND [1 ]
Maziasz, PJ [1 ]
Liu, CT [1 ]
机构
[1] Oak Ridge Natl Lab, Div Met & Ceram, Oak Ridge, TN 37831 USA
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Thermal stability of fully lamellar microstructures in Ti-47Al-2Cr-2Nb (at.%) alloys with and without B additions has been evaluated in the temperature range of 800 to 1200 degrees C. The alloy with 0.15B exhibits an alpha(2)+gamma fully lamellar microstructure containing ribbon-like structures (TiB2+beta) inside the lamellar colonies. During aging at 800 and 1600 degrees C, beta particles surrounded by gamma grains form adjacent to the ribbon-like structures. The formation of these grains is attributed to the precipitation of thin plate-like 0 phase along {1100}(TiB2) within the TiB2 ribbon particles, resulting in the loss of alpha(2) plates around the ribbon-like structure by scavenging Ti. This allows coarsening gamma lamellar plates to form new gamma grains, and then the ribbon-like structure completely dissolves to leave only particles. At 1200 degrees C, discontinuous coarsening (DC) of the lamellae becomes the dominant mode of microstructural change for all the alloys. However, the ribbon-like structures in the alloy with B additions play a role in pinning the DC cells, which leads to higher thermal stability of the lamellar microstructure in that alloy.
引用
收藏
页码:163 / 168
页数:6
相关论文
共 50 条
  • [21] Microstructure and mechanical properties of cast Ti-47Al-2Cr-2Nb alloy melted in various crucibles
    Wang LigangZheng LijingCui RenjieYang LiliZhang Hu School of Materials Science and EngineeringBeihang UniversityBeijing China
    China Foundry, 2012, 9 (01) : 48 - 52
  • [22] EFFECT OF WITHDRAWAL RATE ON THE MICROSTRUCTURE OF DIRECTIONAL SOLIDIFIED Ti-47Al-2Cr-2Nb-0.8B ALLOYS
    Yang Lili
    Zheng Lijing
    Xiao Zhixia
    Yan Jie
    Zhang Hu
    ACTA METALLURGICA SINICA, 2010, 46 (07) : 879 - 884
  • [23] Development of an oxidation resistant glass-ceramic composite coating on Ti-47Al-2Cr-2Nb alloy
    Li, Wenbo
    Zhu, Shenglong
    Chen, Minghui
    Wang, Cheng
    Wang, Fuhui
    APPLIED SURFACE SCIENCE, 2014, 292 : 583 - 590
  • [24] The crack and pore formation mechanism of Ti-47Al-2Cr-2Nb alloy fabricated by selective laser melting
    Shi, Xuezhi
    Wang, Huaxue
    Feng, Wuwei
    Zhang, Yulian
    Ma, Shuyuan
    Wei, Jun
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2020, 91
  • [25] 过热度对Ti-47Al-2Cr-2Nb缩孔缩松的影响研究
    纪玮
    刘宗德
    张虎
    华北电力大学学报(自然科学版), 2011, 38 (02) : 100 - 102+107
  • [26] B、Y及冷却速度对Ti-47Al-2Cr-2Nb合金组织的细化作用
    王建吉
    杨莉莉
    郑立静
    闫洁
    肖志霞
    李国强
    张虎
    特种铸造及有色合金, 2011, 31 (03) : 260 - 263+193
  • [27] High cycle fatigue behaviour of Ti-47Al-2Cr-2Nb and Ti-6242S with (Al,Cr)3Ti plasma spray protective coating
    Wood, TD
    Dewald, DK
    Mikkola, DE
    SURFACE ENGINEERING, 1999, 15 (04) : 335 - 339
  • [28] Influence of elemental B addition on the heat-treated cast structures of Ti–47Al–2Cr–(2–4)Nb alloys
    J. Y. Jung
    J. K. Park
    Journal of Materials Research, 1997, 12 : 665 - 680
  • [29] Influence of elemental B addition on the heat-treated cast structures of Ti-47Al-2Cr-(2-4)Nb alloys
    Jung, JY
    Park, JK
    JOURNAL OF MATERIALS RESEARCH, 1997, 12 (03) : 665 - 680
  • [30] TENSILE AND HIGH CYCLE FATIGUE PROPERTIES OF Ti-47Al-2Cr-2Nb DIRECTIONALLY SOLIDIFIED BY COLD CRUCIBLE METHOD
    Ding Hongsheng
    Shang Zibo
    Wang Yongzhe
    Chen Ruirun
    Guo Jingjie
    Fu Hengzhi
    ACTA METALLURGICA SINICA, 2015, 51 (05) : 569 - 579