Microstructures and Mechanical Properties of Commercial Hot-Extruded Copper Processed by Torsion Deformation

被引:18
|
作者
Guo, Ning [1 ,2 ]
Li, Xiaoxia [1 ]
Xiao, Mei [1 ]
Xin, Renlong [2 ]
Chai, Linjiang [3 ]
Song, Bo [1 ]
Yu, Hongbing [4 ]
Li, Lu [1 ]
机构
[1] Southwest Univ, Fac Mat & Energy, Chongqing 400715, Peoples R China
[2] Chongqing Univ, Sch Mat Sci & Engn, Chongqing 400030, Peoples R China
[3] Chongqing Univ Technol, Sch Mat Sci & Engn, Chongqing 400054, Peoples R China
[4] Queens Univ, Dept Mech & Mat Engn, Kingston, ON K7L 3N6, Canada
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
ULTRAFINE-GRAINED COPPER; PEARLITIC STEEL WIRES; HIGH-PRESSURE TORSION; MAGNESIUM ALLOY RODS; ULTRAHIGH-STRENGTH; LARGE STRAINS; PURE COPPER; EVOLUTION; TENSILE; BEHAVIOR;
D O I
10.1002/adem.201600252
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Free-end torsion deformation is used for processing copper rod in this work. Both microstructures and mechanical properties of the torsional rods are quantitatively analyzed. The results show that gradient lamellar dislocation substructures (LDS) along the radial direction as the main defects are formed after torsion. The increment of the LDS density, the shrinking of spacing size, and the change of length/spacing (L/S) ratio of the LDS are all non-monotonic function of torsion revolution. High-density LDS with fine spacing can retain strain hardening capability, which results in good combination of high tensile strength and good ductility in the torsional deformed sample with large number of revolutions. The influence of torsion strain on primary twin boundaries (TBs) in the hot-extruded rod is also discussed.
引用
收藏
页码:1738 / 1746
页数:9
相关论文
共 50 条
  • [31] Enhanced Mechanical Properties and Corrosion Resistance by Minor Gd Alloying with a Hot-Extruded Mg Alloy
    Yao, Huai
    Wang, Shubo
    Xiong, Yi
    Shi, Xinying
    Singh, Harishchandra
    Huttula, Marko
    Cao, Wei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 9997 - 10009
  • [32] Structure and mechanical properties of hot-extruded Mg-Y-Zn-Mn biodegradable alloys
    Bazhenov, V. E.
    Li, A. V.
    Rogachev, S. O.
    Bazlov, A. I.
    Statnik, E. S.
    Tavolzhanskii, S. A.
    Komissarov, A. A.
    Redko, N. A.
    Korsunsky, A. M.
    Shin, K. S.
    MATERIALS TODAY COMMUNICATIONS, 2024, 40
  • [33] Microstructures and mechanical properties of commercial purity iron processed by asymmetric rolling
    Ding, Yi
    Jiang, Jianhua
    Shan, Aidang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 509 (1-2): : 76 - 80
  • [34] Microstructure and mechanical and corrosion properties of hot-extruded Mg–Zn–Ca–(Mn) biodegradable alloys
    V.E.Bazhenov
    A.V.Li
    A.A.Komissarov
    A.V.Koltygin
    S.A.Tavolzhanskii
    V.A.Bautin
    O.O.Voropaeva
    A.M.Mukhametshina
    A.A.Tokar
    Journal of Magnesium and Alloys, 2021, (04) : 1428 - 1442
  • [35] Effect of solid solution and aging treatment on the microstructures and properties of hot-extruded Cu-Te-Li alloys
    Zeng, T.
    Tang, K.
    Zhu, D.
    Yang, C.
    Chen, P.
    OPTOELECTRONICS AND ADVANCED MATERIALS-RAPID COMMUNICATIONS, 2014, 8 (5-6): : 495 - 499
  • [36] Effects of Al on microstructure and mechanical properties of hot-extruded Mg-3Nd alloys
    Yu, Peichen
    Wang, Lei
    Wang, Liping
    Feng, Yicheng
    Fu, Yuanke
    Zhao, Sicong
    Guo, Erjun
    Wang, Zhiwei
    MATERIALS SCIENCE AND TECHNOLOGY, 2023, 39 (03) : 381 - 391
  • [37] Microstructure and mechanical and corrosion properties of hot-extruded Mg–Zn–Ca–(Mn) biodegradable alloys
    VEBazhenov
    AVLi
    AAKomissarov
    AVKoltygin
    SATavolzhanskii
    VABautin
    OOVoropaeva
    AMMukhametshina
    AATokar
    Journal of Magnesium and Alloys, 2021, 9 (04) : 1428 - 1442
  • [38] Microstructures and mechanical properties of pure tantalum processed by high-pressure torsion
    Huang, Y.
    Maury, N.
    Zhang, N. X.
    Langdon, T. G.
    6TH INTERNATIONAL CONFERENCE ON NANOMATERIALS BY SEVERE PLASTIC DEFORMATION (NANOSPD6), 2014, 63
  • [39] Evaluation of dynamic recrystallization behaviors in hot-extruded AA5083 through hot torsion tests
    Kwang-Tae Son
    Ji-Woon Lee
    Taek-Kyun Jung
    Hyun-Jin Choi
    Sang-Wook Kim
    Shae K. Kim
    Young-Ok Yoon
    Soong-Keun Hyun
    Metals and Materials International, 2017, 23 : 68 - 75
  • [40] Effects of calcium on texture and mechanical properties of hot-extruded Mg-Zn-Ca alloys
    Zhang, Baoping
    Wang, Yin
    Geng, Lin
    Lu, Chunxiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 539 : 56 - 60