共 50 条
- [31] Microstructure and formation of micro-arc oxidation coatings of AZ91D magnesium alloys [J]. Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2015, 44 (10): : 2435 - 2439
- [32] The Characteristic of ceramic coatings prepared on magnesium alloy AZ91D by micro-arc oxidization in silicate electrolyte [J]. ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 941 - 947
- [34] Influences of Micro-arc Oxidation on Pre-corroded Fatigue Property of Magnesium Alloy AZ91D [J]. NEW MATERIALS AND ADVANCED MATERIALS, PTS 1 AND 2, 2011, 152-153 : 51 - 57
- [36] EFFECTS OF OXIDATION TIME ON MICRO-ARC OXIDIZED COATINGS OF MAGNESIUM ALLOY AZ91D IN ALUMINATE SOLUTION [J]. MAGNESIUM TECHNOLOGY 2011, 2011, : 537 - 541
- [38] Interaction of heat-treatment and micro-arc oxidation on AZ91D magnesium alloys [J]. Cailiao Yanjiu Xuebao, 2009, 6 (656-662): : 656 - 662
- [39] Quick forming of coating on AZ91D in AC micro-arc oxidation surface treatment [J]. Zhang, P. (pzhang1@bjtu.edu.cn), 2013, Science Press (42):