Thermal degradation and (nano)mechanical behavior of layered silicate reinforced poly(3-hydroxybutyrate-co-3-hydroxyvalerate) nanocomposites

被引:69
|
作者
Bruzaud, Stephane [1 ]
Bourmaud, Alain [1 ]
机构
[1] Univ Bretagne Sud, Lab Polymeres Proprietes Interfaces & Composites, F-56321 Lorient, France
关键词
poly(3-hydroxybutyrate-co-3-hydroxyvalerate); nanocomposites; layered silicates; nanoindentation;
D O I
10.1016/j.polymertesting.2007.04.001
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Poly(3-hydroxybutyrate-co-3-hydroxyvalerate)-based nanocomposites, containing different amounts of organophilic montmorillonite. were prepared using the solution intercalation method. The microstructures of the so-obtained nanocomposites were investigated by wide angle X-ray scattering and their thermal and mechanical properties were studied by means of thermogravimetric analysis, tensile tests, and nanoindentation. The thermal stability and tensile properties were greatly enhanced with only very few percent organoclay. The effect of various loading levels of nanoclay reinforcement on the nanomechanical material properties was also investigated by the nanoindentation technique. The nanoindentation measurements confirm a significant increase of mechanical properties previously observed by tensile tests. (c) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:652 / 659
页数:8
相关论文
共 50 条
  • [21] Thermal and mechanical properties of poly(3-hydroxybutyrate-co-3-hydroxyvalerate)/cellulose nanowhiskers composites
    Ten, Elena
    Turtle, Joel
    Bahr, David
    Jiang, Long
    Wolcott, Michael
    POLYMER, 2010, 51 (12) : 2652 - 2660
  • [22] COCRYSTALLIZATION OF POLY(3-HYDROXYBUTYRATE-CO-3-HYDROXYVALERATE)
    CUESTA, MS
    MARTINEZSALAZAR, J
    BARKER, PA
    BARHAM, PJ
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (19) : 5335 - 5338
  • [23] HYDROLYTIC DEGRADATION OF MICROBIAL POLY(3-HYDROXYBUTYRATE-CO-3-HYDROXYVALERATE) FIBERS
    KANESAWA, Y
    DOI, Y
    MAKROMOLEKULARE CHEMIE-RAPID COMMUNICATIONS, 1990, 11 (12): : 679 - 682
  • [24] MICROBIAL-DEGRADATION OF POLY(3-HYDROXYBUTYRATE) AND POLY(3-HYDROXYBUTYRATE-CO-3-HYDROXYVALERATE) IN SOILS
    MERGAERT, J
    WEBB, A
    ANDERSON, C
    WOUTERS, A
    SWINGS, J
    APPLIED AND ENVIRONMENTAL MICROBIOLOGY, 1993, 59 (10) : 3233 - 3238
  • [25] ENZYMATIC DEGRADATION OF BLENDS CONTAINING POLY(3-HYDROXYBUTYRATE-CO-3-HYDROXYVALERATE)
    MCCARTHY, SP
    DAVE, P
    JAHEDI, T
    EBERIEL, D
    GROSS, R
    POLYMER DEGRADATION AND STABILITY, 1994, 45 (02) : 197 - 203
  • [27] Mechanical and morphological properties of poly(3-hydroxybutyrate)/poly(3-hydroxybutyrate-co-3-hydroxyvalerate) blends
    Conti, Denise Santos
    Pezzin, Sergio Henrique
    Ferreira Coelho, Luiz Antonio
    MACROMOLECULAR SYMPOSIA, 2006, 245 : 491 - 500
  • [28] The Morphology and Degradation Behavior of Electrospun Poly(3-hydroxybutyrate)/Magnetite and Poly(3-hydroxybutyrate-co-3-hydroxyvalerate)/Magnetite Composites
    Ho, Mao-Hsun
    Li, Si-Yu
    Ciou, Chun-Yu
    Wu, Tzong-Ming
    JOURNAL OF APPLIED POLYMER SCIENCE, 2014, 131 (22)
  • [29] Poly(3-Hydroxybutyrate-co-3-Hydroxyvalerate)/Polylactide Blends: Thermal Stability, Flammability and Thermo-Mechanical Behavior
    Idris Zembouai
    Stéphane Bruzaud
    Mustapha Kaci
    Aida Benhamida
    Yves-Marie Corre
    Yves Grohens
    Aurélie Taguet
    José-Marie Lopez-Cuesta
    Journal of Polymers and the Environment, 2014, 22 : 131 - 139
  • [30] Poly(3-Hydroxybutyrate-co-3-Hydroxyvalerate)/Polylactide Blends: Thermal Stability, Flammability and Thermo-Mechanical Behavior
    Zembouai, Idris
    Bruzaud, Stephane
    Kaci, Mustapha
    Benhamida, Aida
    Corre, Yves-Marie
    Grohens, Yves
    Taguet, Aurelie
    Lopez-Cuesta, Jose-Marie
    JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2014, 22 (01) : 131 - 139