Experimental study on the effect of interface fiber orientation and utilized delamination initiation techniques on fracture toughness of glass/epoxy composite laminates

被引:3
|
作者
Nikbakht, Masood [1 ]
Toudeshky, Hossein Hosseini [1 ]
Mohammadi, Bijan [2 ]
机构
[1] Amirkabir Univ Technol, Tehran, Iran
[2] Iran Univ Sci & Technol, Tehran, Iran
关键词
Multidirectional; composite; double cantilever beam; interface fibers angle; acoustic emission; I INTERLAMINAR FRACTURE; MODE-I; PLY ORIENTATION; CRACK-PROPAGATION; ACOUSTIC-EMISSION; BEHAVIOR;
D O I
10.1177/0731684416666402
中图分类号
TB33 [复合材料];
学科分类号
摘要
Critical energy release rate for delamination initiation in composites as a material property, supposed to be independent from non-material variables. However, a thorough literature review presented in this study shows that in many cases it may vary with the variation of layup configuration or geometrical and dimensions. This study is aimed to investigate the effect of interface layers orientation on fracture toughness by eliminating the other influential parameters such as stacking sequence, by selecting the anti-symmetric layup configuration of Double Cantilever Beam, [+/-theta/0(10)/+/-theta](as), in which theta will be 0 degrees, 30 degrees, 45 degrees and 60 degrees. The energy release rates data have been calculated using different criteria and techniques to obtain the load and displacement at initial crack growth and the results were compared with the standard methods. The damage zone near the crack tip is also illustrated before and after the crack propagation by microscopic images of delamination front, and discussed for all investigated interface fiber angles. Experimental results show that the effect of interface layers orientation on fracture toughness of the investigated layup configurations based on the nonlinear technique as a standard procedure is negligible while other techniques show a considerable changes in the calculated energy release rate with the increase of interface layers angle from zero to 60 degrees.
引用
收藏
页码:1722 / 1733
页数:12
相关论文
共 50 条
  • [41] Effect of fiber orientation on interfacial fracture toughness for adhesively bonded composite plates
    Ilkay Ertugrul Bican
    Mete Onur Kaman
    Serkan Erdem
    Journal of Mechanical Science and Technology, 2020, 34 : 757 - 764
  • [42] Mode II Interlaminar Fracture Toughness of Flax/Glass/Epoxy Hybrid Composite Materials: An Experimental and Numerical Study
    Ekeoseye, Wilfred Stephen
    Kolasangiani, Kamal
    Oguamanam, Donatus C. D.
    Bougherara, Habiba
    JOURNAL OF NATURAL FIBERS, 2022, 19 (11) : 4286 - 4300
  • [43] Translaminar Dynamic Fracture Toughness of Aeronautic Grade Composite Laminates Made With Carbon Fiber-Epoxy Resin
    Tarpani, Jose R.
    Gatti, Maria C. A.
    POLIMEROS-CIENCIA E TECNOLOGIA, 2010, 20 : 345 - 351
  • [44] THE EFFECT OF FIBRE ORIENTATION ON FRACTURE PROPERTIES OF GLASS FIBRE-EPOXY COMPOSITE
    Burzic, Meri
    Radakovic, Zoran
    Manjgo, Mersida
    Burzic, Zijah
    STRUCTURAL INTEGRITY AND LIFE-INTEGRITET I VEK KONSTRUKCIJA, 2012, 12 (01): : 35 - 38
  • [45] Interfacial mobility and its effect on interlaminar fracture toughness in glass-fibre-reinforced epoxy laminates
    Wang, TWH
    Blum, FD
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (19) : 5231 - 5238
  • [46] Effect of fiber orientation of adjacent plies on the mode I delamination fracture of carbon fiber reinforced polymer multidirectional laminates
    Liu, Zhe
    Li, Peifeng
    POLYMER COMPOSITES, 2025, 46 (03) : 2560 - 2572
  • [47] Scale Effect on Impact Performance of Unidirectional Glass Fiber Reinforced Epoxy Composite Laminates
    Shen, Yiou
    Jiang, Bing
    Li, Yan
    MATERIALS, 2019, 12 (08)
  • [48] Fatigue Delamination, Initiation, and Growth, Under Mode I and II of Fracture in a Carbon-Fiber Epoxy Composite
    Argueelles, Antonio
    Vina, Jaime
    Canteli, Alfonso F.
    Bonhomme, Jorge
    POLYMER COMPOSITES, 2010, 31 (04) : 700 - 706
  • [49] Effect of fibre orientation on mode-I interlaminar fracture toughness of glass epoxy composites
    Shetty, MR
    Kumar, KRV
    Sudhir, S
    Raghu, P
    Madhuranath, AD
    Rao, RMVG
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2000, 19 (08) : 606 - 620
  • [50] Experimental characterization of interlaminar fracture toughness of composite laminates assembled with three different carbon fiber lamina
    Gentile, Domenico
    FRATTURA ED INTEGRITA STRUTTURALE, 2018, (43): : 155 - 170