Study of the Deburring Process for Low Carbon Steel by Plasma Electrolytic Oxidation

被引:5
|
作者
Li Hongtao [1 ]
Kan Jinfeng [1 ]
Jiang Bailing [1 ]
Liu Yanjie [1 ]
Liu Zheng [2 ]
机构
[1] Nanjing Tech Univ, Coll Mat Sci & Engn, Nanjing 210009, Jiangsu, Peoples R China
[2] Xian Univ Technol, Sch Mat Sci & Engn, Xian 710048, Peoples R China
基金
中国国家自然科学基金;
关键词
plasma electrolytic oxidation; corrosion; deburring; ceramic films; CORROSION-RESISTANCE; COATINGS; MAGNESIUM; ALUMINUM; ALLOYS; PRECISION;
D O I
10.1088/1009-0630/18/8/12
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
In an appropriate electrochemical environment, the discrete thermal electron emission could be induced in the micro area due to the uneven distribution of electron flux on the anode surface. Thus an oxygen molecule could be ionized at the liquid-solid interface after collision, and then oxygen plasma with distribution characteristics would be formed. The plasma electrolytic oxidation (PEO) could happen at the liquid-solid interface. In this work, the low carbon steel was used to study the deburring process by PEO at a high frequency (70000 Hz) pulse DC mode. Its burr height H from 3.23 mm to 0.04 mm was removed to form a smooth surface within 6 min. The values of corrosion potential and current density for the untreated sample were -0.667 V and 6.735x10(-5) A/cm(2), respectively. But for the treated sample, the corrosion potential and current density were relatively lower, -0.354 V and 1.19x10(-7) A/cm(2). Therefore, PEO was expected to be a new deburring method of carbon steel for the material processing field.
引用
收藏
页码:860 / 864
页数:5
相关论文
共 50 条
  • [31] Improvement of Corrosion Resistance on a Low Carbon Steel 1018 in 3.5% NaCl Solution by Electrolytic-Plasma-Process (EPP)
    Liang, Jiandong
    Hossian, Naser I.
    Wahab, Muhammad A.
    Guo, Shengmin
    INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION - 2012, VOL 3, PTS A-C: DESIGN, MATERIALS, AND MANUFACTURING, 2013, : 821 - 825
  • [32] Localized Surface Modification on 1018 Low-Carbon Steel by Electrolytic Plasma Process and its Impact on Corrosion Behavior
    Liang, Jiandong
    Guo, Shengmin
    Wahab, Muhammad A.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (12) : 4187 - 4192
  • [33] Preparation and properties of ceramic coating on Q235 carbon steel by plasma electrolytic oxidation
    Wang, Yunlong
    Jiang, Zhaohua
    Yao, Zhongping
    CURRENT APPLIED PHYSICS, 2009, 9 (05) : 1067 - 1071
  • [34] Systematic study of the electrolytic plasma oxidation process on a Mg alloy for corrosion protection
    Ma, Y
    Nie, X
    Northwood, DO
    Hu, H
    THIN SOLID FILMS, 2006, 494 (1-2) : 296 - 301
  • [35] Increasing Wear Resistance of Low-Carbon Steel by Anodic Plasma Electrolytic Sulfiding
    Mukhacheva, Tatiana
    Kusmanov, Sergei
    Suminov, Igor
    Podrabinnik, Pavel
    Khmyrov, Roman
    Grigoriev, Sergey
    METALS, 2022, 12 (10)
  • [36] Formation of Diffusion Layers by Anode Plasma Electrolytic Nitrocarburizing of Low-Carbon Steel
    Kusmanov, S. A.
    Kusmanova, Yu V.
    Naumov, A. R.
    Belkin, P. N.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (08) : 3187 - 3193
  • [37] Formation of Diffusion Layers by Anode Plasma Electrolytic Nitrocarburizing of Low-Carbon Steel
    S. A. Kusmanov
    Yu. V. Kusmanova
    A. R. Naumov
    P. N. Belkin
    Journal of Materials Engineering and Performance, 2015, 24 : 3187 - 3193
  • [38] Frequency response studies for the plasma electrolytic oxidation process
    Parfenov, E. V.
    Yerokhin, A. L.
    Matthews, A.
    SURFACE & COATINGS TECHNOLOGY, 2007, 201 (21): : 8661 - 8670
  • [39] Optimisation of the plasma electrolytic oxidation process efficiency on aluminium
    Matykina, E.
    Arrabal, R.
    Skeldon, P.
    Thompson, G. E.
    SURFACE AND INTERFACE ANALYSIS, 2010, 42 (04) : 221 - 226
  • [40] Anode plasma electrolytic nitrohardening of medium carbon steel
    Kusmanov, S. A.
    Smirnov, A. A.
    Kusmanova, Yu. V.
    Belkin, P. N.
    SURFACE & COATINGS TECHNOLOGY, 2015, 269 : 308 - 313