Pre-transition oxidation behaviour of pre-hydrided Zircaloy-2

被引:29
|
作者
Oskarsson, M
Ahlberg, E [1 ]
Södervall, U
Andersson, U
Pettersson, K
机构
[1] Univ Gothenburg, Dept Chem, SE-41296 Gothenburg, Sweden
[2] Royal Inst Technol, Dept Mat Sci & Engn, SE-10044 Stockholm, Sweden
[3] Chalmers Univ Technol, Dept Microelect & Nanosci, SE-41296 Gothenburg, Sweden
关键词
D O I
10.1016/S0022-3115(01)00416-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Oxidation tests with hydrogen present in three different states were performed: (i) Hydrogen in solid solution in the zirconium alloy, corresponding to the initial oxidation prior to precipitation of hydrides. (ii) Uniformly distributed hydrides, simulating a situation where hydrides start to precipitate and (iii) massive surface hydride, claimed to be the main cause of accelerated oxidation. The pre-hydrided samples and a reference (REF) sample were oxidised in steam in a static autoclave at 400 degreesC and 10 MPa for 3, 10 and 25 days. The oxide formed was characterised by X-ray diffraction (XRD), transmission electron microscopy (TEM), secondary ion mass spectrometry (SIMS) and electrochemical impedance spectroscopy (EIS). Based on the results obtained, it is concluded that the oxidation of massive zirconium hydride resembles the oxidation of zirconium metal. This fact shows that the commonly observed accelerated oxidation of zirconium alloys cannot be due to an increased oxidation rate of the hydride compared to the metal,but must require a combined effect of, for example interfacial roughness and hydride precipitation. The results are discussed in relation to the mechanism of corrosion and hydriding of zirconium alloys. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:315 / 328
页数:14
相关论文
共 50 条
  • [41] Redistribution of the alloying elements during Zircaloy-2 oxidation
    Cox, B
    Sheikh, HI
    JOURNAL OF NUCLEAR MATERIALS, 1997, 249 (01) : 17 - 32
  • [42] HIGH-TEMPERATURE OXIDATION OF ZIRCALOY-2 AND ZIRCALOY-4 IN STEAM
    URBANIC, VF
    HEIDRICK, TR
    JOURNAL OF NUCLEAR MATERIALS, 1978, 75 (02) : 251 - 261
  • [43] VOLUMETRIC STUDY OF NEMATIC-ISOTROPIC PRE-TRANSITION REGION
    ARMITAGE, D
    PRICE, FP
    PHYSICAL REVIEW A, 1977, 15 (06): : 2496 - 2500
  • [44] NATURE OF THERMAL PRE-TRANSITION OF SYNTHETIC PHOSPHOLIPIDS - DIMYRISTOYLLECITHIN AND DIPALMITOYLLECITHIN
    JANIAK, MJ
    SMALL, DM
    SHIPLEY, GG
    BIOCHEMISTRY, 1976, 15 (21) : 4575 - 4580
  • [45] Pre-transition and pseudo-elasticity in NiTi(Fe) alloy
    Shen, Huimin
    Hu, Meishen
    Gui, Jianmin
    Yuan, Fang
    Wang, Yening
    Guo, Jinfang
    Qian, Dongfan
    Jinshu Xuebao/Acta Metallurgica Sinica, 1988, 24 (02):
  • [46] Pre-transition phenomena in TGS crystal under microwave irradiation
    Ovchinnikova, GI
    Pirogov, YA
    Golikov, FV
    Merinov, VV
    CONFERENCE DIGEST OF THE 2004 JOINT 29TH INTERNATIONAL CONFERENCE ON INFRARED AND MILLIMETER WAVES AND 12TH INTERNATIONAL CONFERENCE ON TERAHERTZ ELECTRONICS, 2004, : 351 - 352
  • [47] OXIDATION OF ZIRCALOY-2 AND ZIRCALOY-3A AT 300 TO 850-DEGREES C
    GULBRANSEN, EA
    ANDREW, KF
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1958, 212 : 281 - 286
  • [48] Oxidation of Zircaloy-2 and Zircaloy-4 in water and lithiated water at 360°C
    Oskarsson, M
    Ahlberg, E
    Pettersson, K
    JOURNAL OF NUCLEAR MATERIALS, 2001, 295 (01) : 97 - 108
  • [49] PRE-TRANSITION BEHAVIOR NEAR RAYLEIGH-BENARD INSTABILITY
    CLARK, NA
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1977, 22 (01): : 70 - 70
  • [50] Effect of pre-transition stimulus duration on acoustic change complex
    Ganapathy, M. K.
    Narne, Vijay Kumar
    Kalaiah, Mohan Kumar
    Manjula, P.
    INTERNATIONAL JOURNAL OF AUDIOLOGY, 2013, 52 (05) : 350 - 359