Microstructure and ablation behavior of C/C-HfC composites prepared by precursor infiltration and pyrolysis

被引:94
|
作者
Xue, Liang [1 ]
Su, Zhe-an [1 ]
Yang, Xin [1 ]
Huang, Dong [1 ]
Yin, Teng [1 ]
Liu, Chunxuan [1 ]
Huang, Qizhong [1 ]
机构
[1] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
Ceramic matrix composites; SEM; High temperature corrosion; CARBON/CARBON COMPOSITES; ZIRCONIUM CARBIDE; HAFNIUM CARBIDE; OXYACETYLENE FLAME; SIC INTERPHASE; OXIDATION; RESISTANCE;
D O I
10.1016/j.corsci.2015.01.053
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
C/C-HfC composites were prepared by precursor infiltration and pyrolysis using HfC precursor. The microstructure, mechanical properties, and ablation behavior were investigated. The C/C-HfC composites showed good ablation resistance with a surface temperature over 2573 K during ablation. The ablation process was divided into two steps, with the ablation rate dominated by various mechanisms. During ablation, tree-coral-like HfO2 particles formed and functioned as thermal barrier, and the HfCxOy phase acted as oxygen diffusion barrier, protecting the composites from further ablation. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:165 / 170
页数:6
相关论文
共 50 条
  • [41] Microstructure and ablation property of C/C-ZrC-SiC composites fabricated by chemical liquid-vapor deposition combined with precursor infiltration and pyrolysis
    He, Qinchuan
    Li, Hejun
    Wang, Changcong
    Zhou, Huashan
    Lu, Jinhua
    CERAMICS INTERNATIONAL, 2019, 45 (03) : 3767 - 3781
  • [42] Microstructure and Ablation Behavior of W/ZrC/SiC Coating on C/C Composites Prepared by Reactive Melt Infiltration and Atmospheric Plasma Spraying
    Zhou, Zhe
    Niu, Furong
    Hu, Xiangfen
    Yang, Xianfeng
    Liu, Peng
    Zhang, Long
    Fan, Xizhi
    Mao, Weiguo
    Zhang, Bei
    Sun, Zexu
    Yi, Maozhong
    ADVANCED ENGINEERING MATERIALS, 2021, 23 (06)
  • [43] ABLATION BEHAVIOR OF HfC COATING PREPARED BY SUPERSONIC PLASMA SPRAYING FOR SiC-COATED C/C COMPOSITES
    Yang, Yang
    Li, Kezhi
    Li, Hejun
    ADVANCED COMPOSITES LETTERS, 2015, 24 (05) : 113 - 118
  • [44] Microstructure and ablation resistance of C/C-HfC-SiC composites prepared by RMI with different powder particle sizes
    Liu, Zhiqiang
    Sun, Yifan
    Zhang, Shubo
    Wang, Yawen
    Tang, Luncheng
    Li, Tian
    Fu, Qiangang
    Jia, Yujun
    MATERIALS CHARACTERIZATION, 2024, 218
  • [45] Effect of mullite content on microstructure and ablation behavior of mullite modified C/C-SiC-HfC composites
    Tan, Qing
    Jiao, Xiaoyang
    He, Qinchuan
    Wang, Yiqun
    Yin, Xuemin
    CORROSION SCIENCE, 2023, 222
  • [46] High-temperature mechanical properties and microstructure of C/C-ZrC-SiC-ZrB2 composites prepared by a joint process of precursor infiltration and pyrolysis and slurry infiltration
    Jia, Yan
    Chen, Si'an
    Li, Yong
    Wang, Song
    Hu, Haifeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 811
  • [47] Microstructure and ablation performance of SiC-ZrC coated C/C composites prepared by reactive melt infiltration
    Zhou, Zhe
    Sun, Zexu
    Ge, Yicheng
    Peng, Ke
    Ran, Liping
    Yi, Maozhong
    CERAMICS INTERNATIONAL, 2018, 44 (07) : 8314 - 8321
  • [48] Microstructure and ablation behaviour of C/C-SiC-ZrC-Cu composites prepared by reactive melt infiltration
    Wang, Shuai
    Yin, Jian
    Xiefeng, Minyu
    Tang, Lei
    Xiong, Xiang
    Zhang, Hongbo
    Wen, Qingbo
    Ma, Denghao
    Zuo, Jinglv
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [49] Preparation of C/SiBCN composites by precursor infiltration and pyrolysis using a novel precursor
    Jia, Yan
    Ji, Xiaoyu
    Chen, Si'an
    Gou, Yanzi
    Li, Yong
    Hu, Haifeng
    MATERIALS RESEARCH EXPRESS, 2019, 6 (06):
  • [50] Comparison of microstructure and ablation behavior of Si-Mo-Ti/Al/Zr infiltrated C/C composites prepared at different infiltration temperature
    Hao, Zhenhua
    Sun, Wei
    Xiong, Xiang
    Xu, Yonglong
    Chang, Yabin
    Peng, Zheng
    Chen, Zhaoke
    Wang, Yalei
    CERAMICS INTERNATIONAL, 2017, 43 (02) : 2765 - 2773