Metal injection molding of W-Ni-Fe microcutters

被引:0
|
作者
Huang, Ming-Shyan [1 ]
Chung, Chin-Feng
机构
[1] Natl Kaohsiung First Univ Sci & Technol, Dept Mech & Automat Engn, Kaohsiung 811, Taiwan
关键词
metal injection molding; MIM; sintering; Taguchi method; W-Ni-Fe alloy powder; TUNGSTEN HEAVY ALLOYS; MECHANICAL-PROPERTIES; PARTS; MIM; DISTORTION; POLYMER;
D O I
10.1515/POLYENG.2011.074
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
This investigation applies metal injection molding (MIM) to fabricate precise microcutters from W-Ni-Fe alloy powder. The hard and brittle W-Ni-Fe alloy is difficult to machine, and MIM must be applied to produce near net-shaped products. MIM involves the injection molding of feedstock by blending metal powder and binders, debinding, and sintering. Liquid-phase sintering is commonly adopted to improve the density and mechanical properties of the sintered parts, but it is inferior in terms of dimensional stability. This study elucidates the dimensional stability of sintered parts made from W-Ni-Fe alloy feedstocks that contain 83 and 93 wt% W. The powder injection molding of microcutters that demand micrometer-scale precision is considered as an example. The Taguchi method is utilized to optimize injection molding and sintering parameters, effectively optimizing the dimensional stability and mechanical properties. Experimental results show that (1) feedstock with 93 wt% W exhibited little and consistent shrinkage (25%-26%); (2) the optimal injection molding parameters determined by the Taguchi method yield an eccentricity of over 18 %, and (3) in the sintering process, low heating rate significantly improves dimensional stability. The average hardness of microcutters, sintered at various heating rates, ranges from Vickers hardness 446 to 452.
引用
收藏
页码:361 / 367
页数:7
相关论文
共 50 条
  • [41] 高Ni/Fe比W-Ni-Fe系重合金烧结行为
    黄继华
    张立春
    桂晓峰
    工程科学学报, 2000, (02) : 149 - 152
  • [42] Aging behaviors of W-Ni-Fe ternary alloys with high Ni-To-Fe ratios
    Li, RH
    Huang, JH
    Yin, S
    Zhao, J
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2003, 19 (06) : 631 - 633
  • [43] Sintering of Tungsten and Tungsten Heavy Alloys of W-Ni-Fe and W-Ni-Cu: A Review
    Senthilnathan, N.
    Annamalai, A. Raja
    Venkatachalam, G.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2017, 70 (05) : 1161 - 1176
  • [44] Magnetic properties of Fe-50%Ni alloy fabricated by metal injection molding
    Ma, Jidong
    Qin, Mingli
    Zhang, Lin
    Zhang, Ruijie
    Tian, Lusha
    Zhang, Xiaofeng
    Li, Xingquan
    Qu, Xuanhui
    Khan, Dil Faraz
    MATERIALS & DESIGN, 2013, 51 : 1018 - 1022
  • [45] 高抗弯强度W-Ni-Fe粉末压坯
    金公
    兵器材料科学与工程, 1992, (02) : 9 - 9
  • [46] Characteristics of high energy milled W-Ni-Fe nanocomposite powders
    Fan, J.L.
    Huang, B.Y.
    Qu, X.H.
    Zhao, M.Y.
    2001, Rare Metals Materials and Engineering Press (30):
  • [47] Mn对W-Ni-Fe合金性能的影响
    李文超
    曹顺华
    张秀芳
    谢继峰
    硬质合金, 2009, 26 (01) : 10 - 14
  • [48] Synthesis of W-Ni-Fe nanostructured and amorphous materials by mechanical alloying
    Zhang, ZW
    Chen, GL
    Chen, G
    Zhou, JG
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 (07) : 1139 - 1143
  • [49] Penetration performance of W-Ni-Fe alloy shaped charge liner
    Liu, J. (liujinxu@bit.edu.cn), 1600, Science Press (42):
  • [50] Penetration of tungsten grain boundaries by a liquid W-Ni-Fe matrix
    Fredriksson, H.
    Eliasson, A.
    Ekbom, L.
    International Journal of Refractory Metals and Hard Materials, 13 (04):