Effect of Mg and Sr additions on the formation of intermetallics in Al-6 wt pct Si-3.5 wt pct Cu-(0.45) to (0.8) wt pct Fe 319-type alloys

被引:103
|
作者
Samuel, FH [1 ]
Ouellet, P
Samuel, AM
Doty, HW
机构
[1] Univ Quebec, Dept Appl Sci, Chicoutimi, PQ G7H 2B1, Canada
[2] Montupet Ltee, Riviere Beaudette, PQ J0P 1R0, Canada
[3] GM Corp, GM Powertrain MCT, Milford, NH 03055 USA
关键词
D O I
10.1007/s11661-998-0194-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-Si alloys are materials that have been developed over the years to meet the increasing demands of the automotive industry for smaller, lighter-weight, high-performance components. An important alloy in this respect is the 319 alloy, wherein silicon and copper are the main alloying elements, and magnesium is often added in automotive versions of the alloy for strengthening purposes. The mechanical properties are also ameliorated by modifying the eutectic silicon structure (strontium being commonly employed) and by reducing the harmful effect of the beta-Al5FeSi iron intermetallic present in the cast structure. Magnesium is also found to refine the silicon structure. The present study was undertaken to investigate the individual and combined roles of Mg and Sr on the morphologies of Si, Mg,Si, and the iron and copper intermetallics likely to form during the solidification of 319-type alloys at very slow (close to equilibrium) cooling rates. The results show that magnesium leads to the precipitation of Al8Mg3FeSi6, Mg2Si, and Al5Mg8Cu2Si6 intermetallics. With a strontium addition, dissolution of a large proportion of the needle-like beta-Al5FeSi intermetallic in the aluminum matrix takes place; no transformation of this phase into any other intermetallics (including the Al-15(Fe,Mn)(3)Si-2 phase) is observed. When both Mg and Sr are added, the diminution of the beta-Al5FeSi phase is enhanced, through both its dissolution in the aluminum matrix as well as its transformation into Al8Mg3FeSi6. The reactions and phases obtained have been analyzed using thermal analysis, optical microscopy, image analysis, and electron microprobe analysis (EMPA) coupled with energy-dispersive X-ray (EDX) analysis.
引用
收藏
页码:2871 / 2884
页数:14
相关论文
共 37 条
  • [31] Effect of cooling rate and Sr-modification on porosity and Fe-intermetallics formation in Al-6.5% Si-3.5% Cu-Fe alloys
    Samuel, AM
    Pennors, A
    Villeneuve, C
    Samuel, FH
    Doty, HW
    Valtierra, S
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2000, 13 (04) : 231 - 253
  • [32] Characterization and Formation of Rod-Shaped (Al,Si)3Ti Particles in an Al-7Si-0.35Mg-0.12Ti (Wt Pct) Alloy
    Xiang Gao
    Yuman Zhu
    Mark A. Easton
    Barbara Rinderer
    Mal Couper
    Jian-Feng Nie
    Metallurgical and Materials Transactions A, 2015, 46 : 3723 - 3731
  • [33] Characterization and Formation of Rod-Shaped (Al,Si)3Ti Particles in an Al-7Si-0.35Mg-0.12Ti (Wt Pct) Alloy
    Gao, Xiang
    Zhu, Yuman
    Easton, Mark A.
    Rinderer, Barbara
    Couper, Mal
    Nie, Jian-Feng
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (08): : 3723 - 3731
  • [34] Kinetic Effect-Dependent Seaweed Formation in Single-Crystal Al-2 Wt Pct Si Alloy by Laser Surface Remelting
    Wang, Yumin
    Li, Shuangming
    Cao, Cong
    Liu, Zhongli
    Xing, Hui
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2024, 55 (02): : 491 - 499
  • [35] Kinetic Effect-Dependent Seaweed Formation in Single-Crystal Al-2 Wt Pct Si Alloy by Laser Surface Remelting
    Yumin Wang
    Shuangming Li
    Cong Cao
    Zhongli Liu
    Hui Xing
    Metallurgical and Materials Transactions A, 2024, 55 : 491 - 499
  • [36] The Effect of Small Additions of Fe and Heavy Deformation on the Precipitation in an Al-1.1Mg-0.5Cu-0.3Si At. Pct Alloy
    Thronsen, Elisabeth
    Morkeseth, Hanne
    Marioara, Calin D.
    Minakuchi, Kazuhiro
    Katsumi, Tetsuya
    Marthinsen, Knut
    Matsuda, Kenji
    Holmestad, Randi
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2022, 53 (09): : 3296 - 3310
  • [37] The Effect of Small Additions of Fe and Heavy Deformation on the Precipitation in an Al–1.1Mg–0.5Cu–0.3Si At. Pct Alloy
    Elisabeth Thronsen
    Hanne Mørkeseth
    Calin D. Marioara
    Kazuhiro Minakuchi
    Tetsuya Katsumi
    Knut Marthinsen
    Kenji Matsuda
    Randi Holmestad
    Metallurgical and Materials Transactions A, 2022, 53 : 3296 - 3310