Industrial semi-solid casting trials of aluminum A356 brake calipers were performed over five days with the CSIR-RCS and high-pressure die casting process cell. Consecutive visual passed castings were used as the measure of process stability, and common defects between trials were categorized. Short fill results are erratic and caused by unintended underdosing by the furnace or incomplete billet discharge at the delivery point in the shot sleeve. Cold shuts can be significantly reduced by adjusting the shot control profile. Surface finish defects include surface roughness and staining caused by lubricant burn off. Visual passed castings display none of the above-mentioned external defects. X-ray examination and pressure testing of heat-treated castings from the consecutive visual passed castings show improvement over the five days. These initial-stage industrialization efforts pave the way for process commercialization.
引用
收藏
页数:5
相关论文
共 50 条
  • [31] Mechanical properties improvement of semi-solid state joining of aluminum alloys SSM A356
    Geaowdee, Atsadawoot
    Muangjunburee, Prapas
    Key Engineering Materials, 2015, 658 : 146 - 150
  • [32] Preparation of A356 aluminum alloy semi-solid slurry by damper cooling tube method
    School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
    不详
    Tezhong Zhuzao Ji Youse Hejin, 2007, 3 (188-191):
  • [33] Semi-solid rheocasting of grain refined aluminum alloy 7075
    U.A.CURLE
    G.GOVENDER
    Transactions of Nonferrous Metals Society of China, 2010, 20(S3) (S3) : 832 - 836
  • [34] Semi-solid rheocasting of grain refined aluminum alloy 7075
    Curle, U. A.
    Govender, G.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S832 - S836
  • [35] The influence of induction heating on the microstructure of A356 for semi-solid forging
    Choi, JC
    Park, HJ
    Kim, BM
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1999, 87 (1-3) : 46 - 52
  • [36] Effect of yttrium on the microstructure of a semi-solid A356 Al alloy
    Liu Zheng
    Hu Yongmei
    RARE METALS, 2008, 27 (05) : 536 - 540
  • [37] A Compound Process Preparing Semi-Solid A356 Alloy Slurry
    Liu, Zheng
    Mao, Wei Min
    MANUFACTURING SCIENCE AND ENGINEERING, PTS 1-5, 2010, 97-101 : 1003 - +
  • [38] Effect of yttrium on the microstructure of a semi-solid A356 Al alloy
    LIU Zheng and HU Yongmei Faculty of Material and Chemical Engineering
    Rare Metals, 2008, (05) : 536 - 540
  • [39] Study on Thixotropic Property of A356 Alloy in Semi-Solid State
    Simlandi, Sudip
    Barman, Nilkanta
    Chattopadhyay, Himadri
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES XII, 2013, 192-193 : 335 - 340
  • [40] SEMI-SOLID A356 ALLOY SLURRY PREPARED BY A NEW PROCESS
    Liu Zheng
    Mao Wei-min
    Zhao Zhenduo
    ACTA METALLURGICA SINICA, 2009, 45 (04) : 507 - 512