Influence of stabilizers on photo-oxidative degradation of SWy-1/poly (ethylene oxide) composite films

被引:2
|
作者
Lombardo, Patricia Coelho [1 ]
Poli, Alessandra Lima [2 ]
Schmitt, Carla Cristina [2 ]
机构
[1] Univ Sao Paulo, Escola Engn Sao Carlos, Dept Mat Engn, Sao Carlos, SP, Brazil
[2] Univ Sao Paulo, Inst Quim Sao Carlos, Sao Carlos, SP, Brazil
来源
POLIMEROS-CIENCIA E TECNOLOGIA | 2015年 / 25卷 / 01期
关键词
poly (ethylene oxide); montmorillonite; photostabilizers; photooxidative degradation; WATER-SOLUBLE POLYMERS; POLY(ETHYLENE OXIDE); POLYPROPYLENE/MONTMORILLONITE NANOCOMPOSITES; OXIDATIVE-DEGRADATION; UV-IRRADIATION; PHOTODEGRADATION; CLAY; PHOTOTRANSFORMATION; MONTMORILLONITE; BLENDS;
D O I
10.1590/0104-1428.1604
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Poly(ethylene oxide) (PEO) with SWy-1 montmorillonite and stabilizers (2-hydroxybenzophenone and tinuvin 770) composites were prepared by intercalation in solution method. The films of the composites were exposed to UV irradiation. The photodegradation products were monitored by FTIR (Fourier Transform Infrared Spectroscopy) and SEC (Size Exclusion Chromatography) method. The PEO pure showed higher degradation rate coefficients, k(d), compared to the others samples. The system that showed the lowest value for the degradation rate coefficients (k(d) = 1.9 x 10(-6) mol g(-1) h(-1)) was the PEO/SWy-1 5% composite with 0.25% of tinuvin 770. In this case, the stabilization of the PEO matrix can be attributed to clay associated with tinuvin 770. The clay scatters and absorbs UV irradiation and tinuvin acts as a stabilizer of the HALS (hindered amine light stabilizers) kind.
引用
收藏
页码:101 / 108
页数:8
相关论文
共 50 条
  • [21] Photo-oxidative Degradation and Biodegradation of Poly(ether-block-amide) Multiblock Copolymers
    An, Yingjun
    Padermshoke, Adchara
    Nguyen, Thinh Van
    Masunaga, Hiroyasu
    Yokoyama, Risa
    Yonemura, Maina
    Kato, Dai-ichiro
    Kobayashi, Yutaka
    Ito, Hiroshi
    Sasaki, Sono
    Takahara, Atsushi
    ACS APPLIED POLYMER MATERIALS, 2024, 6 (10): : 6140 - 6149
  • [22] Photo-oxidative degradation of poly(p-dioxanone) under ultraviolet light source
    Liang, Bingqing
    Pang, Daolin
    Jin, Chao
    Li, Fang
    Wang, Yuzhong
    POLYMER DEGRADATION AND STABILITY, 2012, 97 (11) : 2162 - 2169
  • [23] A fundamental study on photo-oxidative degradation of linear low density polyethylene films at embrittlement
    Hsu, Yu-Chieh
    Weir, Michael P.
    Truss, Rowan W.
    Garvey, Christopher J.
    Nicholson, Timothy M.
    Halley, Peter J.
    POLYMER, 2012, 53 (12) : 2385 - 2393
  • [24] Photo-oxidative degradation mechanisms in styrene-ethylene-butadiene-styrene (SEBS) triblock copolymer
    Luengo, C
    Allen, NS
    Edge, M
    Wilkinson, A
    Parellada, MD
    Barrio, JA
    Santa, VR
    POLYMER DEGRADATION AND STABILITY, 2006, 91 (04) : 947 - 956
  • [25] INHIBITIVE EFFECTS OF TRANSITION-METAL THIOPICOLINE ANILIDES ON THE PHOTO-OXIDATIVE DEGRADATION OF POLY(2,6-DIMETHYL-1,4-PHENYLENE OXIDE) FILMS
    CHANDRA, R
    EUROPEAN POLYMER JOURNAL, 1981, 17 (05) : 567 - 571
  • [26] Influence of the photo-oxidative degradation on the water barrier and corrosion protection properties of polyester paints
    Deflorian, F
    Fedrizzi, L
    Bonora, PL
    CORROSION SCIENCE, 1996, 38 (10) : 1697 - 1708
  • [27] The effect of comonomer concentration and distribution on the photo-oxidative degradation of linear low density polyethylene films
    Hsu, Yu-Chieh
    Truss, Rowan W.
    Laycock, Bronwyn
    Weir, Michael P.
    Nicholson, Timothy M.
    Garvey, Christopher J.
    Halley, Peter J.
    POLYMER, 2017, 119 : 66 - 75
  • [28] PHOTO-STABILIZING EFFECT OF NI COMPOUNDS IN PHOTO-OXIDATIVE DEGRADATION OF CIS-1,4-POLY(BUTADIENE)
    LALA, D
    RABEK, JF
    POLYMER DEGRADATION AND STABILITY, 1981, 3 (05) : 383 - 396
  • [29] Degradation of Poly(Ethylene Oxide) Films Using Crystal Violet
    da Silva, Thalena Lima
    de Araujo, Francisca Pereira
    da Silva Filho, Edson Cavalcanti
    Furtini, Marcelo Barbosa
    Osajima, Josy Anteveli
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2017, 20 : 869 - 872
  • [30] Application of spectroscopic ellipsometry to probe the environmental and photo-oxidative degradation of poly(p-phenylenevinylene) (PPV)
    Kumar, S
    Biswas, AK
    Shukla, VK
    Awasthi, A
    Anand, RS
    Narain, J
    SYNTHETIC METALS, 2003, 139 (03) : 751 - 753