摘要
Behavior of slag foaming was investigated under the condition of iron oxide reduction by graphite in CaO-Li2O-SiO2-Al2O3 slag systems. Experiments were carried out at 1573 K, under Ar gas atmosphere with a flow rate of 1000 N cm(3)/min. The SiO2 molar fraction of the primary slag was varied between 0.33 and 0.49. The initial concentration of iron oxide in the molten slag was varied between 3 and 15 mass%. The content of sulfur ranged from 0 to 0.68 mass%. The rotation speed of graphite rod was kept constant at 1.67 s(-1). The slag foaming is evaluated by the ratio of the volume of the gas contained in slag to the total volume of foaming slag, namely gas holdup, epsilon. The slag foaming is mainly affected by the CO gas evolution rate. The slag is not foamed when the CO gas evolution rate is less than a critical value. Then with the increase in CO gas evolution rate, the slag foaming becomes vigorous and approaches to a plateau value. Addition of sulfur suppresses the slag foaming and silica favors slag foaming a little. A simple fluid mechanics model, called drift-flux analysis, can be used to fit the present experimental results.
引用
收藏
页码:1339 / 1345
页数:7
相关论文
共 50 条
  • [1] EFFECT OF SLAG FOAMING ON THE REDUCTION OF IRON-OXIDE IN MOLTEN SLAG BY GRAPHITE
    BAFGHI, MS
    KURIMOTO, H
    SANO, M
    ISIJ INTERNATIONAL, 1992, 32 (10) : 1084 - 1090
  • [2] Foaming during reduction of iron oxide in molten slag
    Jouhari, AK
    Galgali, RK
    Datta, P
    Bhattacharjee, S
    Gupta, RC
    Ray, HS
    IRONMAKING & STEELMAKING, 2000, 27 (01) : 27 - 31
  • [3] REDUCTION BEHAVIOR OF CHROMIUM AND IRON OXIDE IN MOLTEN STAINLESS STEEL SLAG WITH GRAPHITE
    Li Qiu-ju
    Lin Jiang-duo
    Liu Zhi-peng
    Hong Xin
    TMS 2010 139TH ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 1: MATERIALS PROCESSING AND PROPERTIES, 2010, : 481 - 487
  • [4] Effect of gas injection on the behavior of slag foaming with smelting reduction of iron oxide by graphite
    Hong, L
    Hirasawa, M
    Sano, M
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2000, 19 (3-4) : 165 - 175
  • [5] Behavior of slag foaming caused by blowing gas in molten slags
    Wu, K
    Qian, W
    Chu, SJ
    Niu, Q
    Luo, HW
    ISIJ INTERNATIONAL, 2000, 40 (10) : 954 - 957
  • [6] REDUCTION OF MOLTEN IRON OXIDE-BASED SLAGS BY SOLID GRAPHITE
    HARA, S
    OGINO, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1990, 76 (03): : 360 - 367
  • [7] FOAMING OF MOLTEN SLAGS CONTAINING IRON OXIDE.
    Hara, Shigeta
    Ikuta, Masahisa
    Kitamura, Mitsuaki
    Ogino, Kazumi
    Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan, 1983, 69 (09): : 1152 - 1159
  • [8] EFFECT OF SLAG COMPOSITION ON THE KINETICS OF THE REDUCTION OF IRON-OXIDE IN MOLTEN SLAG BY GRAPHITE
    BAFGHI, MS
    ITO, Y
    YAMADA, S
    SANO, M
    ISIJ INTERNATIONAL, 1992, 32 (12) : 1280 - 1286
  • [9] BEHAVIOR OF IRON(III) OXIDE IN METALLOTHERMIC REDUCTION OF MOLTEN ZINCIFEROUS SLAGS
    SANNIKOV, YI
    SEREBRYA.GA
    ABDEEV, YM
    MAKAREVI.SP
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY,USSR, 1972, 46 (03): : 471 - &
  • [10] Reduction behavior of chromium oxide in molten slag using aluminum, ferrosilicon and graphite
    Shibata, E
    Egawa, S
    Nakamura, T
    ISIJ INTERNATIONAL, 2002, 42 (06) : 609 - 613