INFLUENCE OF DEFORMATION ON MICROSTRUCTURE OF TI-15V-3CR-3SN-3AL ALLOY

被引:0
|
作者
Spotz, Zdenek [1 ]
Leemet, Tonu [2 ]
Rokicki, Pawel [1 ]
Fusova, Lenka [1 ]
Saksl, Karel [1 ]
Kuokkala, Veli-Tapani [2 ]
Siemers, Carsten [3 ]
机构
[1] Slovak Acad Sci, Inst Mat Res, Watsonova 47, Kosice, Slovakia
[2] Tampere Univ Technol, Dept Mat Sci, Tampere, Finland
[3] Tech Univ Carolo Wilhelmina Braunschweig, Inst Werkstoffe, Braunschweig, Germany
关键词
Titanium alloy; Ti15V-3Cr-3Sn-3Al; hopkinson split pressure bar; phase analysis; lattice parameter; grain size;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Titanium and its alloys are widely used in industrial applications due to their attractive properties. Ti-15V-3Cr-3Al-3Sn, a solute-rich, precipitation hardenable, beta titanium alloy shows a unique combination of low density, high strength, ductility, and corrosion resistance. During the production of semi-finished parts, several deformation steps (e. g., rolling or forging) are necessary, leading to different microstructures and properties especially at the rod ends. The aim of the current study is therefore to investigate the microstructure-property relationships of Ti-15V-3Cr-3Al-3Sn exposed to deformation at different strain rates and temperatures. Samples of Ti-15V-3Cr-3Al-3Sn alloy have been deformed in quasi-static and Hopkinson Split Pressure Bar experiments between room temperature and 900 degrees C at strain rates between 10(-3)s(-1) and 10(3)s(-1). The resulting microstructures were investigated by means of optical microscopy, scanning electron microscopy and hard x-ray diffraction. In addition, the hardness of the samples was investigated. The size and shape of grains were determined and compared with the undeformed state. The microstructure and properties strongly depend on the initial experiment temperature and strain rate. The highest increase of lattice parameter has been observed at low strain rates and low temperature, which has been identified by the x-ray diffraction analyses.
引用
收藏
页码:838 / 843
页数:6
相关论文
共 50 条
  • [41] Grain refinement and superplastic flow in friction stir processed Ti-15V-3Cr-3Sn-3Al alloy
    Zhang, Wenjing
    Liu, Huihong
    Ding, Hua
    Fujii, Hidetoshi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 803 : 901 - 911
  • [42] Ti-15V-3Cr-3Sn-3Al合金中的相变研究
    王世洪
    沈桂琴
    梁佑明
    材料工程, 1992, (S1) : 175 - 177
  • [43] Ti-15V-3Cr-3Sn-3Al合金的高温变形行为
    吴全兴
    钛工业进展, 1997, (04) : 18 - 18
  • [44] Relationships between Spring-back and Microstructure of Ti-15V-3Cr-3Sn-3Al Titanium Alloy Sheet during Bending Process
    Li, Linlin
    Wu, Guoqing
    Liu, Changxu
    Sha, Aixue
    HIGH PERFORMANCE STRUCTURE MATERIALS, 2013, 747-748 : 839 - +
  • [45] EFFECT OF QUENCHED-IN VACANCIES ON AGED MICROSTRUCTURES IN TI-15V-3CR-3SN-3AL
    FUJII, H
    SUZUKI, HG
    MATERIALS TRANSACTIONS JIM, 1993, 34 (04): : 382 - 388
  • [46] ACCELERATION OF ALPHA-PRECIPITATION AND STRENGTHENING OF TI-15V-3CR-3SN-3AL ALLOY BY 2 STEP AGING
    OKADA, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1990, 76 (04): : 614 - 621
  • [47] UNRECRYSTALLIZED GRAINS APPEARING IN TI-15V-3CR-3SN-3AL HOT ROLLED SHEET
    TAKATORI, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (13): : 1633 - 1633
  • [48] WORKABILITY AND HEAT-TREATMENT CHARACTERISTICS OF BETA-TITANIUM ALLOY, TI-15V-3CR-3SN-3AL
    TSUMORI, Y
    MATSUMOTO, T
    KOYAMA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (06): : 603 - 609
  • [49] Fracture Toughness of Ti-15V-3Cr-3Sn-3Al Titanium Alloy in Different Heat-Treated Conditions
    Manikandan, P.
    Kumar, K. Naresh
    Rao, G. Sudarshan
    Jha, Abhay K.
    Narayanan, P. Ramesh
    Pant, Bhanu
    Cherian, Roy M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (06) : 1507 - 1510
  • [50] High-temperature oxidation of a Ti-15V-3Cr-3Sn-3Al alloy in CO2 atmosphere
    Kusabiraki, K
    Fukuda, Y
    Saji, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (03): : 132 - 137