Influences of the quantity of Mg2Sn phase on the corrosion behavior of Mg-7Sn magnesium alloy

被引:131
|
作者
Liu, Xianbin [1 ]
Shan, Dayong [1 ]
Song, Yingwei [1 ]
Chen, Rongshi [1 ]
Han, Enhou [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, State Key Lab Corros & Protect, Shenyang 110016, Liaoning, Peoples R China
关键词
Mg2Sn phase; Mg-7Sn alloy; Corrosion mode; Solution temperature; Stannic oxide; SN; AZ91; MICROSTRUCTURE; ZN;
D O I
10.1016/j.electacta.2010.12.030
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The influence of the quantity of the Mg2Sn phase on the corrosion behavior of different solution temperature treated Mg-7Sn magnesium alloy has been investigated by electrochemical measurements, scanning electron microscope (SEM) observation, X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) analysis. With the increase of solution temperature, the quantity of Mg2Sn phase decreased and the tin concentration of matrix increased. The dissolved tin in Mg matrix took part in the film formation and the constituent of film was magnesium oxide and stannic oxide. The corrosion mode and corrosion rate were associated with the quantity of Mg2Sn phases and tin concentration of the matrix. If most of tin was present as Mg2Sn, the corrosion mode was pitting corrosion and it accelerated the corrosion rate. If most of tin was dissolved in matrix, the corrosion mode was filiform corrosion and it decreased the corrosion rate. The experiment evidences demonstrated that the corrosion resistance can be improved by increasing the tin concentration of matrix and the lowest corrosion rate was observed for sample solution treated at 540 degrees C. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2582 / 2590
页数:9
相关论文
共 50 条
  • [21] Characterization and interpretation of interfacial structure of the Mg2Sn laths in an Mg-Sn-Mn-Ag-Zn alloy
    Huang, X. -F.
    Zhang, W. -Z.
    PHILOSOPHICAL MAGAZINE LETTERS, 2014, 94 (04) : 251 - 259
  • [22] Crystallography of Mg2Sn precipitates with two newly observed orientation relationships in an Mg-Sn-Mn alloy
    Shi, Z. -Z.
    Dai, F. -Z.
    Zhang, W. -Z.
    MATERIALS SCIENCE AND TECHNOLOGY, 2012, 28 (04) : 411 - 414
  • [23] Corrosion behavior of Mg-Mn-Ca alloy: Influences of Al, Sn and Zn
    Bahmani, Ahmad
    Arthanari, Srinivasan
    Shin, Kwang Seon
    JOURNAL OF MAGNESIUM AND ALLOYS, 2019, 7 (01) : 38 - 46
  • [24] Influence of atomic ratio of Mg to Sn on thermoelectric properties of Mg2Sn films
    Liu, Ying
    Song, Guihong
    Tai, Kaiping
    Yu, Zhi
    Ran, Yijun
    He, Juan
    Wu, Yusheng
    Thin Solid Films, 2025, 809
  • [25] Remarkable age-hardening response and microstructural evolution of Mg-7Sn alloy
    Tong, Lin
    Jiang, Jing
    Bi, Guangli
    Xu, Zuocheng
    Li, Yuandong
    Chen, Tijun
    Zhang, Xiaoru
    Fu, Wei
    Fang, Daqing
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 24 : 1442 - 1453
  • [26] Effects of Ca, Ag addition on the microstructure and age-hardening behavior of a Mg-7Sn (wt%) alloy
    Li, Wandong
    Huang, Xuefei
    Huang, Weigang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 692 : 75 - 80
  • [27] Study on microstructure and properties of Mg2(Si,Sn) compound phase in Mg-Sn-Si magnesium alloy
    Zhang Jian-Xin
    Gao Ai-Hua
    Guo Xue-Feng
    Ren Lei
    ACTA PHYSICA SINICA, 2013, 62 (17)
  • [28] AS61 Magnesium Alloy with Nano-Scale Mg2Sn Phase as a Novel Anode for Primary Aqueous Magnesium Battery
    Wang, Naiguang
    Liang, Jianwen
    Liu, Jingjing
    Huang, Yixiang
    Shao, Huaiyu
    Cai, Qiong
    Hu, Mingchang
    Shi, Zhicong
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2021, 168 (10)
  • [29] First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface
    Wang Furong
    Zhang Yongmei
    Bai Guoning
    Guo Qingwei
    Zhao Yuhong
    ACTA METALLURGICA SINICA, 2023, 59 (06) : 812 - 820
  • [30] ELECTRONIC STRUCTURE OF MG2SN CRYSTALS
    DONETSKICH, VI
    SOBOLEV, VV
    SOKOLOV, EB
    ROITER, LA
    PHYSICA STATUS SOLIDI, 1969, 32 (01): : K7 - +