Copper metallization of hydroxyl-modified amorphous Si:C:H films

被引:5
|
作者
Pritchett, M [1 ]
Magtoto, N [1 ]
Tong, J [1 ]
Kelber, JA [1 ]
Zhao, X [1 ]
机构
[1] Univ N Texas, Dept Chem, Denton, TX 76102 USA
关键词
X-ray photoelectron spectroscopy; copper; wetting; diffusion barrier;
D O I
10.1016/S0040-6090(03)00687-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
X-ray photoelectron spectroscopy (XPS) was used to examine the initial stages of copper deposited by Physical vapor deposition (PVD), or sputter deposition, interacting with amorphous silicon:carbon:hydrogen (a-Si:C:H) films and hydroxyl modified amorphous silicon:carbon:hydrogen (a-Si:C:H/OH) films under Ultra-high vacuum (UHV) conditions. Amorphous-Si:C:H films were formed by condensing vinyltrimethylsilane (VTMS) on a titanium substrate (temperature less than or equal to 90 K) followed by electron beam bombardment (500 eV), and annealing to 300 K in UHV Amorphous Si:C:H/OH films were formed by condensing H2O on the condensed VTMS multilayer (less than or equal to 90 K) followed by electron beam bombardment (500 eV) and annealing to 300 K in UHV The stoichiometry of the unmodified and modified a-Si:C:H films was determined by XPS to be C-4.5:S1 and C-4.3:O-0.44:Si, respectively. XPS measurements of PVD Cu on the modified film at 300 K indicate initial conformal growth with Cu(I) and Cu(0) formation at the Cu/Si:C:H/OH film interface. At higher Cu coverages, only Cu(0) was observed. In contrast, 3-dimensional island formation (Volmer-Weber growth) of Cu(0) was observed on the unmodified film. Annealing both the modified and unmodified films up to 800 K in UHV produced no significant change in the Cu(3p)/Cu(2p(3/2)) intensity ratio, indicating negligible Cu diffusion through the film into the titanium substrate below 800 K. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:100 / 108
页数:9
相关论文
共 50 条
  • [31] ELECTRICAL-CONDUCTIVITY IN AMORPHOUS SI(O OR H)-AU FILMS
    HAUSER, JJ
    SOLID STATE COMMUNICATIONS, 1980, 34 (05) : 321 - 324
  • [32] PREPARATION AND CHARACTERIZATION OF REACTIVELY-SPUTTERED AMORPHOUS SI - H FILMS
    IIZIMA, S
    OKUSHI, H
    MATSUDA, A
    YAMASAKI, S
    NAKAGAWA, K
    MATSUMURA, M
    TANAKA, K
    JAPANESE JOURNAL OF APPLIED PHYSICS, 1980, 19 : 521 - 526
  • [33] SURFACE EFFECTS AND THE PHOTOCONDUCTIVITY SPECTRUM OF AMORPHOUS SI-H FILMS
    PERSANS, P
    FRITZSCHE, H
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1980, 25 (03): : 330 - 330
  • [34] Photoelectrochemical behaviour of hydrogenated amorphous silicon (a-Si:H) films
    Wang, BH
    Wang, DJ
    Zhang, LH
    Geng, XH
    Sun, ZL
    Geng, XH
    Sun, ZL
    Li, TJ
    CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 1995, 16 (11): : 172 - 176
  • [35] Photoelectrochemical behaviour of hydrogenated amorphous silicon(a-Si: H) films
    Wang, Bao-hui
    Wang, De-jun
    Zhang, Li-hua
    Geng, Xin-hua
    Sun, Zhong-lin
    Geng, Xin-hua
    Sun, Zhong-lin
    Li, Tie-jin
    Kao Teng Hsueh Hsiao Hua Heush Hsueh Pao/ Chemical Journal of Chinese Universities, 1995, 16 (11 suppl):
  • [36] Photoelectrochemical Behaviour of Hydrogenated Amorphous Silicon(a-Si:H) Films
    Wang, B.-H.
    Wang, D.-J.
    Zhang, L.-H.
    Geng, X.-H.
    Kao Teng Hsueh Hsiao Hua Heush Hsueh Pao/ Chemical Journal of Chinese Universities, 1600, 16 (11-SUP):
  • [37] PLASMA DEPOSITED SEMICONDUCTING SI-B-H AMORPHOUS FILMS
    TSAI, CC
    FRITZSCHE, H
    TANIELIAN, MH
    VESAGHI, MA
    BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1977, 22 (03): : 336 - 336
  • [38] Synthesis, characterization and nanostructuring of (a-C:H):Si and (a-C:H):Si:metal films
    Kirpilenko, G. G.
    Frolov, V. D.
    Zavedeev, E. V.
    Pimenov, S. M.
    Konov, V. I.
    Shelukhin, E. Y.
    Loubnin, E. N.
    DIAMOND AND RELATED MATERIALS, 2006, 15 (4-8) : 1147 - 1150
  • [39] AMORPHOUS SiNx: H FILMS WITH A LOW DENSITY OF Si-H BONDS.
    Hasegawa, S.
    Matuura, M.
    Anbutu, H.
    Kurata, Y.
    Philosophical Magazine B: Physics of Condensed Matter; Electronic, Optical and Magnetic Properties, 1987, 56 (05): : 633 - 640
  • [40] ELECTRICAL-CONDUCTIVITY IN AMORPHOUS SI-H AND SIC-H FILMS
    KOLODZIEJ, A
    PISARKIEWICZ, T
    ACTA PHYSICA POLONICA A, 1989, 75 (02) : 309 - 312