Hydrothermal deactivation of Fe-ZSM-5 catalysts for the selective catalytic reduction of NO with NH3

被引:103
|
作者
Brandenberger, Sandro [1 ]
Kroecher, Oliver [1 ]
Casapu, Maria [1 ]
Tissler, Arno [2 ]
Althoff, Roderik [2 ]
机构
[1] Paul Scherrer Inst, CH-5232 Villigen, Switzerland
[2] Sud Chem AG, D-83052 Bruckmuhl, Germany
关键词
Selective catalytic reduction (SCR); Ammonia; NOx; Hydrothermal aging; Deactivation; NOx reduction efficiency; DeNO(x); Fe-ZSM-5; Zeolite; LOW FE CONTENT; AMMONIUM EXCHANGE; MAS-NMR; ZEOLITE; TEMPERATURE; STABILITY; SITES; STATE; DEALUMINATION; DECOMPOSITION;
D O I
10.1016/j.apcatb.2010.11.006
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The hydrothermal deactivation of Fe-ZSM-5 catalysts for the reduction of NO with NH3 in the presence of 10% H2O was studied. Aged and fresh catalysts were characterized by H-TPR, DRIFTS. Al-27 NMR, Si-29 NMR, XAS and nitrogen physisorption. The analysis of deactivated catalysts indicated that, under moderately aging conditions, dealumination due to hydrolysis occurs only on Al sites that bear a Bronsted acidic proton. Furthermore, the results showed that the cause of hydrothermal aging is Fe migration, which leads to the formation of FeOx clusters that increase in size as the age of the catalyst increases. This Fe migration was not strongly related to the process of dealumination and the stability with respect to SCR activity depends more on the stability of the active iron species in ion exchange sites than the stability of the framework itself. The hydrothermal stability of these active iron sites was not significantly influenced by the presence of Bronsted acid protons. The remaining activity after hydrothermal aging is caused by isolated iron ions located at ion exchange sites. Based on these results a general mechanism for aging under hydrothermal conditions was developed that differentiates between dealumination, migration and clustering of Fe oxides and the temporal sequence of these processes. 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:649 / 659
页数:11
相关论文
共 50 条
  • [41] Deactivation of a Fe-ZSM-5 catalyst during the selective catalytic reduction of NO by n-decane:: An operando DRIFT study
    Delahay, Gerard
    Guzman-Vargas, Ariel
    Coq, Bernard
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2007, 70 (1-4) : 45 - 52
  • [42] Fe-Ce-ZSM-5 a new catalyst of outstanding properties in the selective catalytic reduction of NO with NH3
    Carja, G
    Delahay, G
    Signorile, C
    Coq, B
    CHEMICAL COMMUNICATIONS, 2004, (12) : 1404 - 1405
  • [43] Evolution mechanism of active sites for selective catalytic reduction of NOx with NH3 over Fe-ZSM-5 catalysts doped by Ce/CuCe/Cu掺杂Fe-ZSM-5 催化剂NH3选择性催化还原NOx的活性位点演化机理
    Yu-bo Zhang
    Pan Wang
    Dan Yu
    Hong-yu Zhao
    Xing-lei Lyu
    Li-li Lei
    Journal of Central South University, 2022, 29 : 2239 - 2252
  • [44] Low-temperature SCR of NO with NH3 over noble metal promoted Fe-ZSM-5 catalysts
    Qi, GS
    Yang, RT
    CATALYSIS LETTERS, 2005, 100 (3-4) : 243 - 246
  • [45] Low-temperature SCR of NO with NH3 over noble metal promoted Fe-ZSM-5 catalysts
    Gongshin Qi
    Ralph T. Yang
    Catalysis Letters, 2005, 100 : 243 - 246
  • [46] Efficient Fe-ZSM-5 catalyst with wide active temperature window for NH3 selective catalytic reduction of NO: Synergistic effect of isolated Fe3+ and Fe2O3
    Shi, Jin
    Zhang, Yi
    Zhu, Yong
    Chen, Mingxia
    Zhang, Zhixiang
    Shangguan, Wenfeng
    JOURNAL OF CATALYSIS, 2019, 378 : 17 - 27
  • [47] Promotional Effect of Cerium and/or Zirconium Doping on Cu/ZSM-5 Catalysts for Selective Catalytic Reduction of NO by NH3
    Liu, Ye
    Song, Chonglin
    Lv, Gang
    Fan, Chenyang
    Li, Xiaodong
    CATALYSTS, 2018, 8 (08)
  • [48] Research Progress of the Selective Catalytic Reduction with NH3 over ZSM-5 Zeolite Catalysts for NOx Removal
    Pan, Wangxiang
    He, Jingping
    Huang, Guanlin
    Zhang, Wentao
    Fang, De
    CATALYSTS, 2023, 13 (10)
  • [49] Catalytic wet oxidation of phenol with Fe-ZSM-5 catalysts
    Yan, Ying
    Jiang, Songshan
    Zhang, Huiping
    RSC ADVANCES, 2016, 6 (05) : 3850 - 3859
  • [50] NH3-SCR Performance of Fresh and Hydrothermally Aged Fe-ZSM-5 in Standard and Fast Selective Catalytic Reduction Reactions
    Shi, Xiaoyan
    Liu, Fudong
    Xie, Lijuan
    Shan, Wenpo
    He, Hong
    ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2013, 47 (07) : 3293 - 3298