Minority Carrier Lifetime Behavior in Crystalline Silicon in Rapid Laser Heating

被引:7
|
作者
Sameshima, Toshiyuki [1 ]
Betsuin, Koichi [1 ]
Mizuno, Tomohisa [2 ]
Sano, Naoki [3 ]
机构
[1] Tokyo Univ Agr & Technol, Koganei, Tokyo 1848588, Japan
[2] Kanagawa Univ, Hiratsuka, Kanagawa 2591293, Japan
[3] Aurea Works Corp, Yokohama, Kanagawa 2300046, Japan
关键词
MACROSCOPIC THEORY; PHOSPHORUS ATOMS; SI; ACTIVATION; DOPANT; LAYERS;
D O I
10.1143/JJAP.51.03CA04
中图分类号
O59 [应用物理学];
学科分类号
摘要
We report changes in the light-induced minority carrier effective lifetime tau(eff) of crystalline silicon caused by rapid laser heating. The top surface of n- and p-type silicon substrates with thicknesses of 520 and 150 mu m coated with thermally grown SiO2 layers were heated by a 940nm semiconductor laser for 4ms. tau(eff) was measured by a method of microwave absorption caused by carriers induced by 620nm light illumination at 1.5mW/cm(2). tau(eff) for light illumination of the top surfaces was decreased to 1.0 x 10(-5) and 4.8 x 10(-6) s by laser heating at 5.0 x 10(4) W/cm(2) for nand p-type 520-mu m-thick silicon substrates, respectively. It was decreased to 1.5 x 10(-6) and 6.7 x 10(-6) s by laser heating at 4.2 x 10(4) W/cm(2) for n- and p-type 150-mu m-thick silicon substrates, respectively. The decrease in tau(eff) resulted from the generation of defect states associated with the carrier recombination velocity at the top surface region, Stop. Laser heating increased Stop to 6000 and 10000 cm/s for n- and p-type 520-mu m-thick silicon substrates, respectively and to 9200 and 2150 cm/s for n- and p-type 150-mu m-thick silicon substrates, respectively. Heat treatment at 400 degrees C for 4 h markedly decreased S-top to 21 and 120 cm/s respectively for 520-mu m-thick n- and p-type silicon samples heated at 5.0 x 10(4) W/cm(2). The heat treatment also decreased, 10 and 35 cm/s, respectively, for 150-mu m-thick n- and p-type silicon substrates heated at 4.2 x 10(4) W/cm(2). (C) 2012 The Japan Society of Applied Physics
引用
收藏
页数:6
相关论文
共 50 条
  • [22] Effect of oxygen concentration on minority carrier lifetime at the bottom of quasi-single crystalline silicon
    Huang, Chunlai
    Wu, Peng
    Wang, Lei
    Yang, Deren
    MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2021, 123
  • [23] Minority carrier lifetime measurements in epitaxial silicon layers
    Hara, T
    Tamura, F
    Kitamura, T
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (06) : 2205 - 2205
  • [24] MEASUREMENT OF MINORITY-CARRIER LIFETIME PROFILES IN SILICON
    SCHWAB, G
    BERNT, H
    REICHL, H
    SOLID-STATE ELECTRONICS, 1977, 20 (02) : 91 - &
  • [25] Minority carrier lifetime measurement in epitaxial silicon layers
    Hara, T
    Tamura, F
    Kitamura, T
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (04) : L54 - L57
  • [26] Measurement of minority carrier lifetime in epitaxial silicon layers
    Kitamura, T
    Tamura, F
    Hara, T
    Hourai, M
    Tsuya, H
    PROCEEDINGS OF THE FOURTH INTERNATIONAL SYMPOSIUM ON HIGH PURITY SILICON, 1996, 96 (13): : 533 - 543
  • [27] MINORITY-CARRIER LIFETIME OF ION GETTERED SILICON
    RYSSEL, H
    SCHMIEDT, B
    KRANZ, H
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (08) : C360 - C360
  • [28] THE EFFECT OF QUENCHING ON THE MINORITY-CARRIER LIFETIME IN SILICON
    MILEVSKII, LS
    SOVIET PHYSICS-SOLID STATE, 1961, 2 (09): : 1931 - 1933
  • [29] Enhancement phenomenon of the minority carrier lifetime in annealed silicon
    Lin, Xiaotong
    You, Zhipu
    Guo, Huifen
    1600, (120):
  • [30] CONTACTLESS MEASUREMENT OF MINORITY-CARRIER LIFETIME IN SILICON
    WHITE, JC
    UNTER, TF
    SMITH, JG
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 1977, 24 (09) : 1217 - 1218