Monolayer dispersion of NiO in NiO/Al2O3 catalysts probed by positronium atom

被引:13
|
作者
Zhang, H. J. [1 ]
Chen, Z. Q. [1 ]
Wang, S. J. [1 ]
机构
[1] Wuhan Univ, Dept Phys, Hubei Nucl Solid Phys Key Lab, Wuhan 430072, Peoples R China
来源
JOURNAL OF CHEMICAL PHYSICS | 2012年 / 136卷 / 03期
基金
中国国家自然科学基金;
关键词
ANNIHILATION LIFETIME; HYDROGEN; ALUMINA; DECOMPOSITION; SPECTROSCOPY; ENHANCEMENT; INHIBITION; CHEMISTRY; DEFECTS; SUPPORT;
D O I
10.1063/1.3676259
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
NiO/Al2O3 catalysts with different NiO loadings were prepared by impregnation method. The monolayer dispersion capacity of NiO is determined to be about 9 wt.% through XRD quantitative phase analysis. Positron lifetime spectra measured for NiO/Al2O3 catalysts comprise two long and two short lifetime components, where the long lifetimes tau(3) and tau(4) correspond to ortho-positronium (o-Ps) annihilation in microvoids and large pores, respectively. With increasing loading of NiO from 0 to 9 wt.%, tau(4) drops drastically from 88 to 38 ns. However, when the NiO loading is higher than 9 wt.%, tau(4) shows a slower decrease. Variation of tau(4) (1/tau(4)) as a function of the NiO content can be well fitted by two straight lines with different slopes. The relative intensity of tau(4) also shows a fast decrease followed by a slow decrease for the NiO content lower and higher than 9 wt.%, respectively. The coincidence Doppler broadening measurements reveal a continuous increase of S parameter with increasing NiO loading up to 9 wt.% and then a decrease afterwards. This is due to the variation in intensity of the narrow component contributed by the annihilation of para-positronium (p-Ps). Our results show that the annihilation behavior of positronium is very sensitive to the dispersion state of NiO on the surface of gamma-Al2O3. When the NiO loading is lower than monolayer dispersion capacity, spin conversion of positronium induced by NiO is the dominant effect, which causes decrease of the longest lifetime and its intensity but increase of the narrow component intensity. After the NiO loading is higher than monolayer dispersion capacity, the spin conversion effect becomes weaker and inhibition of positronium formation by NiO is strengthened, which results in decrease of both the long lifetime intensity and the narrow component intensity. The reaction rate constant is determined to be (1.50 +/- 0.04) x 10(10) g mol(-1) s(-1) and (3.43 +/- 0.20) x 10(9) g mol(-1) s(-1) for NiO content below and above monolayer dispersion capacity, respectively. (C) 2012 American Institute of Physics. [doi: 10.1063/1.3676259]
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Effect of ZrO2 on the Structure of NiO/CeO2/γ-Al2O3 Composite Catalysts
    Yang Xiu-Chun
    Lu Zhen-Guang
    Kang Xiao-Chun
    Wei Ya-Nan
    [J]. JOURNAL OF INORGANIC MATERIALS, 2009, 24 (01) : 187 - 191
  • [42] Fabrication of Ni/Al2O3/Ni Heteroepitaxial Junction by Post-Hydrogen Reduction of NiO/Al2O3/NiO Trilayered Epitaxial Thin Film
    Yamauchi, Ryosuke
    Kobayashi, Keisuke
    Hosaka, Makoto
    Suzuki, Toshimasa
    Koyama, Kohji
    Matsuda, Akifumi
    Arai, Hideki
    Kato, Yushi
    Mitsuhashi, Masahiko
    Kaneko, Satoru
    Yoshimoto, Mamoru
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS, 2011, 50 (09)
  • [43] Structure and Reducibility of NiO-MoO3/γ-Al2O3 Catalysts: Effects of Loading and Molar Ratio
    Wang, Yuguang
    Xiong, Guang
    Liu, Xin
    Yu, Xiaochuan
    Liu, Liping
    Wang, Junying
    Feng, Zhaochi
    Li, Can
    [J]. JOURNAL OF PHYSICAL CHEMISTRY C, 2008, 112 (44): : 17265 - 17271
  • [44] A Comparative Study of NiO/Al2O3 Catalysts Prepared by Different Combustion Techniques for Octanal Hydrogenation
    Farahani, Majid D.
    Valand, Jignesh
    Mahomed, Abdul S.
    Friedrich, Holger B.
    [J]. CATALYSIS LETTERS, 2016, 146 (12) : 2441 - 2449
  • [45] STRESSES IN NIO, CR2O3 AND AL2O3 OXIDE SCALES
    HUNTZ, AM
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 201 (1-2): : 211 - 228
  • [46] A Comparative Study of NiO/Al2O3 Catalysts Prepared by Different Combustion Techniques for Octanal Hydrogenation
    Majid D. Farahani
    Jignesh Valand
    Abdul S. Mahomed
    Holger B. Friedrich
    [J]. Catalysis Letters, 2016, 146 : 2441 - 2449
  • [47] Selectivity Reversal in Oxidative Dehydrogenation of Ethane with CO2 on CaO–NiO/Al2O3 Catalysts
    T. V. Sagar
    M. Surendar
    D. Padmakar
    G. Parameswaram
    N. Lingaiah
    K. S. Rama Rao
    I. A. K. Reddy
    C. Sumana
    P. S. Sai Prasad
    [J]. Catalysis Letters, 2017, 147 : 82 - 89
  • [48] A SPECTROSCOPIC STUDY OF THE EFFECT OF H2O AND NIO ON THE SURFACE-STRUCTURE OF NIO-MOO3/AL2O3
    STENCEL, JM
    MAKOVSKY, LE
    DIEHL, JR
    SARKUS, TA
    [J]. JOURNAL OF CATALYSIS, 1985, 95 (02) : 414 - 422
  • [49] Humidity sensing properties of NiO/Al2O3 nanocomposite materials
    Makhlouf, SA
    Khalil, KMS
    [J]. SOLID STATE IONICS, 2003, 164 (1-2) : 97 - 106
  • [50] Amination of aliphatic alcohols catalyzed by CuO–NiO/γ–Al2O3
    Jia-min Huang
    Chao Qian
    Lie Feng
    Yun-bin Chen
    Xin-zhi Chen
    [J]. Monatshefte für Chemie - Chemical Monthly, 2013, 144 : 1187 - 1190