Quasi-Static Mechanical Properties of Post-Processed Laser Powder Bed Fusion Ti6Al4V(ELI) Parts under Compressive Loading

被引:1
|
作者
Muiruri, Amos [1 ,2 ]
Maringa, Maina [2 ]
du Preez, Willie [2 ,3 ]
机构
[1] South Eastern Univ Kenya, Sch Engn & Technol, Dept Mech Engn, Kitui 90201, Kenya
[2] Cent Univ Technol, Dept Mech & Mechatron Engn, ZA-9301 Bloemfontein, Free State, South Africa
[3] Cent Univ Technol, Fac Engn Built Environm & Informat Technol, Ctr Rapid Prototyping & Mfg, ZA-9301 Bloemfontein, Free State, South Africa
来源
APPLIED SCIENCES-BASEL | 2022年 / 12卷 / 19期
关键词
Ti6Al4V(ELI); quasi-static; strain rate; DMLS; microstructure; micro-texture; yield stress; flow stress; HIGH-STRAIN-RATE; TITANIUM-ALLOY; HEAT-TREATMENT; FATIGUE PROPERTIES; VARIANT SELECTION; MELTED TI-6AL-4V; MICROSTRUCTURE; BEHAVIOR; ALPHA; BETA;
D O I
10.3390/app12199552
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The Ti6Al4V structures in aircraft and biomedical industries are usually exposed to quasi-static loads. Therefore, understanding the quasi-static behaviour of this alloy manufactured by an additive manufacturing process is paramount. This paper documents an investigation of the quasi-static mechanical properties of various microstructures of heat-treated Ti6Al4V(ELI) parts manufactured by laser powder bed fusion (LPBF). The effects of different quasi-static strain rates on different microstructures of these samples and their strain hardening are also presented. The test samples were produced using an EOSINT M280 direct metal laser sintering (DMLS) machine and, thereafter, subdivided into three major groups, namely samples C, D and E, for high-temperature annealing at different heat treatment strategies. A universal hydraulic testing machine (UTM) was used to carry out tests at strain rates of 0.001 s(-1), 0.005 s(-1) and 0.1 s(-1). The three forms of LPBF Ti6Al4V(ELI) were found to be sensitive to quasi-static strain rate, whereby values of yield and flow stresses in each form of alloy increased with increasing strain rate. The order of the strength at each strain rate from the highest to the lowest was found to be samples C, D and E. The effects of strain rate on flow hardening were found to be significant in samples C and insignificant in samples D and E.
引用
收藏
页数:21
相关论文
共 50 条
  • [21] A New Approach to Empirical Optimization of Laser Powder Bed Fusion Process for Ti6Al4V Parts
    Alireza Dareh Baghi
    Shahrooz Nafisi
    Reza Hashemi
    Heike Ebendorff-Heidepriem
    Reza Ghomashchi
    Journal of Materials Engineering and Performance, 2023, 32 : 9472 - 9488
  • [22] Fatigue fracture characterization of chemically post-processed electron beam powder bed fusion Ti-6Al-4V
    Sandell, Viktor
    Akerfeldt, Pia
    Hansson, Thomas
    Antti, Marta-Lena
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 172
  • [23] The impact of oxidised powder particles on the microstructure and mechanical properties of Ti-6Al-4 V processed by laser powder bed fusion
    Williams, Robert
    Bilton, Matthew
    Harrison, Neil
    Fox, Peter
    ADDITIVE MANUFACTURING, 2021, 46
  • [24] Anisotropic tensile and fatigue properties of laser powder bed fusion Ti6Al4V under high temperature
    He, Yuxin
    Ma, Yu'e
    Zhang, Weihong
    Wang, Zhenhai
    ENGINEERING FRACTURE MECHANICS, 2022, 276
  • [25] Mechanical Behavior Assessment of Ti-6Al-4V ELI Alloy Produced by Laser Powder Bed Fusion
    Mahmud, Asif
    Huynh, Thinh
    Zhou, Le
    Hyer, Holden
    Mehta, Abhishek
    Imholte, Daniel D.
    Woolstenhulme, Nicolas E.
    Wachs, Daniel M.
    Sohn, Yongho
    METALS, 2021, 11 (11)
  • [26] Microstructure, mechanical, and wear properties of thin-walled Ti6Al4V parts produced using laser powder bed fusion technique
    Kushwaha, Ajay
    Subramaniyan, Anand Kumar
    Kenchappa, Nagesha Bommanahalli
    Barad, Sanjay
    MATERIALS LETTERS, 2022, 308
  • [27] A Review of the Fatigue Behaviour of Laser Powder Bed Fusion Ti6Al4V
    Moloi, Tumelo
    Dzogbewu, Thywill Cephas
    Maringa, Maina
    Muiruri, Amos
    METALLURGICAL & MATERIALS ENGINEERING, 2025, 31 (01) : 288 - 310
  • [29] Laser powder bed fusion of Ti6Al4V lattice structures and their applications
    Dzogbewu, Thywill Cephas
    JOURNAL OF METALS MATERIALS AND MINERALS, 2020, 30 (04): : 68 - 78
  • [30] Quasi-static analysis of mechanical properties of Ti6Al4V lattice structures manufactured using selective laser melting
    Qixiang Feng
    Qian Tang
    Ying Liu
    Rossi Setchi
    Shwe Soe
    Shuai Ma
    Long Bai
    The International Journal of Advanced Manufacturing Technology, 2018, 94 : 2301 - 2313