The generation mechanism and suppression method of the "comet tail" defect on the single-crystal silicon surface polishing with magnetorheological

被引:8
|
作者
Shi, Feng [1 ]
Qiao, Shuo [1 ,2 ]
Tian, Ye [1 ]
Song, Ci [1 ]
Tie, Guipeng [1 ]
Jiao, Zhaoyang [3 ]
Luo, Chi [1 ]
Zhou, Gang [1 ]
机构
[1] Natl Univ Def Technol, Coll Intelligence Sci & Technol, Changsha 410003, Peoples R China
[2] Changsha Univ, Coll Mech & Elect Engn, Changsha 410022, Peoples R China
[3] Chinese Acad Sci, Shanghai Inst Opt & Fine Mech, Natl Lab High Power Laser & Phys, Shanghai 201800, Peoples R China
基金
中国国家自然科学基金;
关键词
Single-crystal silicon; Comet tail; Removal depth; Magnetorheological polishing; CARBIDE;
D O I
10.1016/j.ceramint.2022.03.032
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Single-crystal silicon is an important material in the high precision reflector, and its processing quality directly affects the overall performance index of the reflector. Aiming at the problem of "comet tail" defect produced by the magnetorheological machining process, the process parameters are controlled by the combination of experiments and simulations, and the surface roughness changes after different scanning speeds under the same removal depth are compared and analyzed. The results show that under the same process parameters, the probability of "comet tail" defects are related to density and surface quality. The main factors affecting the occurrence probability and density of "comet tail" defects are process parameters. In actual processing, it is necessary to establish a threshold of process parameters, so that the "Comet tail" defect is less within the threshold and can be quickly removed. The final threshold range is: buffing wheel speed< 220rpm, flow rate< 80L/min, depth coefficient< 0.25, magnetic field strength< 7A. By discussing the "Comet tail" defect suppression method and key technology, it provides technical support for the realization of high precision control manufacturing of single-crystal silicon.
引用
收藏
页码:17621 / 17631
页数:11
相关论文
共 50 条
  • [21] Study on aspherical surface polishing of single crystal silicon lens
    Seimitsu Kogaku Kaishi, 9 (1280-1284):
  • [22] Surface smoothing of single-crystal diamond (100) substrate by polishing technique
    Kubota, Akihisa
    Fukuyama, Sakae
    Ichimori, Yuya
    Touge, Mutsumi
    DIAMOND AND RELATED MATERIALS, 2012, 24 : 59 - 62
  • [23] Investigation of increased removal rate during polishing of single-crystal silicon carbide
    Tsai, M. Y.
    Wang, S. M.
    Tsai, C. C.
    Yeh, T. S.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2015, 80 (9-12): : 1511 - 1520
  • [24] Investigation on Electrical Enhanced Photocatalysis Polishing of Single-Crystal Silicon Carbide Substrates
    Xingjun Gao
    Xiang Li
    Yan He
    Lin Fan
    Meiling Tang
    International Journal of Precision Engineering and Manufacturing, 2022, 23 : 1261 - 1274
  • [25] Investigation of increased removal rate during polishing of single-crystal silicon carbide
    M. Y. Tsai
    S. M. Wang
    C. C. Tsai
    T. S. Yeh
    The International Journal of Advanced Manufacturing Technology, 2015, 80 : 1511 - 1520
  • [26] Investigation on Electrical Enhanced Photocatalysis Polishing of Single-Crystal Silicon Carbide Substrates
    Gao, Xingjun
    Li, Xiang
    He, Yan
    Fan, Lin
    Tang, Meiling
    INTERNATIONAL JOURNAL OF PRECISION ENGINEERING AND MANUFACTURING, 2022, 23 (11) : 1261 - 1274
  • [27] Surface morphology of anisotropically etched single-crystal silicon
    Shikida, M
    Tokoro, K
    Uchikawa, D
    Sato, K
    JOURNAL OF MICROMECHANICS AND MICROENGINEERING, 2000, 10 (04) : 522 - 527
  • [28] WETTING AND SURFACE-TENSION OF SINGLE-CRYSTAL SILICON
    BERENSHTEIN, GV
    DYACHENKO, AM
    RUSANOV, AI
    COLLOID JOURNAL OF THE USSR, 1985, 47 (02): : 200 - 203
  • [29] Effects of polishing speed and a water environment on the mechanism of nanometric mechanical polishing of single-crystal lutetium oxide
    Li, Yuzhu
    Lai, Min
    Fang, Fengzhou
    MATERIALS TODAY COMMUNICATIONS, 2022, 30
  • [30] Investigation of cluster magnetorheological electro-Fenton composite polishing process for single-crystal GaN wafer based on BBD experimental method
    Zheng, Qiongbin
    Wu, Yusen
    Pan, Jisheng
    Xiang, Min
    Wang, Hao
    Yan, Qiusheng
    SMART MATERIALS AND STRUCTURES, 2024, 33 (03)