Relation between parameters of cavitation resistance and structure of steels

被引:3
|
作者
Rudakov, AA [1 ]
机构
[1] Ural State Tech Univ, Ekaterinburg, Russia
关键词
Cavitation; Incubation Period; Final Stage; Transport Phenomenon; Initial Structure;
D O I
10.1007/s11041-005-0023-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The cavitation resistance of steels with different initial structure and hardness (05Kh13, Kh18N10T, St 3, VNS17, 07Kh14AG12M. 12Kh13N3G5, 30Kh13, 03N18K8M5T, 30KHOG10, 95Kh18, 150Kh12M) is studied. Laws of variation of parameters of cavitation resistance are determined as a function of the level of ultimate hardening of the cavitation-affected surface in the final stage of the incubation period under microimpact loading of the studied steels.
引用
收藏
页码:12 / 15
页数:4
相关论文
共 50 条
  • [31] The effect of boron on cavitation resistance of FeCrMnSiB austenitic stainless steels
    Cruz, Juliane R.
    Henke, Sergio Luiz
    Pukasiewicz, Anderson G. M.
    d'Oliveira, Ana Sofia C. M.
    WEAR, 2019, 436
  • [32] CAVITATION RESISTANCE OF CHROMIUM DIFFUSION COATINGS ON STEELS AND CAST IRONS
    VOROSHNIN, LG
    KHAPPALAEV, AY
    ABACHARAEV, MM
    METAL SCIENCE AND HEAT TREATMENT, 1981, 23 (5-6) : 370 - 372
  • [33] CAVITATION RESISTANCE OF STAINLESS STEELS WITH CONSTANT NICKEL AND CARBON CONTENT
    Karabenciov, Adrian
    Dimian, Marcela Elena
    Jurchela, Alin Dan
    Oanca, Octavian
    MODTECH 2011: NEW FACE OF T.M.C.R., VOL I AND II, 2011, : 553 - 556
  • [34] TAKING INTO ACCOUNT STRUCTURE PARAMETERS IN PREDICTING THE CRACKING RESISTANCE OF STRUCTURAL-STEELS
    VIKULIN, AV
    SOVIET MATERIALS SCIENCE, 1992, 27 (06): : 577 - 580
  • [35] Simulation for the Influence of Structure Parameters on Cavitation Jet
    Zhou, Wei
    He, Kai
    Fang, Haitao
    Li, Jiuhua
    Cai, Jiannan
    Hu, Shaojie
    2017 IEEE INTERNATIONAL CONFERENCE ON INFORMATION AND AUTOMATION (IEEE ICIA 2017), 2017, : 870 - 874
  • [36] Correlations between mechanical properties and cavitation erosion resistance for stainless steels with 12% Chromium and variable contents of Nickel
    Bordeasu, I.
    Popoviciu, M. O.
    Mitelea, I.
    Ghiban, B.
    Ghiban, N.
    Sava, M.
    Duma, S. T.
    Badarau, R.
    INTERNATIONAL CONFERENCE ON APPLIED SCIENCES (ICAS2013), 2014, 57
  • [37] Resistance of Plate Shipbuilding Steels to Cavitation-Erosion and Fatigue Fracture
    O. I. Balyts’kyi
    J. Chmiel
    Materials Science, 2015, 50 : 736 - 739
  • [38] Resistance of Plate Shipbuilding Steels to Cavitation-Erosion and Fatigue Fracture
    Balyts'kyi, O. I.
    Chmiel, J.
    MATERIALS SCIENCE, 2015, 50 (05) : 736 - 739
  • [39] Cavitation Erosion Resistance of CrMnSiN Austenitic Stainless Steels Deposited by PTA
    Ribeiro, Helio Ormeu
    de Almeida Buschinelli, Augusto Jose
    Dutra, Jair Carlos
    Climaco Monteiro D'Oliveira, Ana Sofia
    SOLDAGEM & INSPECAO, 2010, 15 (02): : 121 - 129
  • [40] Cavitation Erosion Resistance of CrMnSiN Austenitic Stainless Steels Deposited by PTA
    Ribeiro H.O.
    Buschinelli A.J.A.
    Dutra J.C.
    D'Oliveira A.S.C.M.
    Soldagem e Inspecao, 2010, 15 (02): : 121 - 129