Semisolid joining of aluminum A356 alloy by partial remelting and mechanical stirring

被引:28
|
作者
Alvani, S. M. J. [1 ]
Aashuri, H. [1 ]
Kokabi, A. [1 ]
Beygi, R. [1 ]
机构
[1] Sharif Univ Technol, Dept Mat Sci & Engn, Tehran, Iran
关键词
semisolid joining; A356; localized stirring; shear punch; semi-solid holding; thermal treatment; MICROSTRUCTURAL EVOLUTION;
D O I
10.1016/S1003-6326(09)60376-9
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A method to reach the globular weld structure of A356 aluminum alloy using stirring the localized semisolid zone during butt-joining is developed. Since the heat conductivity of this alloy is very high, the accurate controlling of temperature during joining must be considered. A gas heating system was used to heat up the nitrogen gas up to the required temperature. A dried and free oxygen gas was prepared when a stream of nitrogen gas could pass closely around a hot element. Hot and pure nitrogen gas flow through a precise ceramic nozzle was used to create a localized semisolid pool. At this stage a fine stirrer was introduced into the weld seam in order to mix the two sides into a single uniform joint. Substrates were moved in direction of joint line by a small trolley to avoid the deviation of nozzle from the joint line and its distance and angle from the substrate. A fixture system was used to hold two substrates together on the trolley. A narrow hot plate was located on the trolley to heat up the joint line due to high heat conductivity of aluminum. Effect of gas temperature was investigated on the microstructure and mechanical properties of weld seam. Results showed that increase in temperature promoted the final welding properties, and also at liquid fractions less than 50% joining was not fully practical. The best mechanical properties were achieved with liquid fraction of about 70%.
引用
收藏
页码:1792 / 1798
页数:7
相关论文
共 50 条
  • [21] Microstructural evolution in semisolid forging of A356 alloy
    Byung Keun Kang
    Chun Pyo Hong
    Byoung Hee Choi
    Young Soo Jang
    Il Sohn
    Metals and Materials International, 2015, 21 : 153 - 158
  • [22] On the size effects in micro/meso semisolid extrusion–forging of A356 aluminum alloy
    Zhehe Yao
    Deqing Mei
    Pei Tang
    Zichen Chen
    The International Journal of Advanced Manufacturing Technology, 2014, 73 : 1243 - 1252
  • [23] Fractal Characteristics of Microstructure in Semisolid A356 Alloy
    Liu, Zheng
    Liu, Xiao-mei
    ADVANCED RESEARCH ON INDUSTRY, INFORMATION SYSTEMS AND MATERIAL ENGINEERING, PTS 1-7, 2011, 204-210 : 1575 - 1578
  • [24] The Effect of Electromagnetic Stirring on the Microstructural and Mechanical Properties of A356 Casting Alloy
    Colak, Murat
    Kayikci, Ramazan
    PAMUKKALE UNIVERSITY JOURNAL OF ENGINEERING SCIENCES-PAMUKKALE UNIVERSITESI MUHENDISLIK BILIMLERI DERGISI, 2009, 15 (03): : 345 - 351
  • [25] Effect of electromagnetic stirring method on flow characteristics of A356 aluminum alloy melt
    Li, ZeWen
    Chen, Hao
    Liu, Zheng
    International Journal of Lightweight Materials and Manufacture, 2025, 8 (03) : 321 - 330
  • [26] Vacuum-free stirring brazing of SiCp/A356 composites and aluminum alloy using semisolid filler metal with low solid fraction
    Xu, Huibin
    Luo, Quanxiang
    Xing, Liang
    Zhou, Bofang
    Zeng, Youliang
    Du, Changhua
    EMERGING FOCUS ON ADVANCED MATERIALS, PTS 1 AND 2, 2011, 306-307 : 738 - 741
  • [27] Electromagnetic stirring and Sr modification in A356 alloy
    Jung, BI
    Jung, CH
    Han, TK
    Kim, YH
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 111 (1-3) : 69 - 73
  • [28] Refinement mechanism of mixed rare earth on primary α phase in semisolid A356 alloy under electromagnetic stirring
    Liu, Zheng
    Xu, He-Jun
    Luo, Hao-Lin
    Zhou, Zhi-Peng
    Chen, Qing-Chun
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2013, 23 (08): : 2110 - 2117
  • [29] Rheologic properties of aluminum alloy A356 billets produced by semisolid continuous casting process
    Xing, S.M.
    Zeng, D.B.
    Shi, J.T.
    Tang, J.L.
    Qiu, Y.H.
    Qian, Q.
    Zhuzao/Foundry, 2001, 50 (02):
  • [30] Rheologic behaviors of A356 aluminum alloy billet produced by semisolid continuous casting process
    Shuming XING~1
    2. Department of Mechanical Engineering
    China Foundry, 2004, (01) : 62 - 66