Structural evolution of Al-8%Si hypoeutectic alloy by ultrasonic processing

被引:29
|
作者
Wang, J. Y. [1 ]
Wang, B. J. [1 ]
Huang, L. F. [1 ]
机构
[1] Northwestern Polytech Univ, Dept Appl Phys, Xian 710072, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
Solidification; Microstructure; Metals and alloys; Power ultrasound; Refinement; MECHANICAL-PROPERTIES; SOLIDIFICATION MICROSTRUCTURE; GRAIN-REFINEMENT; IRRADIATION;
D O I
10.1016/j.jmst.2017.07.018
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High intensity power ultrasound was respectively introduced into three different solidification stages of Al-8% Si hypoeutectic alloy, including the fully liquid state before nucleation, the nucleation and growth process of primary alpha (Al) phase and L -> (Al) + (Si) eutectic transformation period. It is found that both the primary alpha(Al) phase and (Al + Si) eutectic structure were refined by different degrees with various growth morphologies depending on the ultrasonic treatment stage. Based on the experimental results, the cavitation-induced nucleation due to the high undercooling caused by the collapse of tiny cavities was proposed as the major reason for refining the primary alpha(Al) phase. Meanwhile, obvious eutectic morphological change was observed only when ultrasound was directly introduced in the eutectic transformation stage, in which typical divorced eutectics and (Al + Si) eutectic cells with symmetrical flower shape were formed at the top of the alloy sample. The introduction of ultrasound in each solidification stage also improves the yield strength of Al-8% Si alloy to a diverse extent. (C) 2017 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:1235 / 1239
页数:5
相关论文
共 50 条
  • [41] Effect of ultrasonic melt processing and cooling rate on microstructure evolution of Al-Cu-Mn-Mg-Fe-Si alloy
    He, Weixiang
    Zhao, Yuliang
    Wei, Qiuyun
    Liu, Huan
    Song, Dongfu
    Shen, Fanghua
    Sun, Zhenzhong
    Li, Runxia
    [J]. JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 3655 - 3669
  • [42] Processing, Microstructure, and Mechanical Properties of Large Spray-Deposited Hypoeutectic Al-Si Alloy Tubular Preform
    Zhigang Chen
    Zhenhua Chen
    Guoning Tang
    [J]. Journal of Materials Engineering and Performance, 2011, 20 : 238 - 243
  • [43] Modification Mechanism of Rare Earth Eu on Eutectic Si in Hypoeutectic Al-Si Alloy
    Feng Mao
    Yongfeng Qiao
    Po Zhang
    Liming Ou
    Chong Chen
    Cheng Zhang
    Yu Wang
    [J]. International Journal of Metalcasting, 2022, 16 : 634 - 645
  • [44] Modification Mechanism of Rare Earth Eu on Eutectic Si in Hypoeutectic Al-Si Alloy
    Mao, Feng
    Qiao, Yongfeng
    Zhang, Po
    Ou, Liming
    Chen, Chong
    Zhang, Cheng
    Wang, Yu
    [J]. INTERNATIONAL JOURNAL OF METALCASTING, 2022, 16 (02) : 634 - 645
  • [45] Solidification Behavior of Intensively Sheared Hypoeutectic Al-Si Alloy Liquid
    Kotadia, H. R.
    Babu, N. Hari
    Zhang, H.
    Arumuganathar, S.
    Fan, Z.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (04): : 1117 - 1126
  • [46] Severe plastic deformation of an as-cast hypoeutectic Al-Si alloy
    Swaminathan, S.
    Garcia-Infanta, J. M.
    McNelley, T. R.
    Ruano, O. A.
    Carreno, F.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2008, 43 (23-24) : 7501 - 7506
  • [47] Distributions of Sr and Fe and their influence on modification of hypoeutectic Al-Si alloy
    Lan, Tu
    Li, Jian-guo
    [J]. CHINA FOUNDRY, 2016, 13 (02) : 85 - 92
  • [48] Ultrasonic solidification and microstructural evolution of binary Al-12.6%Si eutectic alloy
    Wang, BaoJian
    Wang, JianYuan
    Wu, WenHua
    Zhai, Wei
    Wang, Xu
    Jin, ZhanKui
    Wei, BingBo
    [J]. Zhongguo Kexue Jishu Kexue/Scientia Sinica Technologica, 2023, 53 (03): : 353 - 362
  • [49] AUTOCATALYTIC CONTINUOUS PRECIPITATION IN AN AL-8 WT-PERCENT MG ALLOY
    HAMANA, D
    NEBTI, S
    BOUTEFNOUCHET, A
    CHEKROUD, S
    [J]. ZEITSCHRIFT FUR METALLKUNDE, 1993, 84 (01): : 33 - 39
  • [50] Hydrogen desorption behavior in Al-8%Zn-1%Mg alloy
    Fujihara, Hiro
    Toda, Hiroyuki
    Shimizu, Kazuyuki
    Takeuchi, Akihisa
    Uesugi, Kentaro
    [J]. Keikinzoku/Journal of Japan Institute of Light Metals, 2019, 69 (03): : 186 - 193