Microhardness profiles on aged rubber compounds

被引:44
|
作者
Brown, RP [1 ]
Soulagnet, G [1 ]
机构
[1] Rapra Technol Ltd, Shrewsbury SY4 4NR, Salop, England
关键词
rubber; ageing; microhardness; thickness profile;
D O I
10.1016/S0142-9418(00)00035-0
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In a study of the long term natural ageing of rubbers, nineteen compounds were naturally aged for forty years at three sites classified as temperate (Shawbury, UK), hot dry (Cloncurry, Australia) and hot wet (Innisfail, Australia). The specimens were stored in specially constructed aluminium boxes which allowed free circulation of ambient air around the test pieces but excluded direct light and rain. After 40 years ageing, the use of microhardness measurements was investigated as a means of determining the degree of ageing as a function of material thickness. Compression set test pieces were sliced into 1 mm thick sheets and hardness determined. The procedure proved effective for determining hardness profiles. Significant differences were observed between skin and bulk suggesting that differential ageing had taken place. However, only the net effect of scission and crosslinking reactions is detected and differences can be due to differences in cure before exposure to ageing. After consideration of the known macro hardnesses of these materials and differences found at the centres of test pieces from the different exposure sites, it is suggested that the ageing process had not been greatly restricted by the rate of oxygen diffusion. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:295 / 303
页数:9
相关论文
共 50 条
  • [21] The study of fatigue behavior of thermally aged rubber based on natural rubber and butadiene rubber
    Kratina, O.
    Stocek, R.
    Musil, B.
    Johlitz, M.
    Lion, A.
    CONSTITUTIVE MODELS FOR RUBBER X, 2017, : 365 - 370
  • [22] Mechanical behavior and microhardness of swollen natural rubber loaded with carbon black
    Abu-Abdeen, M.
    Almulhem, Abdalaziz A.
    Sedky, A.
    JOURNAL OF APPLIED POLYMER SCIENCE, 2008, 109 (05) : 3361 - 3368
  • [23] Adhesion of rubber compounds to nano-copper-coated iron plates as studied by AES depth profiles
    Jeon, GS
    Jeong, SW
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2004, 18 (08) : 925 - 942
  • [24] HIGH TEMPERATURE MICROHARDNESS PROFILES OF HARD CVD COATINGS.
    Mehrotra, P.K.
    Quinto, D.T.
    Metal Powder Report, 1986, 41 (12) : 891 - 892
  • [25] Relaxation behavior and time-temperature superposition (TTS) profiles of thermally aged styrene-butadiene rubber (SBR)
    Xiang, Kewei
    Wu, Siduo
    Huang, Guangsu
    Zheng, Jing
    Huang, Jingyun
    Li, Guangxian
    MACROMOLECULAR RESEARCH, 2014, 22 (08) : 820 - 825
  • [26] Relaxation behavior and time-temperature superposition (TTS) profiles of thermally aged styrene-butadiene rubber (SBR)
    Kewei Xiang
    Siduo Wu
    Guangsu Huang
    Jing Zheng
    Jingyun Huang
    Guangxian Li
    Macromolecular Research, 2014, 22 : 820 - 825
  • [27] Heats of combustion of rubber and of rubber-sulphur compounds
    Jessup, RS
    Cummings, AD
    BUREAU OF STANDARDS JOURNAL OF RESEARCH, 1934, 13 (03): : 357 - 369
  • [28] Extrusion of physically foamed rubber profiles
    Michaeli, Walter
    Westermann, Kira
    Sitz, Sarah
    JOURNAL OF CELLULAR PLASTICS, 2011, 47 (05) : 483 - 495
  • [29] Extrusion of physically foamed rubber profiles
    Haberstroh, E
    Kremers, A
    Epping, K
    KGK-KAUTSCHUK GUMMI KUNSTSTOFFE, 2005, 58 (09): : 449 - 454
  • [30] Analysis of the production of sponge rubber profiles
    Kremers, A
    Krusche, A
    Haberstroh, E
    MACROMOLECULAR MATERIALS AND ENGINEERING, 2000, 284 (11-12) : 70 - 75