Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C

被引:32
|
作者
Klok, Oksana [1 ,2 ]
Lambrinou, Konstantina [2 ]
Gavrilov, Serguei [2 ]
Stergar, Erich [2 ]
Lim, Jun [2 ]
Van der Donck, Tom [3 ]
Van Renterghem, Wouter [2 ]
De Graeve, Iris [1 ]
机构
[1] VUB, Electrochem & Surface Engn SURF, Pl Laan 2, B-1050 Brussels, Belgium
[2] SCK CEN, Boeretang 200, B-2400 Mol, Belgium
[3] Katholieke Univ Leuven, Dept Mat Engn, Kasteelpk Arenberg 44, B-3001 Leuven, Belgium
关键词
Stainless steel; Plastic deformation; Twinning; De-alloying; Liquid metal corrosion; STACKING-FAULT ENERGY; LONG-TERM CORROSION; AUSTENITIC STEELS; PLASTIC-DEFORMATION; OXYGEN; BEHAVIOR; T91; TEMPERATURES; MECHANISMS; STRENGTH;
D O I
10.1016/j.jnucmat.2018.08.030
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work addresses the effect of deformation twinning on the dissolution corrosion behaviour of 316 L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE). For this purpose, plastically deformed 316 L steel specimens with distinctly different deformation twin densities were simultaneously exposed to oxygen-poor (<10(-13) mass%) static liquid LBE for 1000 hat 500 degrees C. The variation in deformation twin density was achieved by loading in uniaxial tension to similar degrees of plastic deformation (8-10%) specimens made of the same 316 L steel heat. Tensile loading was carried out at -150,25 and 150 degrees C so as to affect the twin density, which increased as the temperature of plastic deformation decreased. Dissolution corrosion was the only liquid metal corrosion mechanism observed in the LBE-exposed steel specimens. The thickness of the dissolution-affected zone increased with the deformation twin density, which was highest in the 316 L steel specimen deformed at -150 degrees C and lowest in the one deformed at 150 degrees C. As deformation twin boundaries accelerated the LBE ingress into the steel bulk, their local orientation with respect to the steel specimen surface affected the thickness of the dissolution-affected zone. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:556 / 567
页数:12
相关论文
共 50 条
  • [31] Thermochromatographic behavior of iodine in 316L stainless steel columns when evaporated from lead-bismuth eutectic
    Karlsson, Erik
    Neuhausen, Joerg
    Eichler, Robert
    Danilov, Ivan I.
    Vogele, Alexander
    Turler, Andreas
    JOURNAL OF RADIOANALYTICAL AND NUCLEAR CHEMISTRY, 2021, 328 (02) : 691 - 699
  • [32] Characterization of oxide scales grown on 216L stainless steels in liquid lead-bismuth eutectic
    Rao, V. Shankar
    Lim, Jun
    Hwang, Il Soon
    Singhal, L. K.
    CORROSION SCIENCE, 2012, 63 : 113 - 118
  • [33] Analysis of bi-layer oxide on austenitic stainless steel, 316L, exposed to Lead-Bismuth Eutectic (LBE) by X-ray Photoelectron Spectroscopy (XPS)
    Koury, D.
    Johnson, A. L.
    Ho, T.
    Farley, J. W.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 440 (1-3) : 28 - 33
  • [34] Superior corrosion resistance of a slurry FeAl coating on 316LN stainless steel in 550 °C liquid lead-bismuth eutectic
    Wang, Wen
    Zhu, Zhaoguang
    Yang, Liujie
    Lu, Jintao
    Huang, Jinyang
    Tan, Jibo
    Kuang, Wenjun
    CORROSION SCIENCE, 2024, 227
  • [35] Structural, electrical and magnetic measurements on oxide layers grown on 316L exposed to liquid lead-bismuth eutectic
    Hosemann, Peter
    Hofer, Christian
    Hlawacek, Gregor
    Li, Ning
    Maloy, Stuart A.
    Teichert, Christian
    JOURNAL OF NUCLEAR MATERIALS, 2012, 421 (1-3) : 140 - 146
  • [36] Effect of oxygen on corrosion of an alumina-forming duplex steel in static liquid lead-bismuth eutectic at 550 °C
    Chen, Lingzhi
    Tsisar, Valentyn
    Wang, Man
    Schroer, Carsten
    Zhou, Zhangjian
    CORROSION SCIENCE, 2021, 189 (189)
  • [37] Low-temperature oxy-nitriding of 316 L austenitic stainless steel for improved corrosion resistance in liquid lead-bismuth eutectic
    Chen, Guang
    Wang, Jun
    Zhang, Hongtao
    Li, Longyi
    Fan, Hongyuan
    SCRIPTA MATERIALIA, 2021, 202
  • [38] Growth and Exfoliation Behavior of the Oxide Scale on 316L and T91 in Flowing Liquid Lead-Bismuth Eutectic at 480 °C
    Tian, S. J.
    OXIDATION OF METALS, 2020, 93 (1-2): : 183 - 194
  • [39] Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels
    Wu Xinqiang
    Rong Lijian
    Tan Jibo
    Chen Shenghu
    Hu Xiaofeng
    Zhang Yangpeng
    Zhang Ziyu
    ACTA METALLURGICA SINICA, 2023, 59 (04) : 502 - 512
  • [40] Creep of 316L austenitic steel at 450-550 °C in static lead-bismuth eutectic covered by argon-hydrogen gas
    Yurechko, Mariya
    Skrypnik, Aleksandr
    Wedemeyer, Olaf
    Konys, Jurgen
    Schroer, Carsten
    JOURNAL OF NUCLEAR MATERIALS, 2022, 558