Experimental study on crack characteristics and acoustic emission characteristics in rock-like material with pre-existing cracks

被引:4
|
作者
Pan, Ji-Shun [1 ]
Yuan, Shuang-Xi [1 ]
Jiang, Tong [1 ]
Cui, Cheng-Hao [1 ]
机构
[1] North China Univ Water Resources & Elect Power, Coll Geosci & Engn, Zhengzhou 450046, Peoples R China
基金
中国国家自然科学基金;
关键词
MECHANICAL-BEHAVIOR; MODEL; COMPRESSION; JOINTS; BLOCK; FLAWS;
D O I
10.1038/s41598-021-03162-6
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Grain size composition, crack pattern, and crack length have a significant influence on the crack characteristics, mechanical characteristics, and acoustic emission characteristics of rock masses. In this paper, the crack characteristics, mechanical characteristics, and acoustic emission characteristics of rock masses with different grain size compositions, different crack patterns, and different crack lengths were investigated under uniaxial compression. The rock masses were made of rock-like materials. The crack initiation locations and crack propagation directions were different for a specimen comprised of one grain size range compared with specimens comprised of two or three grain size ranges. The specimens comprised of one and three grain size ranges crack progressively. The specimen comprised of two-grain size ranges brittle fracture. The highest peak axial load was found in the specimens comprised of one grain size range. The results showed that tensile wing crack, anti-tensile wing crack, transverse shear crack, compression induced tensile crack, and surface spalling were produced in specimens with different crack orientations. The rock mass with 2 cm long crack started to produce cracks from the tip of the crack extending to the top and bottom surface, soon forming through cracks. The rock was brittle fracture. The axial load reached the maximum and then fell rapidly. The acoustic emission energy reached a rapid maximum and then decreased rapidly. The rock mass with 3 cm long fissures started to produce cracks that only extended from the tip of the fissures to the top surface but not to the bottom surface. The rock mass was progressively fractured. The axial load was progressively decreasing. The acoustic emission energy also rose and fell rapidly several times as the rock mass was progressively fractured. Different rock crack lengths led to different crack processes and crack patterns, resulting in very different acoustic emission characteristics.
引用
收藏
页数:33
相关论文
共 50 条
  • [41] Experimental Study on the Crack Initiation and Propagation of Unequal Cracks in Rock-Like Materials
    Chen, Qingfeng
    Huang, Min
    Duan, Jingmin
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2022, 2022
  • [42] Erratum to: Cracks coalescence mechanism and cracks propagation paths in rock-like specimens containing pre-existing random cracks under compression
    Hadi Haeri
    Kourosh Shahriar
    Mohammad Fatehi Marji
    Parviz Moarefv
    Journal of Central South University, 2014, 21 (10) : 4052 - 4052
  • [43] Erratum to: Cracks coalescence mechanism and cracks propagation paths in rock-like specimens containing pre-existing random cracks under compression
    Hadi Haeri
    Kourosh Shahriar
    Mohammad Fatehi Marji
    Parviz Moarefvand
    Journal of Central South University, 2014, 21 : 4052 - 4052
  • [44] Numerical Simulation of Crack Growth and Coalescence in Rock-Like Materials Containing Multiple Pre-existing Flaws
    Zhou, X. P.
    Bi, J.
    Qian, Q. H.
    ROCK MECHANICS AND ROCK ENGINEERING, 2015, 48 (03) : 1097 - 1114
  • [45] Numerical Simulation of Crack Growth and Coalescence in Rock-Like Materials Containing Multiple Pre-existing Flaws
    X. P. Zhou
    J. Bi
    Q. H. Qian
    Rock Mechanics and Rock Engineering, 2015, 48 : 1097 - 1114
  • [46] Experimental and numerical study on mechanical and fracture behavior of rock-like specimens containing pre-existing holes flaws
    Zhao, Zhenlong
    Jing, Hongwen
    Shi, Xinshuai
    Han, Guansheng
    EUROPEAN JOURNAL OF ENVIRONMENTAL AND CIVIL ENGINEERING, 2022, 26 (01) : 299 - 319
  • [47] Failure characteristics of concrete pipes with pre-existing cracks
    Liu, Liping
    Tan, Fei
    Tian, Shugao
    Hong, Zhikai
    Lv, Jiahe
    STRUCTURAL CONCRETE, 2023, 24 (03) : 3744 - 3759
  • [48] Research on direct shear test of rock-like materials with two closed pre-existing cracks of different attitudes
    Yue, Ling
    Niu, Jie
    Ma, Qingshan
    Zhao, Chengxi
    Cao, Minjun
    Yu, Bangyong
    FRONTIERS IN EARTH SCIENCE, 2023, 10
  • [49] Experimental and numerical study on crack development characteristics between two cavities in rock-like material under uniaxial compression
    Liu, Bing
    Zhou, Yu
    Gao, Yong-Tao
    Xu, Chaoshui
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2020, 109
  • [50] Shear Failure Mechanism and Acoustic Emission Characteristics of Jointed Rock-Like Specimens
    Ban, Yuxin
    Xie, Qiang
    Fu, Xiang
    Abdullah, Rini Asnida
    Wang, Jingjing
    SAINS MALAYSIANA, 2021, 50 (02): : 287 - 300