Low cost rare earth elements deposition method for enhancing the oxidation resistance at high temperature of Cr2O3 and Al2O3 forming alloys

被引:19
|
作者
Paúl, A [1 ]
Elmrabet, S [1 ]
Odriozola, JA [1 ]
机构
[1] Univ Seville, Inst Ciencia Mat Sevilla, CSIC, E-41092 Seville, Spain
关键词
pyrolysis; reactive metal effect; stainless steel; high temperature oxidation;
D O I
10.1016/S0925-8388(01)00988-4
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Zn this work a deposition method for coating Cr2O3 and Al2O3 forming alloys with rare earth elements is described. This is a modified CVD deposition method based on the pyrolysis of an aerosol produced by ultrasonic waves focused on the surface of a solution containing a soluble salt of the desired element that will later transform to oxide. To test the efficiency of the deposition method, commercial AISI-303 stainless steel samples were coated with lanthanum and cerium nitrates. Oxidation experiments have been performed in a thermobalance at 1173 K in synthetic air atmosphere for 25 h. Oxidation kinetics of coated samples was compared with that of an untreated one. Results show that samples coated with La and Ce improve their high temperature oxidation resistance by decreasing their parabolic rate constant of one order of magnitude. During the oxidation treatment LaCrO3 perovskite forms in the scale of La-coated specimens while CeO2 is the crystalline phase detected in the Ce-coated ones. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:70 / 73
页数:4
相关论文
共 50 条
  • [21] INFLUENCE OF A MIXED AL2O3 + CR2O3 SUPERFICIAL COATING ON THE NONISOTHERMAL OXIDATION BEHAVIOR OF FE ALLOYS AND FE-CR ALLOYS
    MITRA, SK
    ROY, SK
    BOSE, SK
    OXIDATION OF METALS, 1992, 37 (1-2): : 95 - 108
  • [23] THE INFLUENCE OF LASER SURFACE-TREATMENT ON THE HIGH-TEMPERATURE OXIDATION OF CR2O3 - FORMING ALLOYS
    STOTT, FH
    BARTLETT, PKN
    WOOD, GC
    MATERIALS SCIENCE AND ENGINEERING, 1987, 88 : 163 - 169
  • [24] Accommodation of impurities in α-Al2O3, α-Cr2O3 and α-Fe2O3
    Atkinson, KJW
    Grimes, RW
    Levy, MR
    Coull, ZL
    English, T
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (16) : 3059 - 3070
  • [25] Measuring adhesion of Cr2O3 and Al2O3 scales on Fe-based alloys
    Galerie, A
    Toscan, F
    N'Dah, E
    Przybylski, K
    Wouters, Y
    Dupeux, M
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 631 - 638
  • [26] On the absorption of ammoniac by Al2O3, Fe2O3 and Cr2O3
    Nikitin, N
    ZEITSCHRIFT FUR ANORGANISCHE UND ALLGEMEINE CHEMIE, 1926, 155 (04): : 358 - 360
  • [27] A novel method for preparing α-Al2O3 (Cr2O3)/Fe-Al composite coating with high hydrogen isotopes permeation resistance
    He, Yifu
    Guo, Enkai
    Zhong, Fen
    Fu, Bowen
    Cai, Guangxu
    Zhang, Dongxun
    Jiang, Changzhong
    Ren, Feng
    CERAMICS INTERNATIONAL, 2024, 50 (11) : 20367 - 20375
  • [28] OPTICAL CHARACTERISTICS OF Cr2O3/Al2O3 COMPOSITE STRUCTURE
    Gasenkova, I., V
    Mukhurov, N., I
    Zhvavyi, S. P.
    Kolesnik, E. E.
    HIGH TEMPERATURE MATERIAL PROCESSES, 2021, 25 (03): : 1 - 10
  • [29] STRESSES IN NIO, CR2O3 AND AL2O3 OXIDE SCALES
    HUNTZ, AM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 201 (1-2): : 211 - 228
  • [30] Stresses in NiO, Cr2O3 and Al2O3 oxide scales
    Huntz, A.M.
    Materials Science and Engineering A, 1995, A201 (1-2): : 211 - 228