Experiment and theoretical prediction for subsurface microcracks and damage depth of multi-crystalline silicon wafer in diamond wire sawing

被引:19
|
作者
Li, Xinying [1 ,2 ]
Gao, Yufei [1 ]
Liu, Runtao [1 ]
Zhou, Wei [2 ]
机构
[1] Shandong Univ, Sch Mech Engn, Key Lab High Efficiency & Clean Mech Manufacture, Jinan 250061, Peoples R China
[2] Xiamen Univ, Dept Mech & Elect Engn, Xiamen 361005, Peoples R China
基金
中国国家自然科学基金;
关键词
Diamond wire sawing; Multi-crystalline silicon; Subsurface microcracks; Subsurface damage depth; PLASTIC INDENTATION DAMAGE; SURFACE-MORPHOLOGY; CRACK-PROPAGATION; MATERIAL REMOVAL; CUT; GENERATION; ROUGHNESS; ABRASIVES; MECHANISM; CERAMICS;
D O I
10.1016/j.engfracmech.2022.108391
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
Diamond wire saw slicing is an important process of multi-crystalline silicon (mc-Si) solar cell substrate processing. In wire sawing of silicon crystal, the brittleness removal of materials will lead to subsurface microcrack damage, reduce the fracture strength, increase the breakage probability of the as-sawn wafer and affect the subsequent surface etching texture of wafer. In this paper, a mathematical model calculating subsurface damage depth (SSD) of mc-Si is established based on the analysis of subsurface crack system in diamond wire sawing process. The correctness and rationality of the model are verified by experiments. Then, the model is used to predict the variation trend of the microcracks number (CN) and subsurface damage depth under different process parameters and saw wire parameters. The results show that the SSD decreases and CN increases with the increase of wire speed and decrease of feed speed; With the increase of abrasive density on wire surface, the SSD decreases and CN increase. The change of abrasive average size has little effect on the SSD and CN; a smaller abrasive size range is beneficial to reduce the SSD and increase CN.
引用
收藏
页数:22
相关论文
共 43 条
  • [41] Chemically microsurface-sphericizing on diamond wire-sawn multi-crystalline silicon wafers by metal-assisted chemical etching and rounding etching
    Zhang, Jinbing
    Zhou, Lang
    Zhou, Xiaoying
    Zhang, Fayun
    Liu, Yulong
    He, Liang
    Sun, Jie
    SOLAR ENERGY, 2021, 220 : 1032 - 1039
  • [42] Phase transformation pre-treatment of diamond wire-sawn multi-crystalline silicon wafers for metal-assisted chemical etching of solar cells
    Zhang, Jinbing
    Zhou, Xiaoying
    Hu, Dongli
    Yuan, Shuai
    Cai, Erhui
    SURFACES AND INTERFACES, 2023, 36
  • [43] Morphology of etch-pits on HF-HNO3-H2O vapor-etched diamond wire sawn multi-crystalline silicon wafers
    Xiao, Zhigang
    Geng, Guoying
    Wei, Xiuqin
    Yue, Zhihao
    Zhou, Lang
    SEMICONDUCTOR SCIENCE AND TECHNOLOGY, 2016, 31 (11)