Experimental Study on Deterioration Characteristics of Prestressed Concrete under the Coupling of Freeze-Thaw and Corrosion

被引:7
|
作者
Cui, Wei [1 ]
Liu, Manman [1 ]
Wang, Lixin [1 ]
Guan, Wei [2 ]
Song, Huifang [1 ]
Li, Feng [1 ]
机构
[1] Tianjin Univ, State Key Lab Hydraul Engn Simulat & Safety, Tianjin 300350, Peoples R China
[2] Minist Water Resources, Bur South North Water Transfer Planning Designing, 10 West Third Ring Middle Rd, Beijing 100038, Peoples R China
基金
中国国家自然科学基金;
关键词
Prestressed concrete; Freeze-thaw; Corrosion; Deterioration characteristics; Three-point bending test; Computed tomography (CT); STEEL REINFORCEMENT; CRACKING; PERFORMANCE; PRODUCTS; STRENGTH; DAMAGE; TIME;
D O I
10.1061/(ASCE)MT.1943-5533.0004084
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In order to explore the deterioration characteristics of prestressed concrete under the coupling of freeze-thaw and corrosion, a series of aging tests and three-point bending tests was conducted. Furthermore, the deterioration process was analyzed at the meso-level with the help of computed tomography (CT) technology. The following conclusions can be drawn: (1) within a certain range, under the coupling effect, freeze-thaw and corrosion promote each other, and the degradation effect of the coupling test of freeze-thaw and corrosion is greater than the simple superposition of the two; (2) after the aging test, when the number of freeze-thaw cycles or the corrosion rate are higher, the cracking load and the ultimate load of the prestressed concrete are reduced, but the loss rate of the ultimate load is small; (3) the effective prestress of the aging specimen can be obtained according to the cracking moment, and the calculation formula is simplified according to the mechanical characteristics; and (4) under the coupling of freeze-thaw and corrosion, the size of the cracks and the number of the pores inside the specimen increase, whereas the number of pores in the volume range of 0.1-0.5 mm(3) does not change significantly due to the filling effect of corrosion products. (C) 2021 American Society of Civil Engineers.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Mitigating freeze-thaw deterioration of pavement concrete under multi-field coupling by superabsorbent polymers
    Yao, Chao
    Shen, Aiqin
    Lyu, Zhenghua
    Zeng, Guopeng
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 414
  • [22] Research on Performance Deterioration of Internally Cured Pavement Concrete under the Coupling Effect of Salt Freeze-Thaw
    Xu, Jieting
    Qin, Xiao
    Lin, Yongkang
    Cao, Chaofeng
    Liu, Junhong
    Huang, Qingjian
    POLYMERS, 2023, 15 (03)
  • [23] DURABILITY ANALYSIS OF PRESTRESSED CONCRETE STRUCTURES IN CHLORIDE CORROSION SUBJOINING CYCLIC FREEZE-THAW
    Chen Yu
    Liu Rong-Gui
    Zhou Wei-Ling
    Zhang Yi-Duo
    Liu Tao
    Lu Chun-Hua
    ADVANCES IN CONCRETE STRUCTURAL DURABILITY: PROCEEDINGS OF THE 2ND INTERNATIONAL CONFERENCE ON DURABILITY OF CONCRETE STRUCTURES ICDCS2010, 2010, : 331 - 336
  • [24] Experimental study on creep characteristics of gneiss under freeze-thaw cycles
    Yang Xiu-rong
    Jiang An-nan
    Wang Shan-yong
    Zhang Feng-rui
    ROCK AND SOIL MECHANICS, 2019, 40 (11) : 4331 - 4340
  • [25] Performance and deterioration mechanism of concrete incorporated with corrosion-inhibiting admixtures under the coupling effect of composite salt and freeze-thaw cycles
    Jiang, Minghui
    Liu, Xiao
    Hang, Meiyan
    Xu, Yurui
    Lai, Guanghong
    Li, Shiyu
    JOURNAL OF BUILDING ENGINEERING, 2023, 69
  • [26] On Deterioration Mechanism of Concrete Exposed to Freeze-Thaw Cycles
    Trofimov, B. Ya
    Kramar, L. Ya
    Schuldyakov, K. V.
    INTERNATIONAL CONFERENCE ON CONSTRUCTION, ARCHITECTURE AND TECHNOSPHERE SAFETY (ICCATS 2017), 2017, 262
  • [27] INFLUENCE OF SALT ON FREEZE-THAW DETERIORATION OF CONCRETE - REPLY
    CANTOR, TR
    KNEETER, CP
    MATERIALS PERFORMANCE, 1977, 16 (10) : 43 - 43
  • [28] STUDY ON CREEP OF CONCRETE UNDER FREEZE-THAW CYCLES
    Cao, Jian
    Wang, Yuan-Feng
    Zhao, Shang-Chuan
    ISISS '2009: INNOVATION & SUSTAINABILITY OF STRUCTURES, VOLS 1 AND 2, 2009, : 1111 - 1115
  • [29] Evaluation of freeze-thaw damage on concrete material and prestressed concrete specimens
    Qin, Xiao-chuan
    Meng, Shao-ping
    Cao, Da-fu
    Tu, Yong-ming
    Sabourova, Natalia
    Grip, Niklas
    Ohlsson, Ulf
    Blanksvard, Thomas
    Sas, Gabriel
    Elfgren, Lennart
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 125 : 892 - 904
  • [30] Experimental study on the dynamic mechanical properties of concrete under freeze-thaw cycles
    Han, Nv
    Tian, Wei
    STRUCTURAL CONCRETE, 2018, 19 (05) : 1353 - 1362