Fitness-For-Service Assessment and Failure Analysis of Hydrogen-Induced Cracking in a Pipeline Steel

被引:3
|
作者
Zangeneh, Sh [1 ]
机构
[1] Razi Univ, Fac Engn, Dept Mat & Text Engn, Kermanshah, Iran
关键词
Fitness-for-Service (FFS) assessment; Hydrogen-induced cracking (HIC); Failure assessment diagram (FAD); RESIDUAL-STRESS; EMBRITTLEMENT;
D O I
10.1007/s11668-021-01248-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
During inspection of an 11-km-long pipeline made of API X60 steel carrying hydrocarbons containing wet H2S, hydrogen-induced cracking (HIC) was found at different locations along the pipeline length. Microstructural investigations by scanning electron microscopy (SEM) showed stepwise cracking (SWC) as the result of the presence of MnS inclusions. Fitness-for-service (FFS) assessment based on API579-1/ASME FFS-1 was performed to decide on the pipeline serviceability. The finite element analysis (FEA) results showed that the HIC-damaged pipeline was acceptable per level-3 FFS requirements and the pipeline understudy was fit for service. The remaining life of the damaged pipeline should also be periodically monitored using failure assessment diagram (FAD).
引用
收藏
页码:1875 / 1887
页数:13
相关论文
共 50 条
  • [31] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    Department of Material Physics, Univ. of Sci. and Technology Beijing, Beijing 100083, China
    Sci China Ser E Technol Sci, 4 (x5-382):
  • [32] Application of instrumented indentation technique for enhanced fitness-for-service assessment of pipeline crack
    Jae-Il Jang
    Yeol Choi
    Jung-Suk Lee
    Yun-Hee Lee
    Dongil Kwon
    Ming Gao
    Richard Kania
    International Journal of Fracture, 2005, 131 : 15 - 33
  • [33] Hydrogen-induced cracking susceptibility and hydrogen trapping efficiency of different microstructure X80 pipeline steel
    F. Huang
    X. G. Li
    J. Liu
    Y. M. Qu
    J. Jia
    C. W. Du
    Journal of Materials Science, 2011, 46 : 715 - 722
  • [34] Hydrogen-induced cracking susceptibility and hydrogen trapping efficiency of different microstructure X80 pipeline steel
    Huang, F.
    Li, X. G.
    Liu, J.
    Qu, Y. M.
    Jia, J.
    Du, C. W.
    JOURNAL OF MATERIALS SCIENCE, 2011, 46 (03) : 715 - 722
  • [35] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    Huang, YZ
    Chen, QZ
    Wang, YB
    Chu, WY
    SCIENCE IN CHINA SERIES E-TECHNOLOGICAL SCIENCES, 1998, 41 (04): : 372 - 382
  • [36] Hydrogen-induced cracking
    不详
    MATERIALS PERFORMANCE, 2004, 43 (11) : 55 - 55
  • [37] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    黄一中
    陈奇志
    王燕斌
    褚武扬
    Science in China(Series E:Technological Sciences), 1998, (04) : 372 - 382
  • [38] Hydrogen-induced cracking by nanovoids in 310 stainless steel
    Huang, Yizhong
    Chen, Qizhi
    Wang, Yanbin
    Chu, Wuyang
    Science China Series E Technological Sciences, 1998, 41 (04): : 372 - 382
  • [39] Effect of microstructure on hydrogen embrittlement and hydrogen-induced cracking behaviour of a high-strength pipeline steel weldment
    Zhang, Peng
    Laleh, Majid
    Hughes, Anthony E.
    Marceau, Ross K. W.
    Hilditch, Tim
    Tan, Mike Yongjun
    CORROSION SCIENCE, 2024, 227
  • [40] CORROSION AND HYDROGEN-INDUCED CRACKING OF PIPELINE STEEL IN MOIST TRIETHYLENE GLYCOL DILUTED WITH LIQUID-HYDROGEN SULFIDE
    SCHMITT, G
    SOBBE, L
    BRUCKHOFF, W
    CORROSION SCIENCE, 1987, 27 (10-11) : 1071 - 1076