Electrochemical noise measurements of steel corrosion in the molten NaCl-K2SO4 system

被引:15
|
作者
Cappeln, F [1 ]
Bjerrum, NJ [1 ]
Petrushina, IM [1 ]
机构
[1] Tech Univ Denmark, Dept Chem, Mat Sci Grp, DK-2800 Lyngby, Denmark
关键词
D O I
10.1149/1.1928187
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Electrochemical noise measurements have been carried out on AISI347, 10CrMo910, 15Mo3, and X20CrMoV121 steels in molten NaCl-K2SO4 at 630 degrees C. Different types of current noise have been identified for pitting, intergranular and peeling corrosion. The corrosion mechanism was the so-called active corrosion (i.e., the corrosion proceeds with no passivation due to the influence of chlorine), characterized by the formation of volatile metal chlorides as a primary corrosion product. It was found possible to obtain an empirical separation of general and intergranular corrosion using kurtosis (a statistical parameter calculated from the electrochemical noise data). It was found that average kurtosis values above 6 indicated intergranular corrosion and average values below 6 indicated general corrosion. The response time for localized corrosion detection in in-plant monitoring was approximately 90 min on this basis. Approximate values of polarization resistances of AISI347 and 15Mo3 steels were determined to be 250 and 100 Omega cm(2), respectively. (c) 2005 The Electrochemical Society.
引用
收藏
页码:B228 / B235
页数:8
相关论文
共 50 条
  • [41] Electrochemical Measurements for Assessing Corrosion of Metal Alloys in Molten LiF-NaF-KF and MgCl2-NaCl-KCl
    Choi, Suhee
    Strianese, Andrew R.
    Dale, Olivia
    Simpson, Michael F.
    JOM, 2021, 73 (11) : 3544 - 3554
  • [42] Electrochemical Measurements for Assessing Corrosion of Metal Alloys in Molten LiF-NaF-KF and MgCl2-NaCl-KCl
    Suhee Choi
    Andrew R. Strianese
    Olivia Dale
    Michael F. Simpson
    JOM, 2021, 73 : 3544 - 3554
  • [43] Electrochemical and spectroscopic investigations of the K2SO4-V2O5 molten electrolyte
    Schmidt, DS
    Winnick, J
    Boghosian, S
    Fehrmann, R
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (03) : 1060 - 1068
  • [44] Corrosion behavior of HDA (hot-dip aluminized) carbon steel C45 half immersed in molten salts (NaCl, Na2SO4) isothermally at 973 K
    Muhammed, Hawkar J.
    Koncz-Horvath, Daniel
    Torok, Tamas, I
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2023, 37 (20) : 2807 - 2827
  • [45] Influences of concentrations of H2SO4 and NaCl on stress corrosion cracking of SUS304 stainless steel in H2SO4-NaCl aqueous solutions
    Sunada, S
    Kariba, M
    Majima, K
    Sugimoto, K
    MATERIALS TRANSACTIONS, 2006, 47 (02) : 364 - 370
  • [46] Electrochemical reduction behavior of Hf(IV) in molten NaCl–KCl–K2HfCl6 system
    Xu Liu
    Yan-Ke Wu
    Song Chen
    Bo Song
    Li-Jun Wang
    Rare Metals, 2016, 35 : 655 - 660
  • [47] CORROSION OF STEEL BY H2SO4
    FONTANA, MG
    INDUSTRIAL AND ENGINEERING CHEMISTRY, 1951, 43 (08): : A65 - &
  • [48] Electrochemical reduction behavior of Hf(IV) in molten NaCl-KCl-K2HfCl6 system
    Liu, Xu
    Wu, Yan-Ke
    Chen, Song
    Song, Bo
    Wang, Li-Jun
    RARE METALS, 2016, 35 (08) : 655 - 660
  • [49] Hot Corrosion Behavior of ZrB2-SiC-Graphite Composite in NaCl and Na2SO4 Molten Salts
    Liu, X.
    Wang, G.
    Liu, L.
    Wang, Z.
    Wu, Z.
    Liu, M.
    JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY, 2018, 9 (03): : 309 - 317
  • [50] Influence of concentration of H2SO4 and NaCl on stress corrosion cracking in H2SO4-NaCl solutions
    Sunada, S
    Kariba, M
    Majima, K
    Sugimoto, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2005, 69 (10) : 899 - 906