Fracture of metal/ceramic laminates - II. Crack growth resistance and toughness

被引:69
|
作者
Hwu, KL [1 ]
Derby, B [1 ]
机构
[1] Univ Oxford, Dept Mat, Oxford OX1 3PH, England
关键词
D O I
10.1016/S1359-6454(98)00358-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The propagation of cracks has been studied through Al/alumina, Cu/alumina and Ni/alumina laminates, with a range of metal and ceramic thicknesses. Two specimen orientations were chosen to propagate a crack either through the metal and ceramic layers in parallel or through the layers sequentially and perpendicular to the laminate. In both orientations a rising T-curve (toughness) was found with increasing crack length with a very steeply rising T-curve at large crack extensions. These observations can be explained by a large-scale bridging model with a crack closure traction imposed by the plastically deforming metal ligaments in the wake of the propagating crack. A simple model is derived which predicts the performance of the Ni/alumina laminates well. It does not predict the behaviour of the lower metal yield strength Cu/alumina and Al/alumina laminates so well, although it does account for the general trend of their behaviour. (C) 1999 Acta Metallurgica Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:545 / 563
页数:19
相关论文
共 50 条
  • [31] Pre-crack and Fracture Toughness Evaluation of Ceramic Thin Plates
    Ma, Delong
    Bao, Yiwang
    Wan, Detian
    Qiu, Yan
    Zheng, Dezhi
    Fu, Shuai
    Wuji Cailiao Xuebao/Journal of Inorganic Materials, 2021, 36 (07): : 733 - 737
  • [33] Pre-crack and Fracture Toughness Evaluation of Ceramic Thin Plates
    Ma Delong
    Bao Yiwang
    Wan Detian
    Qiu Yang
    Zheng Dezhi
    Fu Shuai
    JOURNAL OF INORGANIC MATERIALS, 2021, 36 (07) : 733 - 737
  • [34] The role of specimen thickness in the fracture toughness and fatigue crack growth resistance of nanocrystalline platinum films
    Meirom, Roi A.
    Clark, Trevor E.
    Muhlstein, Christopher L.
    ACTA MATERIALIA, 2012, 60 (03) : 1408 - 1417
  • [35] Mode-II interlaminar fracture toughness of carbon/epoxy laminates
    Saidpour, H
    Barikani, M
    Sezen, M
    IRANIAN POLYMER JOURNAL, 2003, 12 (05) : 389 - 400
  • [36] MEASUREMENT OF CRACK-GROWTH RESISTANCE AT GLASS-CERAMIC-METAL INTERFACES
    MECHOLSKY, JJ
    BRINKER, CJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 373 - 373
  • [37] Effects of temperature on mode II fracture toughness of multidirectional CFRP laminates
    Kim, HS
    Wang, WX
    Takao, Y
    Ben, G
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2003, 17 (8-9): : 1717 - 1723
  • [38] FATIGUE CRACK GROWTH RATE AND CRACK INITIATION AND FRACTURE LIFE UNDER MIXED MODES I AND II.
    Yokobori, Toshimitsu
    Yokobori, Takeo
    Ishii, Kenji
    Sato, Kiyoshi
    Shyoji, Kazuo
    Zairyo/Journal of the Society of Materials Science, Japan, 1986, 35 (395) : 930 - 935
  • [39] On the relation between fracture toughness and crack resistance in oxide glasses
    To, Theany
    Jensen, Lars R.
    Smedskjaer, Morten M.
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2020, 534
  • [40] Effect of unstable crack growth on mode II interlaminar fracture toughness of a thermoplastic PEEK composite
    Perez, P. Garcia
    Bouvet, C.
    Chettah, A.
    Dau, F.
    Ballere, L.
    Peres, P.
    ENGINEERING FRACTURE MECHANICS, 2019, 205 : 486 - 497