Influences of Co substitution and annealing treatment on the structure and electrochemical properties of hydrogen storage alloys La0.7Mg0.3Ni2.45-xCo0.75+xMn0.1Al0.2 (x=0.00, 0.15, 0.30)

被引:58
|
作者
Miao, He [1 ]
Pan, Hongge [1 ]
Zhang, Shengcai [1 ]
Chen, Ni [1 ]
Li, Rui [1 ]
Gao, Mingxia [1 ]
机构
[1] Zhejiang Univ, Dept Mat Sci & Engn, Hangzhou 310027, Peoples R China
基金
中国国家自然科学基金;
关键词
hydrogen storage alloys; annealing treatment; structural characteristic; electrochemical properties;
D O I
10.1016/j.ijhydene.2007.02.029
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, the effects of both Co substitution and annealing treatment on the structures and electrochemical properties of La0.7Mg0.3Ni2.45-xCo0.75+xMn0.1Al0.2 (x =0.00, 0.15, 0.30) hydrogen storage alloys have been studied. X-ray diffraction (XRD) analyses show that the main phases of all of the alloys are (La, Mg)Ni-3 phase (PuNi3-type structure) and LaNi5 phase (CaCu5-type structure). Electrochemical investigations show that increasing Co content and annealing treatment can considerably enhance the cyclic stability of the alloy electrodes. For La0.7Mg0.3Ni2.15Co1.05Mn0.1Al0.2 alloy, the value of C-100/C-max was only 65.5% at its as-cast, however, the value reached 80.5% after an annealing treatment of 1173 K x 8 h. The maximum discharge capacity of the alloy electrodes increased by annealing treatment and decreased slightly when Co content increased from x = 0.00 to 0.30 at its as-cast state. But the exchange current density (I-0), the limiting current density (I-L) and the diffusion coefficient of hydrogen (D) of the alloy electrodes decreased, leading to a corresponding reduction of the high rate dischargeability (HRD), with increasing Co content and annealing treatment. (C) 2007 Published by Elsevier Ltd on behalf of the International Association for Hydrogen Energy.
引用
收藏
页码:3387 / 3394
页数:8
相关论文
共 50 条
  • [41] Structure and electrochemical properties of La1-xMgxNi2.8Co0.4Mn0.1Al0.2(x=0.25, 0.30, 0.33) hydrogen storage alloys
    Li, Si
    Zhou, Huai-Ying
    Wang, Zhong-Min
    Deng, Jian-Qiu
    Yao, Qing-Rong
    RARE METALS, 2020, 39 (12) : 1464 - 1468
  • [42] Microstructure and electrochemical properties of La0.8–xMMxMg0.2Ni3.1Co0.3Al0.1 (x = 0, 0.1, 0.2, 0.3) alloys
    Na Zhou
    Wen-Bo Du
    Pei-Long Zhang
    Yong-Guo Zhu
    Zhao-Hui Wang
    Ke Liu
    Shu-Bo Li
    Rare Metals, 2017, 36 : 645 - 650
  • [43] Microstructure and electrochemical properties of La0.8-xMMxMg0.2Ni3.1Co0.3Al0.1(x=0,0.1,0.2,0.3)alloys
    Na Zhou
    Wen-Bo Du
    Pei-Long Zhang
    Yong-Guo Zhu
    Zhao-Hui Wang
    Ke Liu
    Shu-Bo Li
    Rare Metals, 2017, 36 (08) : 645 - 650
  • [44] An investigation on the structural and electrochemical properties of La0.7Mg0.3(Ni0.85Co0.15)x (x=3.15-3.80) hydrogen storage electrode alloys
    Pan, HG
    Liu, YF
    Gao, MX
    Zhu, YF
    Lei, YQ
    Wang, QD
    JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 351 (1-2) : 228 - 234
  • [46] Influence of the substitution Ce for La on structural and electrochemical characteristics of La0.75-xCexMg0.25Ni3Co0.5 (x=0, 0.05, 0.1, 0.15, 0.2 at. %) hydrogen storage alloys
    Lv, Wei
    Yuan, Jianguang
    Zhang, Bao
    Wu, Ying
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 730 : 360 - 368
  • [47] Phase structure and electrochemical properties of La0.7Ce0.3Ni3.75Mn0.35Al0.15Cu0.75-x(Fe0.43B0.57)x hydrogen storage alloys
    Liu, Baozhong
    Hu, Mengjuan
    Ji, Liqiang
    Fan, Yanpin
    Wang, Yongguang
    Zhang, Zhi
    Li, Anming
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 516 : 53 - 57
  • [49] Phase Structure and Electrochemical Performances of La0.63Gd0.2Mg0.17Ni3.0-xCo0.3Alx (x=0.0, 0.1, 0.2, 0.3, 0.4) Alloys
    Gao, Zhijie
    Luo, Yongchun
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (09): : 8382 - 8392
  • [50] Effects of substitution of Ti for ZrMn0.7V0.2Co0.1Ni1.2 storage hydrogen alloys on phase structure and electrochemical properties
    Li, S
    Ji, SJ
    Sun, JC
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 (02) : 283 - 286