Influences of Co substitution and annealing treatment on the structure and electrochemical properties of hydrogen storage alloys La0.7Mg0.3Ni2.45-xCo0.75+xMn0.1Al0.2 (x=0.00, 0.15, 0.30)

被引:58
|
作者
Miao, He [1 ]
Pan, Hongge [1 ]
Zhang, Shengcai [1 ]
Chen, Ni [1 ]
Li, Rui [1 ]
Gao, Mingxia [1 ]
机构
[1] Zhejiang Univ, Dept Mat Sci & Engn, Hangzhou 310027, Peoples R China
基金
中国国家自然科学基金;
关键词
hydrogen storage alloys; annealing treatment; structural characteristic; electrochemical properties;
D O I
10.1016/j.ijhydene.2007.02.029
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, the effects of both Co substitution and annealing treatment on the structures and electrochemical properties of La0.7Mg0.3Ni2.45-xCo0.75+xMn0.1Al0.2 (x =0.00, 0.15, 0.30) hydrogen storage alloys have been studied. X-ray diffraction (XRD) analyses show that the main phases of all of the alloys are (La, Mg)Ni-3 phase (PuNi3-type structure) and LaNi5 phase (CaCu5-type structure). Electrochemical investigations show that increasing Co content and annealing treatment can considerably enhance the cyclic stability of the alloy electrodes. For La0.7Mg0.3Ni2.15Co1.05Mn0.1Al0.2 alloy, the value of C-100/C-max was only 65.5% at its as-cast, however, the value reached 80.5% after an annealing treatment of 1173 K x 8 h. The maximum discharge capacity of the alloy electrodes increased by annealing treatment and decreased slightly when Co content increased from x = 0.00 to 0.30 at its as-cast state. But the exchange current density (I-0), the limiting current density (I-L) and the diffusion coefficient of hydrogen (D) of the alloy electrodes decreased, leading to a corresponding reduction of the high rate dischargeability (HRD), with increasing Co content and annealing treatment. (C) 2007 Published by Elsevier Ltd on behalf of the International Association for Hydrogen Energy.
引用
收藏
页码:3387 / 3394
页数:8
相关论文
共 50 条
  • [1] Structure and electrochemical properties of La0.7Mg0.3Ni2.45-xCo0.75Mn0.1Al0.2Wx (x=0-0.15) hydrogen storage alloys
    Pan, HG
    Wu, XF
    Gao, MX
    Chen, N
    Yue, YJ
    Lei, YQ
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2006, 31 (04) : 517 - 523
  • [2] Effects of annealing temperature on structure and the electrochemical properties of La0.7Mg0.3Ni2.45Co0.75Mn0.1Al0.2 hydrogen storage alloy
    Pan, HG
    Chen, N
    Gao, MX
    Li, R
    Lei, YQ
    Wang, QD
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 397 (1-2) : 306 - 312
  • [3] A study on the microstructures and electrochemical properties of La0.7Mg0.3Ni2.45-xCrxCo0.75Mn0.1Al0.2 (x=0.00-0.20) hydrogen storage electrode alloys
    Miao, He
    Liu, Yongfeng
    Lin, Yan
    Zhu, Dan
    Jiang, Lei
    Pan, Hongge
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2008, 33 (01) : 134 - 140
  • [4] The effect of substitution of Zr for La on the electrochemical properties of La0.7-xZrxMg0.3Ni2.45Mn0.1Co0.75Al0.2 hydrogen storage electrode alloys
    Pan, HG
    Yue, YJ
    Gao, MX
    Wu, XF
    Chen, N
    Lei, YQ
    Wang, QD
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 397 (1-2) : 269 - 275
  • [5] A study on the structural and electrochemical properties of La0.7-xNdxMg0.3Ni2.45Co0.75Mn0.1Al0.2 (x=0.0-3.0) hydrogen storage alloys
    Ma, Shuai
    Gao, Mingxia
    Li, Rui
    Pan, Hongge
    Lei, Yongquan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 457 (1-2) : 457 - 464
  • [6] Influences of Ni addition on the structures and electrochemical properties of La0.7Mg0.3Ni2.65+xCo0.75Mn0.1 (x=0.0-0.5) hydrogen storage alloys
    Liu, YF
    Pan, HG
    Gao, MX
    Li, R
    Lei, YQ
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 389 (1-2) : 281 - 289
  • [7] Effect of the substitution of PR for LA on the microstructure and electrochemical properties of La0.7-xPrxMg0.3Ni2.45Co0.75Mn0.1Al0.2 (x=0.0-0. 3) hydrogen storage electrode alloys
    Pan, Hongge
    Ma, Shuai
    Shen, Jia
    Tan, Junjun
    Deng, Jilu
    Gao, Mingxia
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2007, 32 (14) : 2949 - 2956
  • [8] The effect of substitution Al for Ni on the electrochemical properties of La0.7Mg0.3Ni2.75-xAlxCo0.75 hydrogen storage alloys
    Guo, Jin
    Zhang, Rui
    Jiang, Wei-Qin
    Li, Guang-xu
    Wei, Wen-lou
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 429 (1-2) : 348 - 351
  • [9] Effect of Annealing Treatment on Structure and Electrochemical Properties of New Mg-free Y0.7La0.3Ni3.25Al0.1Mn0.15 Hydrogen Storage Alloys
    Deng, Anqiang
    Luo, Yongchun
    Xia, Yuanhua
    Peng, Sihui
    Ma, Weiqin
    Zhao, Xudong
    Yang, Yang
    Hou, Xiaodong
    CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 2020, 41 (01): : 145 - 154
  • [10] Electrochemical properties of the La0.7Mg0.3Ni2.65-xMn0.1Co0.75Alx (x=0-0.5) hydrogen storage alloy electrodes
    Pan, HG
    Liu, YF
    Gao, MX
    Lei, YQ
    Wang, QD
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (02) : A326 - A332