Effect of residual excess carbon on the densification of ultra-fine HfC powder

被引:6
|
作者
Kim, Jun-Seop [1 ]
Lee, Seung Jun [2 ]
Feng, Lun [3 ]
Silvestroni, Laura [4 ]
Sciti, Diletta [4 ]
Lee, Sea-Hoon [1 ]
机构
[1] Korea Inst Mat Sci, Div Powder Ceram Res, Chang Won 641831, South Korea
[2] Agcy Def Dev, Dept 4, Daejeon 34186, South Korea
[3] Missouri Univ Sci & Technol, Dept Mat Sci & Engn, Rolla, MO 65049 USA
[4] Inst Sci & Technol Ceram, I-6448018 Faenza, Italy
关键词
Hafnium carbides; Powder; Synthesis; Residual carbon; Densification; CARBOTHERMAL REDUCTION; HAFNIUM CARBIDE; ZIRCONIUM CARBIDE; PRECURSOR; DEGRADATION; BEHAVIOR; TEM;
D O I
10.1016/j.jeurceramsoc.2019.12.051
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The residual carbon content of ultra-fine hafnium carbide (HfC) powder was controlled by the optimization of the synthesis process, and the effect of residual carbon on the densification of HfC powder was analyzed. The amount of residual carbon in the HfC powder could be reduced by the de-agglomeration of HfO2 powder before the carbo-thermal reduction (CTR) process. The average particle size of HfO2 powder decreased from 230 to 130 nm after the de-agglomeration treatment. Ultra-fine (d(50): 110 nm) and highly pure (metal basis purity: > 99.9 % except for Zr) HfC powder was obtained after the CTR at 1600 degrees C for 1 h using the C/Hf mixing ratio of 3.3. In contrast, the C/Hf ratio increased to 3.6 without the de-agglomeration treatment, indicating that a large amount of excess carbon was required for the complete reduction of the agglomerated HfO2 particles. HfC ceramics with high relative density (> 98 %) were obtained after spark plasma sintering at 2000 degrees C under 80 MPa pressure when using the HfC powder with low excess carbon content. In contrast, the densification did not complete at a higher temperature (2300 degrees C) and pressure (100 MPa) when the HfC powder contained a large amount of residual carbon. The results clearly indicated that residual carbon suppressed the densification of HfC powder in case the carbide powder had low oxygen content, and the residual carbon content could be controlled by the optimization of the synthesis process. The average grain size and Vickers hardness of the sintered specimen were 6.7(+/- 0.7) mu m and 19.6 GPa, respectively.
引用
收藏
页码:1801 / 1810
页数:10
相关论文
共 50 条
  • [21] New method for ultra-fine crushing and dispersion of powder particles
    Zhang, Xiaoning
    Tuliao Gongye/Paint & Coatings Industry, 1999, 29 (09): : 14 - 16
  • [22] Preparation of ultra-fine silver powder utilized in solar cells
    Gan, W.-P. (gwp@mail.csu.edu.cn), 1600, Central South University of Technology (24):
  • [23] PRODUCTION OF ULTRA-FINE SILICON POWDER BY THE ARC PLASMA METHOD
    TANAKA, K
    ISHIZAKI, K
    YUMOTO, S
    EGASHIRA, T
    UDA, M
    JOURNAL OF MATERIALS SCIENCE, 1987, 22 (06) : 2192 - 2198
  • [24] Study on Electrophoretic Deposition Characteristics of Ultra-fine Diamond Powder
    Mao, Xianyan
    Lu, Jing
    Guo, Hua
    ADVANCED MANUFACTURING TECHNOLOGY, PTS 1-4, 2012, 472-475 : 2702 - 2706
  • [25] FATIGUE OF AN ULTRA-FINE GRAINED LOW CARBON STEEL
    Chapetti, M. D.
    Tagawa, T.
    Miyata, T.
    Fujioka, M.
    NEW DEVELOPMENTS ON METALLURGY AND APPLICATIONS OF HIGH STRENGTH STEELS: BUENOS AIRES 2008, VOLS 1 AND 2, PROCEEDINGS,, 2008, : 813 - +
  • [26] Synthesis and densification of ultra-fine ZrC powders-effects of C/Zr ratio
    Yu, Lei
    Feng, Lun
    Lee, Hyung Ik
    Silvestroni, Laura
    Sciti, Diletta
    Woo, Yi Jin
    Lee, Sea-Hoon
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2019, 81 : 149 - 154
  • [28] Preparing antioxidant peptides from ultra-fine powder of rapeseed meal
    Zhai X.
    Hu L.
    Li Y.
    Liang L.
    Hu X.
    Zhang Z.
    Ban S.
    Wang P.
    Pei H.
    Nongye Gongcheng Xuebao/Transactions of the Chinese Society of Agricultural Engineering, 2024, 40 (04): : 284 - 291
  • [29] An improved sodium silicate binder modified by ultra-fine powder materials
    Wang Ji-na
    Fan Zi-tian
    Wang Hua-fang
    Dong Xuan-pu
    Huang Nai-yu
    CHINA FOUNDRY, 2007, 4 (01) : 26 - 30