Cross-section Morphology of the Scratch-Induced Cracks in Soda-Lime-Silica Glass

被引:16
|
作者
Matsuoka, Jun [1 ]
Guo, Danwei [1 ]
Yoshida, Satoshi [1 ]
机构
[1] Univ Shiga Prefecture, Sch Engn, Dept Mat Sci, Hikone, Shiga, Japan
来源
FRONTIERS IN MATERIALS | 2017年 / 4卷
关键词
soda-lime-silica glass; scratch; cracking; lateral crack; median crack; stress corrosion; SURFACE DAMAGE; PROPAGATION; INITIATION;
D O I
10.3389/fmats.2017.00008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Scratch-induced cracking is a serious problem for the use of glass products. At the scratch process, both median (vertical to the glass surface) and lateral (horizontal to the glass surface) cracks are formed. In this study, morphology of the scratch-induced cracks in a commercial soda-lime-silica glass was investigated by the scanning electron microscopy for the specimen broken across the scratch groove. Scratch test was carried out using a Knoop indenter in water and in dehydrated heptane. When scratch speed was 70 x 10(-6) m s(-1), length of both vertical and horizontal cracks was proportional to the normal load at scratching, and environmental dependence was not observed. When scratch speed was increased with the constant normal load of 200 g, length of both cracks was decreased. In the case of horizontal crack, no environmental effect was observed. On the other hand, length of the vertical crack scratched in water was much longer than that in heptane. At very high scratch speed as high as 1,000 x 10(-6) m s(-1), no vertical crack was formed in the heptane. These differences between horizontal and vertical cracks should be due to the differences of crack initiation position and the influence of subcritical crack growth to these cracks.
引用
收藏
页数:5
相关论文
共 50 条
  • [31] Gas release phenomena in soda-lime-silica glass
    Vernerova, Miroslava
    Nemec, Lubomir
    Klouzek, Jaroslav
    Hujova, Miroslava
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 500 : 158 - 166
  • [32] The Fracture Process of Tempered Soda-Lime-Silica Glass
    Nielsen, J. H.
    Olesen, J. F.
    Stang, H.
    EXPERIMENTAL MECHANICS, 2009, 49 (06) : 855 - 870
  • [33] The brittle to ductile transition in a soda-lime-silica glass
    Rouxel, T
    Sangleboeuf, JC
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2000, 271 (03) : 224 - 235
  • [34] STUDIES ON CHEMICAL STRENGTHENING OF SODA-LIME-SILICA GLASS
    WARD, JB
    SUGARMAN, B
    SYMMERS, C
    GLASS TECHNOLOGY, 1965, 6 (03): : 90 - +
  • [35] Decelerated crystal growth in a soda-lime-silica glass
    Fielitz, Peter
    Cassar, Daniel R.
    Yuritsyn, Nikolay S.
    Abyzov, Alexander S.
    Fokin, Vladimir M.
    Borchardt, Guenter
    Deubener, Joachim
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2022, 596
  • [36] The Fracture Process of Tempered Soda-Lime-Silica Glass
    J. H. Nielsen
    J. F. Olesen
    H. Stang
    Experimental Mechanics, 2009, 49 : 855 - 870
  • [37] SODA-LIME-SILICA GLASS FOR RADIATION-DOSIMETRY
    EZZELDIN, FM
    ABDELREHIM, F
    ABDELAZIM, AA
    AHMED, AA
    MEDICAL PHYSICS, 1994, 21 (07) : 1085 - 1089
  • [38] Surface damage of soda-lime-silica glasses:: indentation scratch behavior
    Le Houérou, V
    Sangleboeuf, JC
    Dériano, S
    Rouxel, T
    Duisit, G
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2003, 316 (01) : 54 - 63
  • [39] Photo-irradiation induced recyclable coloration for soda-lime-silica glass
    Sheng, J
    Kadono, K
    Yazawa, T
    PHYSICS AND CHEMISTRY OF GLASSES, 2004, 45 (01): : 27 - 31
  • [40] Flame-impingement-induced superhydrophilicity of soda-lime-silica glass surface
    Roy, Barsheek
    Schmidt, Anne
    Rosin, Andreas
    Gerdes, Thorsten
    INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2024,