Influence of Ru on the hardness and fracture toughness of WC-VC-Co alloys

被引:22
|
作者
Chipise, L. [1 ,3 ]
Jain, P. K. [2 ,3 ]
Cornish, L. A. [1 ,3 ]
机构
[1] Univ Witwatersrand, DST NRF Ctr Excellence Strong Mat, Sch Chem & Met Engn, Private Bag 3, ZA-2050 Johannesburg, South Africa
[2] Univ Botswana, Phys Dept, Private Bag, Gaborone 0022, Botswana
[3] AMSEN, Johannesburg, South Africa
关键词
CEMENTED CARBIDES; GRAIN-SIZE; MECHANICAL-PROPERTIES; TUNGSTEN CARBIDE; HARDMETALS; MICROSTRUCTURE; DEFORMATION; INDENTATION; ADDITIONS; POWDERS;
D O I
10.1016/j.ijrmhm.2018.07.008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of Ru additions on the hardness and fracture toughness of WC-VC-Co alloys were investigated on the following compositions: 80WC-10VC-(10-x)Co-xRu (0 <= x <= 3) (wt%), (89.6-x)WC-10Co-0.4VC-xRu (0 <= x <= 2) (wt%), (89.2-x)WC-10Co-0.8VC-xRu (0 <= x <= 2) (wt%) and 89.6WC-(10-x)Co-0.4VC-xRu (0 <= x <= 3) (wt%). Hardness increased with increased Ru additions in all alloy series due to a combination of decreased grain size and increased solid solution strengthening. Ruthenium additions generally compromised fracture toughness, although there was improvement for some compositions.
引用
收藏
页码:54 / 60
页数:7
相关论文
共 50 条
  • [41] Fracture strength of WC-Co alloys
    Cao, SH
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1997, 7 (03) : 54 - 56
  • [42] Investigation of hardness and fracture toughness properties of Fe/VC multilayer coatings with coherent interfaces
    Wang, Chen
    Pureza, Julio Miranda
    Yang, Yanqing
    Chung, Yip-Wah
    SURFACE & COATINGS TECHNOLOGY, 2016, 288 : 179 - 184
  • [43] INFLUENCE OF THE MICROSTRUCTURE OF WC-CO CEMENTED CARBIDES ON THE FRACTURE-TOUGHNESS AND ABRASIVE WEAR
    ZUMGAHR, KH
    FISCHER, A
    METALL, 1981, 35 (01): : 38 - 44
  • [44] Fracture toughness of a nanoscale WC-Co tool steel
    Densley, JM
    Hirth, JP
    SCRIPTA MATERIALIA, 1997, 38 (02) : 239 - 244
  • [45] Fracture toughness KIC of cemented carbide WC-Co
    Doi, S.
    Yasuoka, M.
    MATERIALS CHARACTERISATION IV: COMPUTATIONAL METHODS AND EXPERIMENTS, 2009, 64 : 217 - +
  • [46] Fracture toughness of solar-sintered WC with Co additive
    Rosa, LG
    Amaral, PM
    Anjinho, C
    Fernandes, JC
    Shohoji, N
    CERAMICS INTERNATIONAL, 2002, 28 (03) : 345 - 348
  • [47] Influence of microstructure on the fracture toughness of tungsten alloys
    Gludovatz, B.
    Faleschini, M.
    Wurster, S.
    Hoffmann, A.
    Pippan, R.
    TMS 2008 ANNUAL MEETING SUPPLEMENTAL PROCEEDINGS, VOL 1: MATERIALS PROCESSING AND PROPERTIES, 2008, : 449 - +
  • [48] Effect of WC content on hardness and fracture toughness of WC-Ni60A wear-resistant coatings
    Wei, Min
    Li, Jing
    Xie, Kun
    Xiao, Yang-yi
    Wan, Qiang
    Yang, Zhen-ting
    Huang, Yong-jun
    Refai, Mohamed
    SURFACE & COATINGS TECHNOLOGY, 2024, 491
  • [49] TEMPERATURE DEPENDENCE OF STRENGTH AND HARDNESS OF WC-TAC-CO AND WC-NBC-CO ALLOYS
    PANOV, VS
    MEYERSON, GA
    RUSSIAN METALLURGY-METALLY-USSR, 1968, (05): : 109 - &
  • [50] Hardness to toughness relationship of fine-grained WC-Co hardmetals
    Schubert, WD
    Neumeister, H
    Kinger, G
    Lux, B
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 1998, 16 (02): : 133 - 142