Durability of GFRC Modified by Calcium Sulfoaluminate Cement under Elevated Curing Temperatures
被引:3
|
作者:
Song, Meimei
论文数: 0引用数: 0
h-index: 0
机构:
Xian Shiyou Univ, Sch Mech Engn, Xian, Peoples R China
Wuhan Univ Technol, State Key Labs Silicate Mat Architectures, Wuhan, Peoples R ChinaXian Shiyou Univ, Sch Mech Engn, Xian, Peoples R China
Song, Meimei
[1
,2
]
Wu, Ke
论文数: 0引用数: 0
h-index: 0
机构:
Univ Coll Dublin, Sch Mech & Mat Engn, Dublin, IrelandXian Shiyou Univ, Sch Mech Engn, Xian, Peoples R China
Wu, Ke
[3
]
Dou, Yihua
论文数: 0引用数: 0
h-index: 0
机构:
Xian Shiyou Univ, Sch Mech Engn, Xian, Peoples R ChinaXian Shiyou Univ, Sch Mech Engn, Xian, Peoples R China
Dou, Yihua
[1
]
机构:
[1] Xian Shiyou Univ, Sch Mech Engn, Xian, Peoples R China
[2] Wuhan Univ Technol, State Key Labs Silicate Mat Architectures, Wuhan, Peoples R China
CSA/GFRC is an advanced composite material possessed with great ductility and durability. However, its bending performance and fibre condition, as well as intrinsic microstructural changes, under elevated temperature have not been understood so far. XRD was applied in this study to investigate the hydration mechanism of CSA cement under 50 degrees C, 70 degrees C, and 80 degrees C. Bending performance was carried out to test the toughness of CSA/GFRC. SEM was applied to observe the underlying microstructural changes of CSA/GFRC under different curing regimes. It was found out that there was a gradual degradation of both ultimate tensile strength and ultimate strain of CSA/GFRC with elevated curing temperature and curing age, but glass fibre still shows considerable ability to carry stress alone by bridging cracks. Microstructural studies showed that, at accelerated temperatures of 50 degrees C and 70 degrees C, the space between fibres remained empty in general only with some hydration products adhering to the fibre surface occasionally. At a higher accelerated curing temperature of 80 degrees C, densification of the interfilamentary spaces by larger and clustered hydration products can be observed at longer curing ages, causing the fibres to lose parts of the flexibility. Therefore, it can be concluded that densification of interfilamentary spaces may have a greater role to play in the strength degradation of CSA/GFRC than mechanisms associated with fibre weakening caused by chemical corrosion.
机构:
Slovenian Natl Bldg & Civil Engn Inst, Dimiceva Ulica 12, Ljubljana 1000, Slovenia
Jozef Stefan Int Postgrad Sch, Jamova Cesta 39, Ljubljana 1000, SloveniaSlovenian Natl Bldg & Civil Engn Inst, Dimiceva Ulica 12, Ljubljana 1000, Slovenia
Borstnar, Marusa
Daneu, Nina
论文数: 0引用数: 0
h-index: 0
机构:
Jozef Stefan Inst, Jamova Cesta 39, Ljubljana 1000, SloveniaSlovenian Natl Bldg & Civil Engn Inst, Dimiceva Ulica 12, Ljubljana 1000, Slovenia
Daneu, Nina
Dolenec, Sabina
论文数: 0引用数: 0
h-index: 0
机构:
Slovenian Natl Bldg & Civil Engn Inst, Dimiceva Ulica 12, Ljubljana 1000, SloveniaSlovenian Natl Bldg & Civil Engn Inst, Dimiceva Ulica 12, Ljubljana 1000, Slovenia