Simulations of chemical vapor deposition diamond film growth using a kinetic Monte Carlo model and two-dimensional models of microwave plasma and hot filament chemical vapor deposition reactors

被引:14
|
作者
May, P. W. [1 ]
Harvey, J. N. [1 ]
Allan, N. L. [1 ]
Richley, J. C. [1 ]
Mankelevich, Yu. A. [2 ]
机构
[1] Univ Bristol, Sch Chem, Bristol BS8 1TS, Avon, England
[2] Moscow MV Lomonosov State Univ, Skobeltsyn Inst Nucl Phys, Moscow 119991, Russia
基金
英国工程与自然科学研究理事会;
关键词
SOOT PARTICLES; SURFACE; MECHANISM; DISCHARGES; MIGRATION; RADICALS;
D O I
10.1063/1.3516498
中图分类号
O59 [应用物理学];
学科分类号
摘要
A one-dimensional kinetic Monte Carlo (KMC) model has been developed to simulate the chemical vapor deposition of a diamond (100) surface under conditions used to grow single-crystal diamond (SCD), microcrystalline diamond (MCD), nanocrystalline diamond (NCD), and ultrananocrystalline diamond (UNCD) films. The model considers adsorption, etching/desorption, lattice incorporation and surface migration but not defect formation or renucleation processes. Two methods have been devised for estimation of the gas phase concentrations of species at the growing diamond surface, and are used to determine adsorption rates for C1Hx hydrocarbons for the different conditions. The rate of migration of adsorbed carbon species is governed by the availability of neighboring radical sites, which, in turn, depend upon the rates of H abstraction and of surface-radical migration. The KMC model predicts growth rates and surface roughness for each of diamond types consistent with experiment. In the absence of defect formation and renucleation the average surface diffusion length, l, is a key parameter controlling surface morphology. When l < 2, surface migration is limited by the lack of availability of surface radical sites, and the migrating surface species simply hop back and forth between two adjacent sites but do not travel far beyond their initial adsorption site. Thus, Eley-Rideal processes dominate the growth, leading to the rough surfaces seen in NCD and UNCD. The maximum or "intrinsic" surface roughness occurs for nominally zero-migration conditions (l = 0) with an rms value of approximately five carbon atoms. Conversely, when migration occurs over greater distances (l > 2), Langmuir-Hinshelwood processes dominate the growth producing the smoother surfaces of MCD and SCD. By extrapolation, we predict that atomically smooth surfaces over large areas should occur once migrating species can travel approximately five sites (l similar to 5). beta-scission processes are found to be unimportant for MCD and SCD growth conditions, but can remove up to 5% of the adsorbing carbon for NCD and UNCD growth. C1Hx insertion reactions also contribute <1% to the growth for nearly all conditions, while C2Hx (x < 2) insertion reactions are negligible due their very low concentrations at the surface. Finally, the predictions for growth rate and morphology for UNCD deposition in a microwave system were found to be anomalous compared to those for all the other growth conditions, suggesting that carbonaceous particulates created in these plasmas may significantly affect the gas chemistry. (C) 2010 American Institute of Physics. [doi: 10.1063/1.3516498]
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Chemical vapor deposition of diamond films in hot filament reactor
    Grus, M
    Jankowska-Frydel, A
    Bohdanowicz, J
    Zawada, K
    CRYSTAL RESEARCH AND TECHNOLOGY, 2001, 36 (8-10) : 961 - 970
  • [22] The Effect of Sound on Diamond Hot Filament Chemical Vapor Deposition
    Karim, Syed Md. Ihsanul
    Chowdhury, Mohammad Asaduzzaman
    Helali, Md. Maksud
    INTERNATIONAL JOURNAL OF CHEMICAL REACTOR ENGINEERING, 2009, 7
  • [23] The morphology of diamond grown by hot filament chemical vapor deposition
    Menon, PM
    Clausing, RE
    Heatherly, L
    Feigerle, CS
    DIAMOND AND RELATED MATERIALS, 1998, 7 (08) : 1201 - 1206
  • [24] Nucleation kinetics of diamond in hot filament chemical vapor deposition
    Yu, Jie
    Huang, Rong Fang
    Wen, Lishi
    Shi, Changxu
    Materials Research Bulletin, 34 (14): : 2319 - 2325
  • [25] Nucleation kinetics of diamond in hot filament chemical vapor deposition
    Yu, J
    Huang, RF
    Wen, LS
    Shi, CX
    MATERIALS RESEARCH BULLETIN, 1999, 34 (14-15) : 2319 - 2325
  • [26] A kinetic Monte Carlo model for the growth and etching of graphene during chemical vapor deposition
    Chen, Shuai
    Gao, Junfeng
    Srinivasan, Bharathi M.
    Zhang, Gang
    Sorkin, Viacheslav
    Hariharaputran, Ramanarayan
    Zhang, Yong-Wei
    CARBON, 2019, 146 : 399 - 405
  • [27] Selective growth of diamond and carbon nanostructures by hot filament chemical vapor deposition
    Yang, Q
    Xiao, C
    Chen, W
    Hirose, A
    DIAMOND AND RELATED MATERIALS, 2004, 13 (03) : 433 - 437
  • [28] NUCLEATION AND GROWTH OF DIAMOND IN HOT FILAMENT ASSISTED CHEMICAL VAPOR-DEPOSITION
    HYER, RC
    GREEN, M
    MISHRA, KK
    SHARMA, SC
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1991, 10 (09) : 515 - 518
  • [29] Epitaxially oriented growth of diamond on silicon by hot filament chemical vapor deposition
    Chen, QJ
    Wang, LX
    Zhang, Z
    Yang, J
    Lin, ZD
    APPLIED PHYSICS LETTERS, 1996, 68 (02) : 176 - 178